Displaying publications 1 - 20 of 28 in total

Abstract:
Sort:
  1. Nur Ain, A.R., Mohd Sabri, M.G., Wan Rafizah, W.A., Nurul Azimah, M.A., Wan Nik, W.B.
    ASM Science Journal, 2018;11(101):56-67.
    MyJurnal
    Corrosion is a natural deterioration process that destructs metal surface. Metal of highly
    protected by passivation layer such as Stainless Steel 316L also undergoes pitting corrosion
    when continuously exposed to aggressive environment. To overcome this phenomenon, application
    of epoxy based coating with addition of zinc oxide- poly (3,4-ethylenedioxythiophene)
    doped with poly (styrene sulphonate) hybrid nanocomposite additive was introduced as
    paint/metal surface coating. The compatibility between these two materials as additive
    was studied by Fourier Transform Infrared Spectroscopy (FTIR), X-ray Diffraction (XRD),
    Field Emission Scanning Electron Microscopy/Energy-Dispersive X-ray spectroscopy (FESEM/EDX)
    and Transmission Electron Microscopy (TEM) analysis. The effect of nanocomposite
    wt.% in epoxy based coating with immersion duration in real environment on corrosion
    protection performance was analyzed through potentiodynamic polarization analysis. The
    main finding showed that addition of hybrid nanocomposite had increased corrosion protection
    yet enhanced corrosion process when excess additives was loaded into epoxy coating.
    Addition of 2 wt.% ZnO-PEDOT:PSS was found significantly provided optimum corrosion
    protection to stainless steel 316L as the corrosion rate for 0 day, 15 days and 30 days of
    immersion duration is 0.0022 mm/yr, 0.0004 mm/yr and 0.0015 mm/yr; respectively.
    Matched MeSH terms: Paint
  2. Suhaida Sabdi, Wan Zaripah Wan Bakar, Adam Husein
    MyJurnal
    Some restorative materials are susceptible to erosion but whether it also causes microleakage is still questionable. The aim of this study was to assess the microleakage of few restorative materials after immersion in acidic solution. Standardized ‘U’ shaped cavity of 4mm diameter and 2mm depth were prepared on buccal or lingual surface of 52 human premolar and molar teeth. The teeth were divided into 4 groups which contains 13 samples and 3 controls for each and were restored either with Filtek Z250 (Group 1), Fuji IX (Group 2), Fuji II LC (Group 3), or Silverfill amalgam (Group 4).
    All surfaces were painted with nail varnish leaving only 2mm of tooth structure surrounding the restoration before the study samples were immersed in acidic solution, lemon juice (pH 2.74) and control samples in deionised distilled water for 24 hours. Surface photos for erosion were taken before immersion in methylene blue for 7 days. After sectioning, the assessment of dye penetration was done using Leica Imaging System DMLM (Germany). Photos showed that Fuji IX demonstrated severe erosion but no obvious changes were seen on other materials. Kruskal-Wallis test indicated that microleakage between all four groups were statistically significant. The most significant difference was between Filtek Z250 and Fuji IX (p
    Matched MeSH terms: Paint
  3. Saini, D., Nadig, G., Saini, R.
    MyJurnal
    The main objective of a root end filling material is to provide an apical seal that prevents the movement of bacteria and the diffusion of bacterial products from the root canal system into periapical tissues. The aim of this study was to compare the microleakage of three root end filling materials Mineral trioxide aggregate (MTA), Glass ionomer cement (GIC) and Silver GIC (Miracle Mix) using dye penetration technique under stereomicroscope. Forty-five extracted human maxillary central incisors were instrumented and obturated with gutta percha using lateral compaction technique. Following this, the teeth were stored in saline. After one week, teeth were apically resected at an angle of 90ï° to the long axis of the root and root end cavities were prepared. The teeth were divided into three groups of fifteen specimens each and were filled with Group I -MTA, Group II - GIC and Group III - Miracle Mix. The samples were coated with varnish and after drying, they were immersed in 1% methylene blue dye for 72 hours. The teeth were then rinsed, sectioned longitudinally and observed under stereomicroscope. The depth of dye penetration was measured in millimeters. Microleakage was found to be significantly less in MTA (0.83 mm) when compared to GIC (1.32 mm) (p < 0.001) and with Miracle Mix (1.39 mm) (p < 0.001) No significant difference was found when microleakage in Miracle Mix was compared to that of GIC (p = 0.752). Thus we concluded that MTA is a better material as root end filling material to prevent microleakage, in comparison to GIC and Miracle Mix.
    Matched MeSH terms: Paint
  4. Shafqat SR, Bhawani SA, Bakhtiar S, Ibrahim MNM
    BMC Chem, 2020 Dec;14(1):27.
    PMID: 32266334 DOI: 10.1186/s13065-020-00680-8
    Congo red (CR) is an anionic azo dye widely used in many industries including pharmaceutical, textile, food and paint industries. The disposal of huge amount of CR into the various streams of water has posed a great threat to both human and aquatic life. Therefore, it has become an important aspect of industries to remove CR from different water sources. Molecular imprinting technology is a very slective method to remove various target pollutant from environment. In this study a precipitation polymerization was employed for the effective and selective removal of CR from contaminated aqueous media. A series of congo red molecularly imprinted polymers (CR-MIPs) of uniform size and shape was developed by changing the mole ratio of the components. The optimum ratio (0.1:4: 20, template, functional monomer and cross-linking monomer respectively) for CR1-MIP from synthesized polymers was able to rebind about 99.63% of CR at the optimum conditions of adsorption parameters (contact time 210 min, polymer dosage 0.5 g, concentration 20 ppm and pH 7). The synthesized polymers were characterized by various techniques such as Fourier Infra-red spectroscopy (FTIR), scanning electron microscopy (SEM), Thermogravimetric analysis (TGA), energy-dispersive X-ray spectroscopy (EDX), and Brumauer-Emmett-Teller (BET). The polymer particles have successfully removed CR from different aqueous media with an efficiency of about ~ 90%.
    Matched MeSH terms: Paint
  5. Ravizza M, Giosio D, Henderson A, Hovenden M, Hudson M, Salleh S, et al.
    Biofouling, 2016 07;32(6):685-97.
    PMID: 27244248 DOI: 10.1080/08927014.2016.1184255
    Biofouling in canals and pipelines used for hydroelectric power generation decreases the flow capacity of conduits. A pipeline rig was designed consisting of test sections of varying substrata (PVC, painted steel) and light levels (transparent, frosted, opaque). Stalk-forming diatoms were abundant in both the frosted and transparent PVC pipes but negligible in the painted steel and opaque PVC pipes. Fungi were slightly more abundant in the painted steel pipe but equally present in all the other pipes while bacterial diversity was similar in all pipes. Photosynthetically functional biofouling (mainly diatoms) was able to develop in near darkness. Different biological fouling compositions generated differing friction factors. The highest friction factor was observed in the transparent pipe (densest diatom fouling), the lowest peak friction for the opaque PVC pipe (lowest fouling biomass), and with the painted steel pipe (high fouling biomass, but composed of fungal and bacterial crusts) being intermediate between the opaque and frosted PVC pipes.
    Matched MeSH terms: Paint
  6. Aisami Abubakar, Mohd Yunus Shukor
    MyJurnal
    Environmental pollution is one of the major concerns in the 21st century; where billions of tonnes
    of harmful chemicals are produced by industries such as petroleum, paints, food, rubber, and
    plastic. Phenol and its derivatives infiltrate the ecosystems and have become one of the top major
    pollutants worldwide. This review covers the major aspects of immobilization of phenoldegrading
    bacteria as a method to improve phenol bioremediation. The use of various forms of
    immobilization matrices is discussed along with the advantages and disadvantages of each of the
    immobilization matrices especially when environmental usage is warranted. To be used as a
    bioremediation tool, the immobilized system must not only be effective, but the matrices must be
    non-toxic, non-polluting and if possible non-biodegradable. The mechanical, biological and
    chemical stability of the system is paramount for long-term activity as well as price is an
    important factor when the very large scale is a concern. The system must also be able to tolerate
    high concentration of other toxicants especially heavy metals that form as co-contaminants, and
    most immobilized systems are geared towards this last aspect as immobilization provides
    protection from other contaminants.
    Matched MeSH terms: Paint
  7. Clark CS, Rampal KG, Thuppil V, Roda SM, Succop P, Menrath W, et al.
    Environ Res, 2009 Oct;109(7):930-6.
    PMID: 19656507 DOI: 10.1016/j.envres.2009.07.002
    In 2006 a report on the analysis for lead in 80 new residential paints from four countries in Asia revealed high levels in three of the countries (China, India and Malaysia) and low levels in a fourth country (Singapore) where a lead in paint regulation was enforced. The authors warned of the possible export of lead-painted consumer products to the United States and other countries and the dangers the lead paint represented to children in the countries where it was available for purchase. The need for a worldwide ban on the use of lead in paints was emphasized to prevent an increase in exposure and disease from this very preventable environmental source. Since the earlier paper almost 300 additional new paint samples have been collected from the four initial countries plus 8 additional countries, three from Asia, three from Africa and two from South America. During the intervening time period two million toys and other items imported into the United States were recalled because the lead content exceeded the United States standard. High lead paints were detected in all 12 countries. The average lead concentration by country ranged from 6988 (Singapore) to 31,960ppm (Ecuador). One multinational company sold high lead paint in one country through January 2007 but sold low lead paint later in 2007 indicating that a major change to cease adding lead to their paints had occurred. However, the finding that almost one-third of the samples would meet the new United States standard for new paint of 90ppm, suggests that the technology is already available in at least 11 of the 12 countries to produce low lead enamel paints for domestic use. The need remains urgent to establish effective worldwide controls to prevent the needless poisoning of millions of children from this preventable exposure.
    Matched MeSH terms: Paint/analysis*
  8. Clark CS, Rampal KG, Thuppil V, Chen CK, Clark R, Roda S
    Environ Res, 2006 Sep;102(1):9-12.
    PMID: 16782088
    Worldwide prohibitions on lead gasoline additives were a major international public health accomplishment, the results of which are still being documented in parts of the world. Although the need to remove lead from paints has been recognized for over a century, evidence reported in this article indicates that lead-based paints for household use, some containing more than 10% lead, are readily available for purchase in some of the largest countries in the world. Sixty-six percent of new paint samples from China, India, and Malaysia were found to contain 5000 ppm (0.5%) or more of lead, the US definition of lead-based paint in existing housing, and 78% contained 600 ppm (0.06%) or more, the limit for new paints. In contrast, the comparable levels in a nearby developed country, Singapore, were 0% and 9%. In examining lead levels in paints of the same brands purchased in different countries, it was found that some brands had lead-based paints in one of the countries and paints meeting US limits in another; another had lead-free paint available in all countries where samples were obtained. Lead-based paints have already poisoned millions of children and likely will cause similar damage in the future as paint use increases as countries in Asia and elsewhere continue their rapid development. The ready availability of lead-based paints documented in this article provides stark evidence of the urgent need for efforts to accomplish an effective worldwide ban on the use of lead in paint.
    Matched MeSH terms: Paint/analysis*
  9. Ali HR, Ariffin MM, Omar TFT, Ghazali A, Sheikh MA, Shazili NAM, et al.
    Environ Sci Pollut Res Int, 2021 Oct;28(37):52247-52257.
    PMID: 34002317 DOI: 10.1007/s11356-021-14424-1
    Irgarol 1051 and diuron are photosystem II inhibitors in agricultural activities and antifouling paints in the shipping sector. This study focused on three major ports (western, southern, and eastern) surrounding Peninsular Malaysia to construct the distribution of both biocides on the basis of the seasonal and geographical changes. Surface seawater samples were collected from November 2011 to April 2012 and pretreated using the solid-phase extraction technique followed by quantification with GC-MS and LC-MS-MS for Irgarol 1051 and diuron, respectively. Generally, the distribution of Irgarol 1051 was lowest during November 2011 and highest during April 2012, and similar patterns were observed at all ports, whereas the distribution of diuron was rather vague. The increasing pattern of Irgarol 1051 from time to time is probably related to its accumulation in the seawater as a result of its half-life and consistent utilization. On the basis of the discriminant analysis, the temporal distribution of Irgarol 1051 varied at Klang North Port, Klang South Port, and Pasir Gudang Port, whereas diuron was temporally varied only at Kemaman Port. Furthermore, Irgarol 1051 was spatially varied during November 2011, whereas diuron did not show any significant changes throughout all sampling periods. Ecological risk assessment exhibited a high risk for diuron and Irgarol 1051, but Irgarol 1051 should be of greater concern because of its higher risk compared to that of diuron. Thus, it is recommended that the current Malaysian guidelines and regulations of biocide application should be reevaluated and improved to protect the ecosystem, as well as to prevent ecological risks to the aquatic environment.
    Matched MeSH terms: Paint
  10. Anezaki K, Kannan N, Nakano T
    Environ Sci Pollut Res Int, 2015 Oct;22(19):14478-88.
    PMID: 24809497 DOI: 10.1007/s11356-014-2985-6
    This study reports the concentrations and congener partners of polychlorinated biphenyls (PCBs) in commercially available paints. Polycyclic-type pigments containing dioxazine violet (pigment violet (PV) 23, PV37) and diketopyrrolopyrrole (PR254, PR255) were found to contain PCB-56, PCB-77, PCB-40, PCB-5, and PCB-12, and PCB-6, PCB-13, and PCB-15, respectively, as major congeners. Dioxazine violet is contaminated with by-products during synthesis from o-dichlorobenzene, which is used as a solvent during synthesis, and diketopyrrolopyrrole is contaminated with by-products during synthesis from p-chlorobenzonitrile. The concentration of PCBs in paint containing PV23 or PV37 was 0.050-29 mg/kg, and toxic equivalency (TEQ) values ranged 1.1-160 pg-TEQ/g. The concentration of PCBs in paint containing PR254 or PR255 was 0.0019-2.4 mg/kg. Naphthol AS is an azo-type pigment, and PCB-52 was detected in paint containing pigment red (PR) 9 with 2,5-dichloroaniline as its source. PCB-146, PCB-149, and PCB-153 were identified from paint containing PR112 produced from 2,4,5-trichloroaniline, as major congeners. These congeners have chlorine positions similar to aniline, indicating that these congeners are by-products obtained during the synthesis of pigments. The concentrations of PCBs in paints containing PR9 and PR112 were 0.0042-0.43 and 0.0044-3.8 mg/kg, respectively. The corresponding TEQ for PR112 was 0.0039-8.6 pg-TEQ/g.
    Matched MeSH terms: Paint/analysis*; Paint/standards
  11. Lee HL, Rohani A, Khadri MS, Nazni WA, Rozilawati HA, Nurulhusna AH, et al.
    MyJurnal
    Dengue is a serious mosquito borne disease common in tropical and sub-tropical countries including Malaysia. There is at present a lack of specific treatment and an effective tetravalent vaccine against dengue. The control of dengue depends solely on the suppression of the two most important vectors namely, Aedes aegypti and Ae albopictus. Despite intensive and extensive control efforts by health agencies, the disease continues to spread. This paper updates various innovations on control of dengue vectors. Gene-based sterile insect technique using the RIDL technology for both Aedes aegypti & Ae albopictus control has now been actively researched and field trials are pursued to evaluate the effectiveness of the technology. The release of Wolbachia-infected Ae aegypti is another dengue control innovation. The infected mosquito cannot support development of dengue virus and has shorter life span. Other innovations include: auto-dissemination of insect control agents using ovitrap, autocidal adult and larva trap, outdoor residual spraying, insecticidal paint and biocontrol agent. In other innovation, outbreak prediction capability is enhanced by developing model based on environmental data and analysis utilising neural network.
    Matched MeSH terms: Paint
  12. Naidu S, Tandon S, Nayak R, Ratnanag PV, Prajapati D, Kamath N
    Int J Clin Pediatr Dent, 2016 Oct-Dec;9(4):296-302.
    PMID: 28127159 DOI: 10.5005/jp-journals-10005-1381
    To assess the effect of combined use of chlorhexidine and fluoride varnish on the remineralization of incipient carious lesions in young children.
    Matched MeSH terms: Paint
  13. Rohani Abu Bakar, Asrul Mustafa
    MyJurnal
    Adhesives serve many functions in daily life, starting from sticking envelopes to rejoining broken
    materials. Adhesives are usually developed for a specific purpose and the performances can vary
    according to their specific end-use. Most of the commercially available adhesives comprised nonrenewable or petroleum derived raw materials. Thus, in order to mitigate negative impact of using nonrenewable material as the raw material for adhesives, a new type of adhesive containing epoxidised
    natural rubber (NR) latex is developed. Epoxidised NR latex adhesive was initially prepared and pigment
    was subsequently added to produce desired colours of the adhesive. Hence, the newly developed adhesive
    can serve as adhesive and also as paint for art. The adhesives were characterised and the results indicated
    that they were free from heavy metal contents and volatile organic compounds (VOCs). The adhesives
    exhibited comparable odour concentration to commercial synthetic-based adhesive. In terms of toxicity
    level, the adhesive developed exhibited low acute oral toxicity. Peel adhesion test of A4 and drawing
    papers on stainless steel and glass substrates, opacity and glossiness were also investigated in the present
    study. This coloured adhesive is deemed to support the STEM (science, technology, engineering and
    mathematics) learning by indirectly imparting polymer science and technology in art education and
    further promotes creative learning among school children. The adhesive is also derived from renewable
    material rendering it more environmentally friendly.
    Matched MeSH terms: Paint
  14. Ahmed, Al-Halemi, Jaafar, M.S.
    MyJurnal
    Radon-222 emanation from selected locally produced samples of building materials, used in Malaysia were measured using the Professional Continuous Radon Monitor Model 1027, which is a patented electronic detecting-junction photodiode sensor to measure the concentration of radon gas. Each sample was placed for 72 hours inside a 3.11 x 10 -2 m 3 sealed container. It was found that the average radon concentration Bqm -3 of air for concrete bricks, concrete brick with cemented coatings, concrete brick with cemented coatings and paint samples were, 303.7 Bq/m 3, 436.6 Bqm -3, and 410.7 Bqm -3, respectively. (Bqm -3 ) for brown clay brick, brown clay brick with cemented coatings, brown clay brick with cemented coatings and paint were 166.5 Bqm -3, 166.5 Bqm -3, and 148 Bqm -3, respectively. (Bqm -3 ) for sample of compact ceramic tile was 0 Bqm -3. The findings show that concrete brick samples are important source of radon emanation, while brown clay brick have been accepted as the recommendation of the U.S. Environmental Protection Agency (EPA), and ceramic tiles had no emanation of radon gas due to their compact surface, or the glazed layer created on the tile surface during the manufacturing process, which blocks radon emanation. A positive correlation between radon emanation and radium content has been observed for both brown clay brick and concrete brick samples whereas a negative correlation for ceramic tile has been observed. Consequently from the findings, in order to reduce radon emanation and radon exposure in house dwellings and in addition to EPA recommendation of sealed cracks and established good ventilation, we recommend concrete walls to be painted and concrete floors to be paved with ceramic tiles.
    Matched MeSH terms: Paint
  15. Huang SL, Yin CY, Yap SY
    J Hazard Mater, 2010 Feb 15;174(1-3):839-42.
    PMID: 19836131 DOI: 10.1016/j.jhazmat.2009.09.129
    In this study, the particle size distribution and concentration of metallic elements of solvent- and water-based paint dust from bulk dust collected from dust-collecting hoppers were determined. The mean particle size diameter over a 12-week sampling period was determined using a particle size analyzer. The metals composition and concentration of the dust were determined via acid digestion technique followed by concentration analysis using inductively coupled plasma. The volume weighted mean particle diameters were found to be 0.941+/-0.016 and 8.185+/-0.201 microm for solvent- and water-based paint dust, respectively. The mean concentrations of metals in solvent-based paint dust were found to be 100+/-20.00 microg/g (arsenic), 1550+/-550.00 microg/g (copper), 15,680+/-11,780.00 microg/g (lead) and 30,460+/-10,580.00 microg/g (zinc) while the mean concentrations of metals in water-based paint dust were found to be 20.65+/-6.11 microg/g (arsenic), 9.14+/-14.65 microg/g (copper), 57.46+/-22.42 microg/g (lead) and 1660+/-1260 microg/g (zinc). Both paint dust types could be considered as hazardous since almost all of the dust particles were smaller than 10 microm. Particular emphasis on containment of solvent-based paint dust particles should be given since it was shown that they were very fine in size (<1 microm) and had high lead and zinc concentrations.
    Matched MeSH terms: Paint*
  16. Shaharom, N.A., Nyamah, M.A., Norashikin, M., Zaharah, M.S., Zuhaida, A.J., Norb, H., et al.
    MyJurnal
    The state of Johore suffered a massive flood disaster from 19th December 2006 to 1st January and from 12th January to 19th February 2007. The possible upsurge of dengue was of foremost concern and led to efforts in increasing control activities. Anyone with history of high fever with at least two symptoms of severe headache, pain behind the eyes, muscles and joint paint, rashes and petechiae were notified as dengue. Active and passive case finding was initiated at all 371 evacuation centres as well through health facilities and hospitals through an active surveillance system. Presumptive larval survey was also carried together with control activities by 46 health teams. Data were collected using the format ‘Aktiviti harian kawalan denggi di kawasan pos banjir- Lampiran E‘ and ‘Laporan aktiviti harian kawalan denggi di pusat pemindahan banjir – Lampiran D2’. Dengue serology and blood film for malaria was sent for as well as vector species identification. A total of 594 dengue cases were reported for the period of 19th December 2006 till 19th February 2007, which was an increase in comparison to the 5-year median but less than that reported in year 2006. However only 14 (2.3%) cases were from flood affected areas. During the flood phase, a total of 5,929 inspections were carried out at the evacuation centres with Aedes Index (AI) of 1.86%, while the post flood period showed a lower index. However Breteau Index (BI) and Container Index (CI) were higher. Preventive fogging were carried out at the evacuation centres using adulticides, thermal fogging was carried out at 21,959 premises (40.04% of inspected premises) and 350.6 L adulticides (malathion, fenitrothion and permethrin) were used. Dengue was expected to increase during flood as a result of increase Aedes potential breeding sites. However with intensive and integrated control activities, Johore was able to minimize the impact of flood for vector-borne diseases as seen from the low cases reported in flood related areas. A special guidelines for surveillance and control was developed during this flood as a reference for future occurrences.
    Matched MeSH terms: Paint
  17. Ali HR, Arifin MM, Sheikh MA, Shazili NA, Bakari SS, Bachok Z
    Mar Pollut Bull, 2014 Aug 15;85(1):287-91.
    PMID: 24934440 DOI: 10.1016/j.marpolbul.2014.05.049
    The use of antifouling paints to the boats and ships is one among the threats facing coastal resources including coral reefs in recent decades. This study reports the current contamination status of diuron and its behaviour in the coastal waters of Malaysia. The maximum concentration of diuron was 285 ng/L detected at Johor port. All samples from Redang and Bidong coral reef islands were contaminated with diuron. Temporal variation showed relatively high concentrations but no significant difference (P>0.05) during November and January (North-East monsoon) in Klang ports (North, South and West), while higher levels of diuron were detected during April, 2012 (Inter monsoon) in Kemaman, and Johor port. Although no site has shown concentration above maximum permissible concentration (430 ng/L) as restricted by the Dutch Authorities, however, long term exposure studies for environmental relevance levels of diuron around coastal areas should be given a priority in the future.
    Matched MeSH terms: Paint
  18. Hanapiah M, Zulkifli SZ, Mustafa M, Mohamat-Yusuff F, Ismail A
    Mar Pollut Bull, 2018 Feb;127:453-457.
    PMID: 29475685 DOI: 10.1016/j.marpolbul.2017.12.015
    Diuron is an alternative biocide suggested to replace organotin in formulating antifouling paints to be applied on water-going vessels hull. However, it is potentially harmful to various non-targeted marine organisms due to its toxic properties. Present study aimed to isolate, screen and identify the potential of Diuron-degrading bacteria collected from the marine sediments of Port Klang, Malaysia. Preliminary screening was conducted by exposing isolated bacteria to 430ng/L (background level), followed by 600ng/L and 1000ng/L of Diuron concentrations. Nine bacteria colonies survived the exposure of the above concentrations. However, only two strains can tolerate to survive up to 1000μg/L, which were then characterised and identified using phenotypic tests and the standard 16S rRNA molecular identification. The strains were identified as Comamonas jiangduensis SZZ 10 and Bacillus aerius SZZ 19 (GenBank accession numbers: KU942479 and KU942480, respectively). Both strains have the potential of Diuron biodegradation for future use.
    Matched MeSH terms: Paint
  19. Tamrin KF, Moghadasi K, Jalil MH, Sheikh NA, Mohamaddan S
    Materials (Basel), 2021 Apr 16;14(8).
    PMID: 33923675 DOI: 10.3390/ma14082009
    This study discloses a method for painting artwork using a CO2 laser. The continuous-wave laser beam, at a predetermined heat flux and a predetermined number of laser beam passes, mixes and displaces the plurality of colored polymer-based compositions, respectively, by way of melting and vaporizing them. Experiments showed a great accuracy of colors and designed patterns between the computer aided design (CAD) drawing and what was achieved after laser discoloration. It was found that lower values of power and speed provide sufficient energy and time to make a melt pool of colors and cause their vaporization from the surface. A detailed numerical simulation was performed to obtain a detailed understanding of the physics of laser interaction with paint using ABAQUS software. The comparative analysis indicated that the top layer of paint (including yellow and green colors) melted upon increasing cutting speed and employing one laser pass. For blue and red paints, two passes of lasers are required; in the case of red color, lower laser speed is also necessary to intensify the heat. This method can be applied for making art designs on each surface color because it is based on melting and vaporization using a laser.
    Matched MeSH terms: Paint
  20. Huynh TT, Jamil I, Pianegonda NA, Blanksby SJ, Barker PJ, Manefield M, et al.
    Microbiologyopen, 2017 04;6(2).
    PMID: 27998037 DOI: 10.1002/mbo3.425
    Microbial colonization of prepainted steel, commonly used in roofing applications, impacts their aesthetics, durability, and functionality. Understanding the relevant organisms and the mechanisms by which colonization occurs would provide valuable information that can be subsequently used to design fouling prevention strategies. Here, next-generation sequencing and microbial community finger printing (T-RFLP) were used to study the community composition of microbes colonizing prepainted steel roofing materials at Burrawang, Australia and Kapar, Malaysia over a 52-week period. Community diversity was low and was dominated by Bacillus spp., cyanobacteria, actinobacteria, Cladosporium sp., Epicoccum nigrum, and Teratosphaeriaceae sp. Cultivation-based methods isolated approximately 20 different fungi and bacteria, some of which, such as E. nigrum and Cladosporium sp., were represented in the community sequence data. Fluorescence in situ hybridization imaging showed that fungi were the most dominant organisms present. Analysis of the sequence and T-RFLP data indicated that the microbial communities differed significantly between locations and changed significantly over time. The study demonstrates the utility of molecular ecology tools to identify and characterize microbial communities associated with the fouling of painted steel surfaces and ultimately can enable the targeted development of control strategies based on the dominant species responsible for fouling.
    Matched MeSH terms: Paint/microbiology
Related Terms
Filters
Contact Us

Please provide feedback to Administrator (afdal@afpm.org.my)

External Links