  1. Mustafa AA, Matinlinna JP, Saidin S, Kadir MR
    J Prosthet Dent, 2014 Dec;112(6):1498-506.
    PMID: 24993375 DOI: 10.1016/j.prosdent.2014.05.011
    STATEMENT OF PROBLEM: The inconsistency of dentin bonding affects retention and microleakage.

    PURPOSE: The purpose of this laboratory and finite element analysis study was to investigate the effects on the formation of a hybrid layer of an experimental silane coupling agent containing primer solutions composed of different percentages of hydroxyethyl methacrylate.

    MATERIAL AND METHODS: A total of 125 sound human premolars were restored in vitro. Simple class I cavities were formed on each tooth, followed by the application of different compositions of experimental silane primers (0%, 5%, 25%, and 50% of hydroxyethyl methacrylate), bonding agents, and dental composite resins. Bond strength tests and scanning electron microscopy analyses were performed. The laboratory experimental results were validated with finite element analysis to determine the pattern of stress distribution. Simulations were conducted by placing the restorative composite resin in a premolar tooth by imitating simple class I cavities. The laboratory and finite element analysis data were significantly different from each other, as determined by 1-way ANOVA. A post hoc analysis was conducted on the bond strength data to further clarify the effects of silane primers.

    RESULTS: The strongest bond of hybrid layer (16.96 MPa) was found in the primer with 25% hydroxyethyl methacrylate, suggesting a barely visible hybrid layer barrier. The control specimens without the application of the primer and the primer specimens with no hydroxyethyl methacrylate exhibited the lowest strength values (8.30 MPa and 11.78 MPa) with intermittent and low visibility of the hybrid layer. These results were supported by finite element analysis that suggested an evenly distributed stress on the model with 25% hydroxyethyl methacrylate.

    CONCLUSIONS: Different compositions of experimental silane primers affected the formation of the hybrid layer and its resulting bond strength.

    Matched MeSH terms: Resin Cements/chemistry
  2. Elnafar AA, Alam MK, Hasan R
    J Orthod, 2014 Sep;41(3):201-7.
    PMID: 25143559 DOI: 10.1179/1465313314Y.0000000097
    The aim of this study was to assess the effects of four enamel preparation techniques on shear bond strength (SBS) of brackets bonded with a resin-modified glass ionomer cement (RMGIC). Adhesive Remnant Index (ARI) and enamel surface roughness (Ra) were also investigated after cement removal.
    Matched MeSH terms: Resin Cements/chemistry*
  3. Tapsir Z, Aly Ahmed HM, Luddin N, Husein A
    J Contemp Dent Pract, 2013 Jan 1;14(1):47-50.
    PMID: 23579892
    To evaluate and compare the microleakage of various restorative materials used as coronal barriers between endodontic appointments.
    Matched MeSH terms: Resin Cements/chemistry
  4. Baig MR, Gunaseelan R
    J Oral Implantol, 2012 Apr;38(2):149-53.
    PMID: 20932151 DOI: 10.1563/AAID-JOI-D-09-00089
    Passive fit of a long-span screw-retained implant prosthesis is an important criteria for the success of the restoration. This article describes a technique for fabricating a ceramometal implant fixed dental prosthesis (FDP) for a long-span partially edentulous situation by altering the conventional screw-retained design. The possibility of a passive fit is maximized by intraoral luting of the cast frame to milled abutments, and the potential framework distortion during fabrication is compensated to a major extent. Retrievability is ensured by screw retention of the prosthesis to the implants. Compared with conventional porcelain fused to metal screw-retained FDP, this prosthesis is relatively inexpensive to fabricate.
    Matched MeSH terms: Resin Cements/chemistry
  5. Baig MR, Rajan G
    J Oral Implantol, 2010;36(3):219-23.
    PMID: 20553176 DOI: 10.1563/AAID-JOI-D-09-00048
    Abstract This article describes the clinical and laboratory procedures involved in the fabrication of laboratory-processed, provisional, screw-retained, implant-supported maxillary and mandibular fixed complete dentures incorporating a cast metal reinforcement for immediate loading of implants. Precise fit is achieved by intraoral luting of the cast frame to milled abutments. Effective splinting of all implants is attained by the metal substructure and retrievability is provided by the screw-retention of the prosthesis.
    Matched MeSH terms: Resin Cements/chemistry
  6. Razak AA, Harrison A
    J Prosthet Dent, 1997 Apr;77(4):353-8.
    PMID: 9104710
    Dimensional accuracy of a composite inlay restoration is important to ensure an accurate fit and to minimize cementation stresses.
    Matched MeSH terms: Resin Cements/chemistry
  7. Al-Nabulsi M, Daud A, Yiu C, Omar H, Sauro S, Fawzy A, et al.
    Materials (Basel), 2019 Aug 07;12(16).
    PMID: 31394743 DOI: 10.3390/ma12162504
    Objective: To evaluate the effect of a new application method of bulk-fill flowable composite resin material on bond-strength, nanoleakage, and mechanical properties of dentine bonding agents.

    MATERIALS AND METHODS: Sound extracted human molars were randomly divided into: manufacturer's instructions (MI), manual blend 2 mm (MB2), and manual blend 4 mm (MB4). Occlusal enamel was removed and flattened, dentin surfaces were bonded by Prime & Bond universal (Dentsply and Optibond FL, Kerr). For the MI group, adhesives were applied following the manufacturer's instructions then light-cured. For MB groups, SDR flow+ bulk-fill flowable composite resin was applied in 2- or 4-mm increment then manually rubbed by a micro brush for 15 s with uncured dentine bonding agents and the mixture was light-cured. Composite buildup was fabricated incrementally using Ceram.X One, Dentsply nanohybrid composite resin restorative material. After 24-h water storage, the teeth were sectioned to obtain beams of about 0.8 mm2 for 24-h and thermocycled micro-tensile bond strength at 0.5 mm/min crosshead speed. Degree of conversion was evaluated with micro-Raman spectroscopy. Contraction gaps at 24 h after polymerization were evaluated and atomic force microscopy (AFM) nano-indentation processes were undertaken for measuring the hardness across the interface. Depth of resin penetration was studied using a scanning electron microscope (SEM). Bond strength data was expressed using two-way ANOVA followed by Tukey's test. Nanoindentation hardness was separately analyzed using one-way ANOVA.

    RESULTS: Factors "storage F = 6.3" and "application F = 30.11" significantly affected the bond strength to dentine. For Optibond FL, no significant difference in nanoleakage was found in MI/MB4 groups between baseline and aged specimens; significant difference in nanoleakage score was observed in MB2 groups. Confocal microscopy analysis showed MB2 Optibond FL and Prime & Bond universal specimens diffusing within the dentine. Contraction gap was significantly reduced in MB2 specimens in both adhesive systems. Degree of conversion (DC) of the MB2 specimens were numerically more compared to MS1 in both adhesive systems.

    CONCLUSION: Present study suggests that the new co-blend technique might have a positive effect on bond strengths of etch-and-rinse adhesives to dentine.

    Matched MeSH terms: Resin Cements
  8. Yahya, N.A., Lui, J.L., Chong, K.W.A., Abu Kasim, N.H., Radzi, Z., Lim, C.M.
    Ann Dent, 2008;15(1):11-19.
    MyJurnal
    The objective of this study was to investigate the effect of various luting cement systems on bond strength of fibre-reinforced posts to root canal dentine. 40 extracted single rooted sound premolar teeth were root filled, decoronated and randomly divided into four groups. Fibre posts, Aestheti- Plus™ (Bisco,Inc. Schaumburg, IL, USA) were cemented using four luting cements: Group A (control): Elite 100® Zinc phosphate (GC Corp, Japan), Group B: Calibra ™ Esthetic Resin Cement (Dentsply Caulk, USA), Group C: RelyX ARC Adhesive Resin (3M ESPE), Group D: RelyX Unicem Aplicap (3M ESPE). Each root was sliced into 2 discs representing the coronal and middle portions of the root canal giving rise to 20 specimens per group. Bond strength was determined using push-out tests and data was analyzed using SPSS version 14.0. The mean bond strength of Group A to Aestheti-Plus™ post was 7.71 MPa (±2.51) and Group B was 5.69 MPa (±3.23). Group C exhibited the lowest mean bond strength, 4.29 MPa (±3.53) while the highest bond strength was obtained from Group D, 7.98 MPa (±2.61). One way ANOVA showed significant interaction between all groups (p=.OOI). Post-hoc Bonferroni test reve;iled that bond strength of Group C was significantly lower compared to Group A (p=.008) and D (p=.004). In conclusion, the mean bond strength of Aestheti- Plus™ post to root canal dentine was highest when cemented with RelyX Unicem resin cement followed by Elite 100® zinc phosphate cement, Calibra and RelyX ARC resin cements. However, the bond strengths of Cali bra and RelyX Unicem resin cements were not significantly different from Elite 100® zinc phosphate cement.
    Matched MeSH terms: Resin Cements
  9. Daood U, Sauro S, Pichika MR, Omar H, Liang Lin S, Fawzy AS
    Dent Mater, 2020 01;36(1):145-156.
    PMID: 31818524 DOI: 10.1016/j.dental.2019.11.003
    OBJECTIVE: To modify a universal dentine adhesive with different concentrations of riboflavin and D-Alpha 1000 Succinate polyethylene (VE-TPGS) as a chemical enhancer and to assess the micro-tensile bond strength (24h/12 months), determine resin penetration, measurement of intermolecular interactions and cytotoxicity.

    MATERIALS AND METHODS: An experimental adhesive system based on bis-GMA, HEMA and hydrophobic monomer was doped with RF0.125 (RF - Riboflavin) or RF/VE-TPGS (0.25/0.50) and submitted to μTBS evaluation. Resin dentine slabs were prepared and examined using SEM and TEM. Adhesion force was analysed on ends of AFM cantilevers deflection. Quenched peptide assays were performed using fluorescence scanner and wavelengths set to 320nm and 405nm. Cytotoxicity was assessed using human peripheral blood mononuclear cell line. Molecular docking studies were carried out using Schrödinger small-molecule drug discovery suite 2018-2. Data from viable cell results was analyzed using one-way ANOVA. Bond strength values were analysed by two-way ANOVA. Nonparametric results were analyzed using a Kruskal-Wallis test at a 0.05 significance level.

    RESULTS: RF/VE-TPGS0.25 groups showed highest bond strength results after 24-h storage in artificial saliva (p<0.05). RF/VE-TPGS0.50 groups showed increased bond strength after 12-months of ageing. RF/VE-TPGS modified adhesives showed appreciable presence of a hybrid layer. Packing fraction indicated solid angle profiles describing well sized density and topology relations for the RF/VE-TPGS adhesives, in particular with the RF/VE-TPGS0.50 specimens. Qualitative analysis of the phenotype of macrophages was prominently CD163+ in the RF/VE-TPGS0.50. Both the compounds showed favourable negative binding energies as expressed in terms of 'XP GScore'.

    CONCLUSION: New formulations based on the incorporation of RF/VE-TPGS in universal adhesives may be of significant potential in facilitating penetration, distribution and uptake of riboflavin within the dentine surface.

    Matched MeSH terms: Resin Cements
  10. Samer MS, Faraz Q, Al-Dubai SAR, Vohra F, Abdullah H, Taiyeb-Ali TB, et al.
    Med Princ Pract, 2017;26(5):470-479.
    PMID: 28965115 DOI: 10.1159/000481864
    OBJECTIVES: The aim of this study was to determine the clinical outcomes and predictors of satisfaction in patients with lithium disilicate (LD) ceramic crowns.

    SUBJECTS AND METHODS: Clinical outcomes were assessed in 47 patients with 88 LD crowns using modified United States Public Health Service (USPHS) evaluation criteria and survival rates. The questionnaire for predictors included 3 aspects: (a) sociodemographic characteristics, (b) oral health habits (tooth brushing frequency, flossing frequency, and dental visits), and (c) satisfaction of the restorations (aesthetics, function, fit, cleansability, and chewing ability of the crowns, and overall satisfaction). Frequency distributions were computed using univariate and multivariate analysis. The Student t test and analysis of variance (ANOVA) were used to compare means across variables. Correlation analysis was done to assess the association between continuous variables.

    RESULTS: The age of crowns was 34.7 ± 9.7 months. The survival rate was 96.6% at 35.9 ± 9.2 months. There was a significant association between successful crown function and oral hygiene measures: tooth brushing (p˂ 0.001), dental visits (p = 0.006), and flossing (p = 0.009). A strong negative correlation was observed between aesthetic satisfaction (r = -0.717, p˂ 0.001) and chewing ability (r = -0.639, p˂ 0.001) with crown age. The linear regression model was significant for all predictors (p < 0.05) except overall satisfaction (p > 0.05).

    CONCLUSION: The LD crowns had long survival rates of 96.6% up to 35.9 ± 9.2 months and provided satisfactory clinical performance (low risk of failure). Oral hygiene habits such as brushing, flossing, and regular dental visits influenced patient satisfaction with LD crowns.

    Matched MeSH terms: Resin Cements
  11. Al-Maqtari AA, Lui JL
    J Prosthodont, 2010 Jul;19(5):347-56.
    PMID: 20456026 DOI: 10.1111/j.1532-849X.2010.00593.x
    The purpose of this in vitro study was to determine if packable resin composite with/without flowable resin composite has the ability to prevent coronal leakage in restored endodontic access openings following aging.
    Matched MeSH terms: Resin Cements/chemistry
  12. Purmal K, Sukumaran P
    Aust Orthod J, 2010 Nov;26(2):184-8.
    PMID: 21175030
    To investigate the shear bond strengths of buccal tubes and to determine the sites of failure.
    Matched MeSH terms: Resin Cements/chemistry
  13. Al-Makramani BMA, Razak AAA, Abu-Hassan MI
    J Prosthodont, 2008 Feb;17(2):120-124.
    PMID: 18047490 DOI: 10.1111/j.1532-849X.2007.00270.x
    PURPOSE: The current study investigated the effect of different luting agents on the fracture resistance of Procera AllCeram copings.

    METHODS: Six master dies were duplicated from the prepared maxillary first premolar tooth using nonprecious metal alloy (Wiron 99). Thirty copings (Procera AllCeram) of 0.6-mm thickness were manufactured. Three types of luting media were used: zinc phosphate cement (Elite), glass ionomer cement (Fuji I), and dual-cured composite resin cement (Panavia F). Ten copings were cemented with each type. Two master dies were used for each group, and each of them was used to lute five copings. All groups were cemented according to manufacturer's instructions and received a static load of 5 kg during cementation. After 24 hours of distilled water storage at 37 degrees C, the copings were vertically compressed using a universal testing machine at a crosshead speed of 1 mm/min.

    RESULTS: ANOVA revealed significant differences in the load at fracture among the three groups (p < 0.001). The fracture strength results showed that the mean fracture strength of zinc phosphate cement (Elite), glass ionomer cement (Fuji I), and resin luting cement (Panavia F) were 1091.9 N, 784.8 N, and 1953.5 N, respectively.

    CONCLUSION: Different luting agents have an influence on the fracture resistance of Procera AllCeram copings.

    Matched MeSH terms: Resin Cements/chemistry
  14. Mohd Zainal Abidin R, Luddin N, Shamsuria Omar N, Mohamed Aly Ahmed H
    J Clin Pediatr Dent, 2015;39(3):235-40.
    PMID: 26208068 DOI: 10.17796/1053-4628-39.3.235
    To compare the cytotoxicity of conventional GIC and Resin Modified GIC (RMGIC) polymerized at 2 different times on stem cells from human exfoliated deciduous teeth (SHED).
    Matched MeSH terms: Resin Cements/toxicity*
  15. Beh YH, Halim MS, Ariffin Z
    PeerJ, 2023;11:e16469.
    PMID: 38025677 DOI: 10.7717/peerj.16469
    BACKGROUND: This study aimed to evaluate the load capacity of maxillary central incisors with simulated flared root canal restored with different fiber-reinforced composite (FRC) post cemented with either self-adhesive or self-etch resin cement and its mode of fracture.

    METHODS: Sixty-five extracted maxillary incisors were decoronated, its canal was artificially flared and randomly categorized into group tFRC (tapered FRC post) (n = 22), mFRC (multi-FRC post) (n = 21), and DIS-FRC (direct individually shaped-FRC (DIS-FRC) post) (n = 22), which were further subdivided based on cementation resin. The posts were cemented and a standardized resin core was constructed. After thermocycling, the samples were loaded statically and the maximum load was recorded.

    RESULTS: The load capacity of the maxillary central incisor was influenced by the different FRC post system and not the resin cement (p = 0.289), and no significant interaction was found between them. Group mFRC (522.9N) yielded a significantly higher load capacity compared to DIS-FRC (421.1N). Overall, a 55% favorable fracture pattern was observed, and this was not statistically significant.

    CONCLUSION: Within the limitation of the study, it can be concluded that prefabricated FRC posts outperform DIS-FRC posts in terms of the load capacity of a maxillary central incisor with a simulated flared root canal. The cementation methods whether a self-adhesive or self-etch resin cement, was not demonstrated to influence the load capacity of a maxillary central incisor with a flared root canal. There were no significant differences between the favorable and non-favorable fracture when FRC post systems were used to restored a maxillary central incisor with a flared root canal.

    Matched MeSH terms: Resin Cements/therapeutic use
  16. Reza F, Ibrahim NS
    Eur J Dent, 2015 2 26;9(1):74-79.
    PMID: 25713488 DOI: 10.4103/1305-7456.149646
    OBJECTIVE: Fiber post is cemented to a root canal to restore coronal tooth structure. This research aims to evaluate the effect of ultraviolet (UV) irradiation on bond strength of fiber post with resin cement.

    MATERIALS AND METHODS: A total of 40 of the two types of fiber posts, namely, FRC Prostec (FRC) and Fiber KOR (KOR), were used for the experiment. UV irradiation was applied on top of the fiber post surface for 0, 15, 20, and 30 min. The irradiated surface of the fiber posts (n = 5) were immediately bonded with resin cement (Rely X U200) after UV irradiation. Shear bond strength (SBS) MPa was measured, and the dislodged area of post surfaces was examined with scanning electron microscopes. Changes in surface roughness (Ra) of the FRC group after UV irradiation were observed (n = 3) using atomic force microscopy. Data of SBS were statistically analyzed using one-way analysis of variance, followed by multiple comparisons (P < 0.05).

    RESULTS: SBS was significantly higher for 20 min of UV irradiation of the FRC group while significantly higher SBS was observed with 15 min of UV irradiation of the KOR group. Resin cement was more evident (cohesive failure) on the dislodged post surface of the UV treated groups compared with the control. The surface roughness of the FRC post was Ra = 175.1 nm and Ra = 929.2 nm for the control and the 20 min group, respectively.

    CONCLUSIONS: Higher surface roughness of the UV irradiated group indicated formation of mechanical retention on the fiber post surface. Evidence of cohesive failure was observed which indicated higher SBS of fiber post with the UV irradiated group.

    Matched MeSH terms: Resin Cements
  17. Saman SA, Chang KH, Abdullah AFL
    J Forensic Sci, 2021 Mar;66(2):608-618.
    PMID: 33202056 DOI: 10.1111/1556-4029.14625
    Abuse of solvent-based adhesives jeopardizes world population, especially the young generation. Adhesive-related exhibits encountered in forensic cases might need to be determined if they could have come from a particular source or to establish link between cases or persons. This study was aimed to discriminate solvent-based adhesives, especially to aid forensic investigation of glue sniffing activities. In this study, thirteen brands with three samples each, totaling at 39 adhesive samples, were analyzed using attenuated total reflectance-Fourier transform infrared (ATR-FTIR) spectroscopy followed by chemometric methods. Experimental output showed that adhesive samples utilized in this study were less likely to change in their ATR-FTIR profiles over time, at least up to 2 months. No interference from plastic materials was noticed based on ATR-FTIR profile comparison. Physical examination could differentiate the samples into two groups, namely contact adhesives and cement adhesives. A principal component analysis-score linear discriminative analysis (PC-score LDA) model resulted in 100% and 98.6% correct classification in discriminating the two groups of adhesive samples, forming seven discriminative clusters. Test set with adhesive samples applied glass slide and plastic substrates also demonstrated a 100% correct classification into their respective groups. As a conclusion, the method allowed for discrimination of adhesive samples based on the spectral features, displaying relationship among samples. It is hoped that this comparative information is beneficial to trace the possible source of solvent-based adhesives, whenever they are recovered from a crime scene, for forensic investigation.
    Matched MeSH terms: Resin Cements
  18. Fawzy AS, Daood U, Matinlinna JP
    Dent Mater, 2019 07;35(7):979-989.
    PMID: 31003759 DOI: 10.1016/j.dental.2019.04.001
    OBJECTIVE: This study introduced the potential and proof-of-concept of high intensity focused ultrasound (HIFU) technology for dentin-surface treatment for resin-dentin bonding without acid-aided demineralization. This new strategy could provide a way to enhance interface-integrity and bond-durability by changing the nature of dentin-substrate; bonded-interface structure and properties; and minimizing denuded-collagen exposure.

    METHODS: The interaction between HIFU waves and dentin-surface in terms of structural, mechanical and chemical variations were investigated by SEM, TEM, AFM, nano-indentation and Raman-analysis. The bonding between HIFU-treated dentin and two-step, etch-and-rinse, adhesive was preliminary explored by characterizing dentin-bound proteases activities, resin-dentin interfacial morphology and bond-durability with HIFU exposure at different time-points of 60, 90 and 120 s compared to conventional acid-etching technique.

    RESULTS: With the increase in HIFU exposure-time from 60-to-120 s, HIFU waves were able to remove the smear-layer, expose dentinal-tubules and creating textured/rough dentin surface. In addition, dentin surfaces showed a pattern of interlocking ribbon-like minerals-coated collagen-fibrils protruding from the underlaying amorphous dentin-background with HIFU exposure for 90 s and 120 s. This characteristic pattern of dentin-surface showing inorganic-minerals associated/aligned with collagen-fibrils, with 90-to-120 s HIFU-treatment, was confirmed by the Raman-analysis. HIFU-treated specimens showed higher nano-indentation properties and lower concentrations of active MMP-2 and Cathepsin-K compared to the acid-etched specimens. The resin-dentin bonded interface revealed the partial/complete absence of the characteristic hybrid-layer formed with conventional etch-and-rinse bonding strategy. Additionally, resin-infiltration and resin-tags formation were enhanced with the increase in HIFU exposure-time to 120 s. Although, all groups showed significant decrease in bond-strength after 12 months compared to 24 h storage in artificial saliva, groups exposed to HIFU for 90 s and 120 s showed significantly higher μTBS compared to the control acid-etched group.

    SIGNIFICANCE: The implementation of HIFU-technology for dental hard-tissues treatment could be of potential significance in adhesive/restorative dentistry owing to its ability of controlled, selective and localised combined tissue alteration/ablation effects.

    Matched MeSH terms: Resin Cements
  19. Fu C, Deng S, Koneski I, Awad MM, Akram Z, Matinlinna J, et al.
    J Mech Behav Biomed Mater, 2020 12;112:104082.
    PMID: 32979607 DOI: 10.1016/j.jmbbm.2020.104082
    OBJECTIVE: To investigate the effect of blue light photoactivated riboflavin modified universal adhesives on dentin collagen biodegradation resistance, dentin apparent elastic modulus, and resin-dentin bond strength with interfacial morphology.

    METHODS: Dentin slabs were treated with 0.1% riboflavin-5-phosphate modified (powder added slowly while shaking and then sonicated to enhance the dispersion process) Universal Adhesive Scotch Bond and Zipbond™ along with control (non-modified) and experimental adhesives, photoactivated with blue light for 20s. Hydroxyproline (HYP) release was assessed after 1-week storage. Elastic-modulus testing was evaluated using universal testing machine at 24 h. Resin-dentin interfacial morphology was assessed with scanning electron-microscope, after 6-month storage. 0.1% rhodamine dye was added into each adhesive and analyzed using CLSM. Detection of free amino groups was carried out using ninhydrin and considered directly proportional to optical absorbance. Collagen molecular confirmation was determined using spectropolarimeter to evaluate and assess CD spectra. For molecular docking studies with riboflavin (PDB ID file), the binding pocket was selected with larger SiteScore and DScore using Schrodinger PB software. After curing, Raman shifts in Amide regions were obtained at 8 μm levels. Data were analyzed using Two-way analysis of variance (ANOVA, p ≤ 0.05) and Tukey-Kramer multiple comparison post hoc tests.

    RESULTS: At baseline, bond strength reduced significantly (p ≤ 0.05) in control specimens. However, at 6 months' storage, UVA Zipbond™ had significantly higher μTBS. Resin was able to diffuse through the porous demineralized dentin creating adequate hybrid layers in both 0.1%RF modified adhesives in CLSM images. In riboflavin groups, hybrid layer and resin tags were more pronounced. The circular dichroism spectrum showed negative peaks for riboflavin adhesive specimens. Best fitted poses adopted by riboflavin compound are docked with MMP-2 and -9 proteases. Amide bands and CH2 peaks followed the trend of being lowest for control UA Scotch bond adhesive specimens and increasing in Amides, proline, and CH2 intensities in 0.1%RF modified adhesive specimens. All 0.1%RF application groups showed statistically significant (p resin-dentin interfacial integrity and bond strength of universal adhesive to dentin.

    Matched MeSH terms: Resin Cements
  20. Lim, Siau Peng, Fazal Reza, Zaihan Ariffin
    MyJurnal
    The purpose of this study was to evaluate hardness (indicator for polymerization) and thickness of two types of resin cement at coronal, middle and apical level of tooth root canal. Ten extracted maxillary incisors were instrumented and post space was prepared for cementation of titanium post. Samples were divided into two groups and each group was cemented either of the two types of resin cements; Panavia F [dual-cured (PF)] and Rely X Luting 2 [self-cured (RL)]. The teeth were longitudinally sectioned; hardness and thickness was measured using Vickers hardness tester and a microscope (Leica DMLM). SEM observations along the cement line at the 3 different root levels were performed. Statistical analysis was performed to test significance of differences in hardness and thickness of the two types of cement (t-test; p= 0.05) and at different levels of the same type (one-way ANOVA followed by multiple comparison; p= 0.05). Significant difference of hardness was found at the apical level between the two groups and between the coronal and apical level of PF (p0.05). Moreover, voids were more obvious within the dual-cured group of cement. Dual-cured resin cement was found to be less polymerized than self-cured type at apical level. Increased thicknesses of resin cements in comparison to post space size were observed in both groups. Use of metallic post with resin cements needs further evaluation.
    Matched MeSH terms: Resin Cements
Filters
Contact Us

Please provide feedback to Administrator (afdal@afpm.org.my)

External Links