Displaying publications 1 - 20 of 106 in total

Abstract:
Sort:
  1. Allmers H
    Contact Derm., 2001 Jan;44(1):30-3.
    PMID: 11156008
    72 subjects reporting symptoms indicating Type I hypersensitivity reactions to natural rubber latex (NRL) gloves were included in this study. 44 of them had a positive prick test to NRL. They underwent wearing tests using 2 types of NRL gloves with high (n=63) and low (n=70) allergen contents. Unigloves Malaysia with a high allergen content caused positive skin reactions in 47% of SPT-positive and no IgE-negative subjects. After application of Hand Sense skin protection cream, the frequency of positive skin responses in wearing tests decreased to 30% in prick-test-positive subjects. The Biogel Diagnostic gloves with low allergen caused hypersensitivity with and without Hand Sense in 2 cases (5%) of the prick-test-positive. 60% of all test participants had a positive prick test to NRL. No prick-test-negative subjects showed any urticaria during the glove-wearing test. Our study demonstrates that high allergen contents in latex gloves frequently elicit skin responses in NRL-sensitized subjects. Since other skin protection creams have shown to increase allergic symptoms, it is encouraging to report that Hand Sense skin cream may hamper the uptake of allergens from gloves, thus decreasing allergic reactions.
    Matched MeSH terms: Latex Hypersensitivity/etiology; Latex Hypersensitivity/prevention & control*
  2. Dazylah Darji, Ma'zam Md Said
    MyJurnal
    Epoxidised Natural Rubber (ENR) is now a commercially available polymer produced by chemical modification of natural rubber. Currently, three types of ENR are commercially available, and these are ENR 10, ENR 25, and ENR 50 with 10%, 25%, and 50% mol epoxidation, respectively. Studies on prevulcanisation of ENR 50 and postvulcanisation of the latex films were carried out. The objective of this study was to develop ENR 50 that could be dipped easily in coagulant dipping solution to produce dipped products. Several attempts were made by compounding prevulcanised ENR 50 at various sulphur levels ranging from 0.5 to 3.0 pphr. Using suitable coagulant dipping systems, ENR 50 film could be formed despite the high contents of non-ionic surfactant. It was found that the tensile strength of prevulcanised ENR 50 film decreased with the increase in the sulphur level. The results show that as level of sulphur increased, M300 also increased to an optimum value of 1.5 pphr of sulphur. For the postvulcanised ENR 50 film, however, the tensile strength increased and then decreased with the increasing sulphur level. Meanwhile M300 increased with the increasing postvulcanization time and sulphur level. The postvulcanisation of ENR 50 film seems to be a more effective way of increasing tensile properties than by prevulcanisation of ENR 50.
    Matched MeSH terms: Latex
  3. Rohaida Abd Rahman, Faridah Afandi, Tun Maizura Mohd Fathullah, Rafeezul Mohamed
    MyJurnal
    The National Blood Center, Kuala Lumpur interprets laboratory results for the von Willebrand factor (vWF) profile based on guidelines provided by the U.S. National Heart, Lung, and Blood Institute, which were established based on the Caucasian population [1-2]. The vWF profiles among the Malay population has not yet been established.

    The goals of this study were to determine the vWF profiles of the different ABO blood types among Malays and to evaluate their association with demographic characteristics and smoking habits.

    One hundred and forty Malay donors participated in this study. Factor VIII (FVIII), vWF antigen, and ristocetin cofactor (RiCof) levels and collagen binding activity (CBA) were measured by coagulometric clot detection, latex agglutination, and enzyme-linked immunosorbent assay.
    Matched MeSH terms: Latex
  4. Naji, H.R., Sahri, M.H., Bakar, E.S., Soltani, M., Hamid, H.A.
    ASM Science Journal, 2014;8(1):36-43.
    MyJurnal
    Wood density and types of shrinkage were examined in two rubberwood latex timber clones of rubber (Hevea brasiliensis) namely RRIM 2020 and RRIM 2025, planted at densities of 500, 1000, 1500, and 2000 trees/ha, within a trial plot. The mean wood density showed a low descending trend towards high planting densities in both clones. Wood density was significantly and negatively correlated with planting density. The strength of correlation was moderate. The mean longitudinal shrinkage in both clones and tangential shrinkages in clone RRIM 2020 showed no significant difference among planting densities. The tangential (in RRIM 2025), radial and volumetric shrinkages in both clones decreased from low to high planting densities and the differences were more pronounced between densities of 500 trees/ha and 2000 trees/ha. The magnitudes of correlation between these shrinkages and planting density were low. The regression models indicated that wood density could be more ascribed by planting density followed by volumetric shrinkage. This study exhibited low variations in wood density and shrinkages among clones and the respective planting densities; however, RRIM 2025 was more stable than RRIM 2020.
    Matched MeSH terms: Latex
  5. Samrot AV, Saigeetha S, Mun CY, Abirami S, Purohit K, Cypriyana PJJ, et al.
    Sci Rep, 2021 12 31;11(1):24511.
    PMID: 34972829 DOI: 10.1038/s41598-021-03328-2
    Latex, a milky substance found in a variety of plants which is a natural source of biologically active compounds. In this study, Latex was collected from raw Carica papaya and was characterized using UV-Vis, FTIR and GC-MS analyses. Super Paramagnetic Iron Oxide Nanoparticles (SPIONs) were synthesized, coated with C. papaya latex (PL-Sp) and characterized using UV-Vis, FT-IR, SEM-EDX, XRD, VSM and Zeta potential analyses. SPIONs and latex coated SPIONs (PL-Sp) were used in batch adsorption study for effective removal of Methylene blue (MB) dye, where (PL-Sp) removed MB dye effectively. Further the PL-Sp was used to produce a nanoconjugate loaded with curcumin and it was characterized using UV-Vis spectrophotometer, FT-IR, SEM-EDX, XRD, VSM and Zeta potential. It showed a sustained drug release pattern and also found to have good antibacterial and anticancer activity.
    Matched MeSH terms: Latex/chemistry*
  6. Jutarut Iewkittayakorn, Juntima Chungsiriporn, Prukraya Pongyeela
    Sains Malaysiana, 2017;46:1763-1769.
    Ammonium-enriched skim latex serum - used for absorption of contaminating ammonia gas - when composted with other rubber tree wastes, is promising as a good compost. The objective of this research was to utilize ammonium-enriched skim latex serum (S) as a raw composting ingredient after being combined with para sawdust (W1) and para rubber leaves (W2). Several ratios of S, W1 and W2 were experimented in a 15L composting vessel to determine the most effective compost. The best ratio was found to be 3:1:3 by weight at 12-day retention. The modified 30 L composting reactor employed with the derived optimum mixing conditions yielded N, P and K of 2.40, 1.51 and 14.84 %w/w. The growth of Brassica alboglabra after application of this compost combined with a chemical fertilizer generated the highest fresh weight (4.48 g/plant). Thus, compost from these wastes could be used as a fertilizer and logically should contribute to cost saving of waste disposal.
    Matched MeSH terms: Latex
  7. Habib MAH, Gan CY, Abdul Latiff A, Ismail MN
    Biochem. Cell Biol., 2018 12;96(6):818-824.
    PMID: 30058361 DOI: 10.1139/bcb-2018-0020
    The natural rubber latex extracted from the bark of Hevea brasiliensis plays various important roles in modern society. Post-translational modifications (PTMs) of the latex proteins are important for the stability and functionality of the proteins. In this study, latex proteins were acquired from the C-serum, lutoids, and rubber particle layers of latex without using prior enrichment steps; they were fragmented using collision-induced dissociation (CID), higher-energy collisional dissociation (HCD), and electron-transfer dissociation (ETD) activation methods. PEAKS 7 were used to search for unspecified PTMs, followed by analysis through PTM prediction tools to crosscheck both results. There were 73 peptides in 47 proteins from H. brasiliensis protein sequences derived from UniProtKB were identified and predicted to be post-translationally modified. The peptides with PTMs identified include phosphorylation, lysine acetylation, N-terminal acetylation, hydroxylation, and ubiquitination. Most of the PTMs discovered have yet to be reported in UniProt, which would provide great assistance in the research of the functional properties of H. brasiliensis latex proteins, as well as being useful biomarkers. The data are available via the MassIVE repository with identifier MSV000082419.
    Matched MeSH terms: Latex/metabolism*; Latex/chemistry
  8. Abu Bakar MF, Kamerkar U, Abdul Rahman SN, Muhd Sakaff MKL, Othman AS
    Data Brief, 2020 Oct;32:106188.
    PMID: 32904357 DOI: 10.1016/j.dib.2020.106188
    Hevea brasiliensis is exploited for its latex production, and it is the only viable source of natural rubber worldwide. The demand for natural rubber remains high due its high-quality properties, which synthetic rubber cannot compete with. In this paper, we present transcriptomic data and analysis of three H. brasiliensis clones using tissue from latex and bark tissues collected from 10-year-old plant. The combined, assembled transcripts were mapped onto an H. brasiliensis draft genome. Gene ontology analysis showed that the most abundant transcripts related to molecular functions, followed by biological processes and cellular components. Simple sequence repeats (SSR) and single nucleotide polymorphisms (SNP) were also identified, and these can be useful for selection of parental and new clones in a breeding program. Data generated by RNA sequencing were deposited in the NCBI public repository under accession number PRJNA629890.
    Matched MeSH terms: Latex
  9. Rohani Abu Bakar, Asrul Mustafa
    MyJurnal
    Adhesives serve many functions in daily life, starting from sticking envelopes to rejoining broken
    materials. Adhesives are usually developed for a specific purpose and the performances can vary
    according to their specific end-use. Most of the commercially available adhesives comprised nonrenewable or petroleum derived raw materials. Thus, in order to mitigate negative impact of using nonrenewable material as the raw material for adhesives, a new type of adhesive containing epoxidised
    natural rubber (NR) latex is developed. Epoxidised NR latex adhesive was initially prepared and pigment
    was subsequently added to produce desired colours of the adhesive. Hence, the newly developed adhesive
    can serve as adhesive and also as paint for art. The adhesives were characterised and the results indicated
    that they were free from heavy metal contents and volatile organic compounds (VOCs). The adhesives
    exhibited comparable odour concentration to commercial synthetic-based adhesive. In terms of toxicity
    level, the adhesive developed exhibited low acute oral toxicity. Peel adhesion test of A4 and drawing
    papers on stainless steel and glass substrates, opacity and glossiness were also investigated in the present
    study. This coloured adhesive is deemed to support the STEM (science, technology, engineering and
    mathematics) learning by indirectly imparting polymer science and technology in art education and
    further promotes creative learning among school children. The adhesive is also derived from renewable
    material rendering it more environmentally friendly.
    Matched MeSH terms: Latex
  10. Abdul Samad S, Yusoff H, Fadilah SAW
    Med J Malaysia, 2001 Mar;56(1):32-8.
    PMID: 11503293
    A biotin-avidin-linked immunosorbent assay was developed to detect Aspergillus antigens in sera of immunocompromised patients. The assay was based on a double antibody sandwich ELISA using polyclonal antibodies raised against water-soluble antigens of Aspergillus fumigatus. Aspergillus antigens were positive in sera of 9 of 16 (56%) patients who were studied prospectively and in 13 of 73 (19%) patients studied retrospectively. The 9 prospectively studied patients who were antigen positive were febrile neutropenic hematological malignancy patients who exhibited a high risk of acquiring invasive aspergillosis.
    Matched MeSH terms: Latex Fixation Tests
  11. Lau NS, Makita Y, Kawashima M, Taylor TD, Kondo S, Othman AS, et al.
    Sci Rep, 2016 06 24;6:28594.
    PMID: 27339202 DOI: 10.1038/srep28594
    Hevea brasiliensis Muell. Arg, a member of the family Euphorbiaceae, is the sole natural resource exploited for commercial production of high-quality natural rubber. The properties of natural rubber latex are almost irreplaceable by synthetic counterparts for many industrial applications. A paucity of knowledge on the molecular mechanisms of rubber biosynthesis in high yield traits still persists. Here we report the comprehensive genome-wide analysis of the widely planted H. brasiliensis clone, RRIM 600. The genome was assembled based on ~155-fold combined coverage with Illumina and PacBio sequence data and has a total length of 1.55 Gb with 72.5% comprising repetitive DNA sequences. A total of 84,440 high-confidence protein-coding genes were predicted. Comparative genomic analysis revealed strong synteny between H. brasiliensis and other Euphorbiaceae genomes. Our data suggest that H. brasiliensis's capacity to produce high levels of latex can be attributed to the expansion of rubber biosynthesis-related genes in its genome and the high expression of these genes in latex. Using cap analysis gene expression data, we illustrate the tissue-specific transcription profiles of rubber biosynthesis-related genes, revealing alternative means of transcriptional regulation. Our study adds to the understanding of H. brasiliensis biology and provides valuable genomic resources for future agronomic-related improvement of the rubber tree.
    Matched MeSH terms: Latex/biosynthesis*
  12. Czuppon AB, Chen Z, Rennert S, Engelke T, Meyer HE, Heber M, et al.
    J Allergy Clin Immunol, 1993 Nov;92(5):690-7.
    PMID: 8227860
    BACKGROUND: Allergy to latex-containing articles is becoming more and more important because it can result in unexpected life-threatening anaphylactic reactions in sensitized individuals.

    METHODS: A protein of 58 kd with an isoelectric point of 8.45 was purified from raw latex and from latex gloves and identified as the major allergen, completely blocking specific IgE antibodies in the serum of latex-sensitized subjects. The allergen is a noncovalent homotetramer molecule, in which the 14.6 kd monomer was identified, by amino acid composition and sequence homologies of tryptic peptides, to be the rubber elongation factor found in natural latex of the Malaysian rubber tree.

    RESULTS: Competitive immunoinhibition tests showed that the starch powder covering the finished gloves is the airborne carrier of the allergen, resulting in bronchial asthma on inhalation. The purified allergen can induce allergic reactions in the nanogram range.

    CONCLUSION: The identification of the allergen (Hev b I) may help to eliminate it during the production of latex-based articles in the future.

    Matched MeSH terms: Latex/adverse effects*
  13. Hasma H, Subramaniam A
    Lipids, 1978 Dec;13(12):905-7.
    PMID: 27520427 DOI: 10.1007/BF02533847
    Methyl esters from the triglyceride fraction of the neutral lipids of natural rubber latex were found by gas liquid chromatography to contain about 90% of a furanoid acid. Spectroscopic analysis identified the acid as 10,13-epoxy-11-methyloctadeca-10,12-dienoic acid.
    Matched MeSH terms: Latex
  14. Yip E, Cacioli P
    J Allergy Clin Immunol, 2002 Aug;110(2 Suppl):S3-14.
    PMID: 12170237 DOI: 10.1067/mai.2002.124499
    Gloves that will provide a barrier of protection from infectious organisms are an essential feature of medical practice for the protection of both patients and medical personnel. Natural rubber latex has consistently been the most satisfactory raw material for the manufacture of gloves. Certain latex proteins, carried over into the finished product by inadequate manufacturing processes, may pose a risk of provoking allergic reactions in some patients and medical workers. As with any allergy, the risk depends on the route of exposure and dose. Hence, the method of manufacture, including the means used to coat gloves to make donning easy, can influence the eventual exposure of sensitive people to latex allergens. In this article, we describe the several processes in use and their effects on latex protein content.
    Matched MeSH terms: Latex/immunology; Latex/isolation & purification
  15. Ahmad Nazrun Shuid, Mohd Syukri Anwar, Ahmad Asmadi Yusof
    MyJurnal
    This study was carried out to compare the rate of burn wound healing with the applications of the latex of Carica papaya Linn. (papaya) or of silver sulfadiazine cream (SSD). Partial and full thickness burn wound (2 cm x 2 cm) was induced on the dorsal part of anaesthetized rats by using heated metal plates. The rats were divided into three groups, i.e. untreated group and groups treated daily with SSD and papaya latex, respectively. A digital camera was used to take photographs of the burn wounds daily to monitor their healing. It was found that there was no significant difference in the healing time of papaya latex treated group compared to the SSD treated group. Papaya latex contained digestive enzymes which might clean burn wounds but might also cause wound bleeding in a few rats of the papaya latex group.
    Matched MeSH terms: Latex
  16. Kathleen J. Jalani, Razuan Hilmi Md Sulji, Hannis Fadzillah Mohsin, Ibtisam Abdul Wahab
    ESTEEM Academic Journal, 2019;15(1):18-24.
    MyJurnal
    Aloe vera which is also known as Aloe barbadensis Miller,is a plant that is commonly used for medicinal purposes and as treatments for various health issues. It produces two substances; gel and latex, which are used for commercial household products, halal food and cosmetics. Aloe gel is the clear, jelly-like substance found in the inner part of the Aloe leaf while Aloe’s yellow latex comes from the peel. Aloe vera is able to provide therapeutic effects such as wound healing, anti-inflammatory, antioxidant, laxative and antimicrobial properties. The objective of this study was to
    investigate the extracts via spectrophotometry (λ = 200 – 400 nm) and liquid chromatography. After 21 days, the ultraviolet spectra showed the evidence of the water molecules interactions and the hydroxyl groups in hydroalcoholic extracts. Significant peaks were also observed in the chromatograms. Further studies evaluating the stability of A. vera extracts should be carried out.
    Matched MeSH terms: Latex
  17. Irnidayanti Y, Soegianto A, Brabo AH, Abdilla FM, Putranto TWC, Payus CM
    Bull Environ Contam Toxicol, 2023 Sep 13;111(3):37.
    PMID: 37704797 DOI: 10.1007/s00128-023-03786-6
    This study examined the characteristics of microplastics (MPs) in the gills and gastrointestinal tract (GIT) of mackerel (Rastrelliger kanagurta) captured in Jakarta Bay, Indonesia. All 120 fish contained MPs, with fragment > fiber > film being the most prevalent types, in that order. The total abundances of fragments, fibers, and films in the gills were as follows: 4.8 ± 1.6, 1.0 ± 0.7, and 0.3 ± 0.3, respectively. The total abundances of fragments, fibers, and films in the GIT were 5.9 ± 2.3, 1.3 ± 0.8, and 0.4 ± 0.4, respectively. Statistical analysis showed that the abundance of fragments, fibers and films in both the gills and GIT of mackerel did not differ significantly between sampling locations. In the gills and GIT, MPs with sizes less than 0.1 mm and MPs that were black in color were most prevalent. Fourier transform infrared (FTIR) spectroscopy tests on MPs from the tissues of mackerel showed that there were 8 different types of MP polymers, namely, latex, nylon, polymethyl methacrylate (PMMA), cellulose acetate (CA), polyurethane (PU), polycarbonate (PC), polystyrene (PS), and polytetrafluoroethylene (PTFE). Latex and polycarbonate were detected in fish samples from Jakarta Bay.
    Matched MeSH terms: Latex
  18. Yeang HY, Cheong KF, Sunderasan E, Hamzah S, Chew NP, Hamid S, et al.
    J Allergy Clin Immunol, 1996 Sep;98(3):628-39.
    PMID: 8828541 DOI: 10.1016/s0091-6749(96)70097-0
    Two major water-insoluble proteins are located on the surface of rubber particles in Hevea brasiliensis latex. A 14.6 kd protein (Hev b 1), found mainly on large rubber particles (> 350 mm in diameter), and a 24 kd protein (Hev b 3), found mainly on small rubber particles (average diameter, 70 nm), are recognized by IgE from patients with spina bifida and latex allergy. Although Hev b 1 (also called the rubber elongation factor [REF]) has previously been reported as a major latex allergen, this conclusion has been disputed on the basis of results from other studies. The allergenicity of Hev b 1 is verified in this study by testing the recombinant protein generated from its gene. Because allergenicity is confined to patients with spina bifida and not observed in adults sensitive to latex, it is not a major latex allergen. The identification of Hev b 3 as another allergen originating from rubber particles is confirmed by immunogold labeling and electron microscopy. Observations with the monoclonal antibody USM/RC2 developed against Hev b 3 show that the protein has a tendency to fragment into several polypeptides of lower molecular weight (from 24 kd to about 5 kd) when stored at -20 degrees C. There is also indication of protein aggregation from the appearance of proteins with molecular weights greater than 24 kd. Fragmentation of Hev b 3 is induced immediately on he addition of latex B-serum, which is normally compartmentalized in the lutoids in fresh latex. In the preparation of ammoniated latex (used for the manufacture of latex products), the lutoids are ruptured, and the released B-serum reacts with Hev b 3 on the rubber particles to give rise to an array of low molecular weight polypeptides that are allergenic to patients with spina bifida.
    Matched MeSH terms: Latex/immunology*; Latex/metabolism; Latex/chemistry
  19. Chai CK, Md. Soot Ahmad, Wan Manshol W. Zin
    Electron beam vulcanization of natural rubber latex has been developed as an alternative to the conventional sulphur vulcanization method. This study aimed at determining the effect of electron beam dose, beam current and centrifugation to the tensile properties of field natural rubber latex. Irradiation dose and beam current ranged from 50 to 300 kGy and 1 to 15 mA respectively. The determination of tensile properties were done on cast film prepared from irradiated field latex before and after centrifugation. It was found that tensile properties increased with radiation dose but decreased with beam current. Rubber films made from centrifuged irradiated field latex were softer and showed higher tensile strength.
    Matched MeSH terms: Latex
  20. Sofian Ibrahim, Keong, Chai Chee, Ratnam, Chantara Thevy, Khairiah Badri
    ASM Science Journal, 2018;11(2):67-75.
    MyJurnal
    Radiation pre-vulcanised natural rubber latex (RVNRL) prepared by using gamma irradiation technique has many advantages over the conventionally prepared sulphur pre-vulcanised natural rubber latex (SPVL). Despite the fact that many potential latex dipped products can be made from RVNRL, little effort was made to fully commercialise the products because of the inferior strength of RVNRL products compared to SPVL products. An attempt was made to improve the tensile strength of RVNRL by combining both radiation and peroxide vulcanisation in order to ensure that the products will not tear or fail, and has sufficient stretch. Hexanediol diacrylate (HDDA) plays the main role as sensitizer during radiation vulcanisation and tert-butyl hydroperoxide (t-BHPO) as the co-sensitizer in peroxide vulcanisation. Pre-vulcanised natural rubber latex dipped films via hybrid radiation and peroxidation vulcanisations obtained showed tensile strength of 26.7 MPa, an increment of more than 15% compared to controlled film (22.5 MPa). Besides, the crosslink percentage of the rubber films also showed around 5% increment from 90.7% to 95.6%.
    Matched MeSH terms: Latex
Filters
Contact Us

Please provide feedback to Administrator (afdal@afpm.org.my)

External Links