  1. Febriyenti, Azmin Mohd. Noor, Saringat Baei
    MyJurnal
    The objective of this research was to formulate an aerosol concentrate containing haruan (Channa
    striatus) water extract that would produce a thin film when sprayed onto a wound and could be used for wound dressing. The aerosol concentrates were formulated with various polymer and plasticiser mixtures and tested in dispersion systems. The polymers evaluated were hydroxypropyl methylcellulose (HPMC), carboxymethylcellulose sodium (CMC Sodium), acacia, tragacanth, chitosan, gelatine and gelatine (bloom 151–160), all at concentrations of 2%. The plasticisers evaluated were polyethylene glycol (PEG) 400 and 4000, glycerine, propylene glycol, and triacetin. Films were prepared from film-forming dispersions by casting techniques. Film-forming dispersions were characterised in terms of pH, density, surface tension, rheological properties, particle size distribution, and tackiness. Based on these evaluations, HPMC was chosen as the best polymer. It produced a film with the expected qualities and was easy to reproduce in the form of dispersions or as thin transparent films. Glycerine was judged as the most appropriate plasticiser because it produced the concentrate having the desired qualities and properties expected from an aerosol concentrate.
  2. Laila L, Febriyenti F, Salhimi SM, Baie S
    Int Wound J, 2011 Oct;8(5):484-91.
    PMID: 21722317 DOI: 10.1111/j.1742-481X.2011.00820.x
    Haruan (Channa striatus) is a type of fresh water fish in Malaysia that is known to promote wound healing. Haruan water extract has been formulated in an aerosol system which can produce a film for wound dressing. As topical preparation, Haruan spray needs to be evaluated in terms of the possibility to cause irritation reaction or toxic response. Three experiments were carried out to evaluate the safety of Haruan spray which are Primary Skin Irritation test, Intracutaneous test and Systemic Injection test. The result shows that Haruan spray gave no significant responses to all the above tests. The investigation of the effect of Haruan spray as wound dressing in the healing process was performed in Sprague-Dawley rats where 6-cm long full-thickness incision wound and burn wound were made on the back of the animals. Haruan spray was tested and compared with blank formula as control. Tensile strength test of treated wound was carried out at the 3rd, 6th, 9th and 12th day after wounding and treatment. The burn wounds contraction was measured daily for 21 days. Results showed that haruan water extract spray formula is not only effective but also safe for application to both incision and burn wounds.
Related Terms
Filters
Contact Us

Please provide feedback to Administrator (afdal@afpm.org.my)

External Links