Displaying 1 publication

Abstract:
Sort:
  1. SH, Ku, YS, Tan, Yahya NA
    Ann Dent, 2014;21(1):25-32.
    MyJurnal
    The study aimed to evaluate the quality of the hybrid
    layer form by three different adhesive systems. Class V
    cavities were prepared on the buccal surface of fourty
    extracted human premolars. The prepared teeth were
    randomly assigned into four groups according to the
    adhesive system and application mode. The systems
    were: Optibond S (OS, total-etch); Optibond Versa (OV,
    two-bottles, self-etch); Single Bond Universal (SBU,
    one-bottle, self-etch) and Single Bond Universal with
    etchant (SBU + etchant). All cavities were restored with
    composite (Filtek Z350XT). The samples were sectioned,
    polished and pretreated to remove minerals, protein
    and water prior to SEM evaluation. From the images,
    thickness of the hybrid layers was measured. Present of
    resin tags and adaptation failure were also recorded. The
    data obtained were analyzed using ANOVA, Dunnett’s
    T3, Kruskal-Wallis and Mann-Whitney tests. OS group
    showed the highest average hybrid layer thickness (4.34
    µm), followed by SBU + etchant (3.06 µm), OV (1.91 µm)
    and SBU (0.95 µm). Both adhesive and cohesive failures
    were observed in SBU group. Present of prominent resin
    tags were seen in both OS and OV groups. In conclusion,
    all the investigated adhesive systems were able to perform
    distinguishable actions as shown in micro-morphological
    alteration and hybrid layer thickness. Two-bottles, selfetch
    adhesive (OV) was proven to produce negligible
    adaptation failure compared to other adhesive systems in
    the present study. Combined all-in-one adhesive (SBU)
    was found to render a superior bonding performance in
    total-etch mode comparing to self-etch mode.