Displaying all 7 publications

Abstract:
Sort:
  1. Ishak KA, Velayutham TS, Annuar MSM, Sirajudeen AAO
    Int J Biol Macromol, 2021 Feb 01;169:311-320.
    PMID: 33340632 DOI: 10.1016/j.ijbiomac.2020.12.090
    Dielectric spectroscopy is employed to study the relaxation phenomena in natural polyhydroxyalkanoates (PHAs) upon temperature and frequency variations. Effects of PHAs molecular structure on the relaxation, arising from the differences in monomeric composition, are investigated under identical conditions in a frequency range of 10-2-106 Hz, and at different temperatures. All PHA samples showed different dielectric response at different temperature. Primary α-relaxation signals are observed at temperature corresponding to the glass transition temperature. On the other hand, secondary β- and γ-relaxations are detected at low temperatures, and attributed to local motions of polar groups and small segments of the polymer chain. The dielectric properties of representative PHA samples are compared and discussed.
  2. Hassan SH, Velayutham TS, Chen YW, Lee HV
    Int J Biol Macromol, 2021 Jun 01;180:392-402.
    PMID: 33737185 DOI: 10.1016/j.ijbiomac.2021.03.066
    The present work focuses on the development of cellulose nanofibrils (CNF) film that derived from sustainable biomass resources, which potentially to work as bio-based conductive membranes that assembled into supercapacitors. The chemically purified cellulose was isolated from different parts of coconut (coconut shell and its husk) and further subjected to 2,2,6,6-tetramethylpiperidine-1-oxyl radical (TEMPO)-mediated oxidation for CNF preparation. Physicochemical properties of prepared CNFs were studied in terms of chemical characteristics & crystallinity, surface functionalities, surface morphology, and thermal properties. Both coconut shell-derived CNF and coconut husk-derived CNF fulfilled with nanocellulose's characteristics with fibres width ranged of 70-120 nm and 150-330 nm, respectively. CNF films were further prepared by solvent casting method to measure the modulus elasticity, piezoelectric and dielectric properties of the films. Mechanical study indicated that coconut shell-derived CNF film showed a higher value of elastic modulus than the coconut husk-derived CNF film, which was 8.39 GPa and 5.36 GPa, respectively. The effectiveness of electrical aspects for CNF films are well correlated with the crystallinity and thermal properties, associated with it's composition of different coconut's part.
  3. Velayutham TS, Ng BK, Gan WC, Abd Majid WH, Hashim R, Zahid NI, et al.
    J Chem Phys, 2014 Aug 28;141(8):085101.
    PMID: 25173043 DOI: 10.1063/1.4893873
    Glycolipid, found commonly in membranes, is also a liquid crystal material which can self-assemble without the presence of a solvent. Here, the dielectric and conductivity properties of three synthetic glycolipid thin films in different thermotropic liquid crystal phases were investigated over a frequency and temperature range of (10(-2)-10(6) Hz) and (303-463 K), respectively. The observed relaxation processes distinguish between the different phases (smectic A, columnar/hexagonal, and bicontinuous cubic Q) and the glycolipid molecular structures. Large dielectric responses were observed in the columnar and bicontinuous cubic phases of the longer branched alkyl chain glycolipids. Glycolipids with the shortest branched alkyl chain experience the most restricted self-assembly dynamic process over the broad temperature range studied compared to the longer ones. A high frequency dielectric absorption (Process I) was observed in all samples. This is related to the dynamics of the hydrogen bond network from the sugar group. An additional low-frequency mechanism (Process II) with a large dielectric strength was observed due to the internal dynamics of the self-assembly organization. Phase sensitive domain heterogeneity in the bicontinuous cubic phase was related to the diffusion of charge carriers. The microscopic features of charge hopping were modelled using the random walk scheme, and two charge carrier hopping lengths were estimated for two glycolipid systems. For Process I, the hopping length is comparable to the hydrogen bond and is related to the dynamics of the hydrogen bond network. Additionally, that for Process II is comparable to the bilayer spacing, hence confirming that this low-frequency mechanism is associated with the internal dynamics within the phase.
  4. Hashim R, Zahid NI, Velayutham TS, Aripin NFK, Ogawa S, Sugimura A
    J Oleo Sci, 2018 Jun 01;67(6):651-668.
    PMID: 29760332 DOI: 10.5650/jos.ess17261
    Also recognized as carbohydrate liquid crystals, glycolipids are amphiphiles whose basic unit comprises of a sugar group attached to an alkyl chain. Glycolipids are amphitropic, which means these materials form liquid crystal self-assemblies when dry (thermotropic) as well as when dissolved in solvents (lyotropic/surfactants) such as water. Many glycolipids are also naturally derived since these can be found in cell membranes. Their membrane and surfactant functions are largely understood through their lyotropic properties. While glycolipids are expected to play major roles as eco-friendly surfactants in the global surfactant market, their usefulness as thermotropic liquid crystal material is, to date, unknown, due to relatively lack of research performed and data reported in the literature. Understandably since glycolipids are hygroscopic with many hydroxy groups, removing the last trace water is very challenging. In recent time, with careful lyophilization and more consistent characterization technique, some researchers have attempted serious studies into "dry" or anhydrous glycolipids. Motivated by possible developments of novel thermotropic applications, some results from these studies also provide surprising new understanding to support conventional wisdom of the lyotropic systems. Here we review the dry state of glycosides, a family of glycolipids whose sugar headgroup is linked to the lipid chain via a glycosidic oxygen linker. The structure property relationship of both linear and anhydrous Guerbet glycosides will be examined. In particular, how the variation of sugar stereochemistry (e.g. anomer vs. epimer), the chain length and chain branching affect the formation of thermotropic liquid crystals phases, which not only located under equilibrium but also far from equilibrium conditions (glassy phase) are scrutinized. The dry glycolipid assembly has been subjected to electric and magnetic fields and the results show interesting behaviors including a possible transient current generation.
  5. Ng CYB, Gan WC, Velayutham TS, Goh BT, Hashim R
    Phys Chem Chem Phys, 2020 Jan 29;22(4):2414-2423.
    PMID: 31939468 DOI: 10.1039/c9cp01556f
    The effects of solvents and temperature on the crystal formation were investigated for vinylidene fluoride/trifluoroethylene copolymer P(VDF-TrFE). Highly crystalline P(VDF-TrFE) thin films were fabricated by spin-casting using various polar solvents such as diethyl carbonate (DEC), methyl ethyl ketone (MEK), N,N-dimethylformamide (DMF) and dimethyl sulfoxide (DMSO). Ferroelectric polarisation reversal of the P(VDF-TrFE) was evidenced by a displacement (D)-electric field (E) hysteresis loop measurement and supported by the presence of pyroelectric activity. The samples which were annealed above 100 °C gave elongated rod-like crystalline structures and the highest crystallinity, Xc of 83% was formed at 120 °C. Consequently, remnant polarisation (85 mC m-2) and the pyroelectric coefficient (30 μC m-2 K-1) were enhanced. Thus, annealing plays a substantial role in controlling the crystalline structure of P(VDF-TrFE) films regardless of the choice of solvent. Although, the crystalline structure control is almost independent of the solvent's polarity, the choice of solvent is essential in preparing a smoother film surface. Molecular dynamics of P(VDF-TrFE) are discussed from the observation of two dielectric relaxation processes, β and γ related to the segmental micro-Brownian and local modes, respectively. The complete ferroelectric polarization reversal caused a reduction in the dielectric polarization and reduced the lattice spacing of the 110/200 planes.
  6. Gopal SR, Velayutham TS, Gan WC, Cheong JY, Soh AE
    RSC Adv, 2023 Mar 08;13(12):7921-7928.
    PMID: 36909754 DOI: 10.1039/d3ra00077j
    A hybrid piezo/triboelectric nanogenerator (H/P-TENG) is designed for mechanical energy harvesting using polymer ceramic composite films; polydimethylsiloxane/Ba(Zr0.2Ti0.8)O3-0.5(Ba0.7Ca0.3)TiO3 (PDMS/BZT-BCT) and polyvinyl alcohol (PVA). A lead-free BZT-BCT piezoelectric ceramic was prepared via solid-state method and blended into PDMS to form a series of polymer-ceramic composite films, ranging from 5% to 30% by weight. The films were forward/reverse poled with corona poling and their electrical properties were compared to non-poled samples. The H/P-TENG constructed with forward-poled 15 wt% BZT-BCT in PDMS achieved the highest open-circuit voltage, V oc of 127 V, short-circuit current density, J sc of 67 mA m-2, short-circuit charge density, Q sc of 118 μC m-2, and peak power density of 7.5 W m-2, an increase of 190% over pristine PDMS-based TENG. It was discovered that incorporating BZT-BCT into the PDMS matrix improved the triboelectric properties of PDMS. The overlapping electron cloud (OEC) model was used to explain the enhancement and the effect of poling direction of the PDMS/BZT-BCT composite used in H/P-TENG, providing fundamental knowledge of the influence of piezoelectric polarisation on contact electrification.
  7. Velayutham TS, Nguan HS, Ng BK, Gan WC, Manickam Achari V, Zahid NI, et al.
    Phys Chem Chem Phys, 2016 06 01;18(22):15182-90.
    PMID: 27199168 DOI: 10.1039/c6cp00583g
    The molecular dynamics of a synthetic branched chain glycolipid, 2-decyl-tetradecyl-β-d-maltoside (C14-10G2), in the dry assemblage of smectic and columnar liquid crystal phases has been studied by dielectric spectroscopy as a function of frequency and temperature during the cooling process. Strong relaxation modes were observed corresponding to the tilted smectic and columnar phases, respectively. At low frequency (∼900 Hz to 1 kHz) in the smectic phase, Process I* was observed due to the tilted sugar bilayer structure. The process continued in the columnar phase (Process I) with an abrupt dynamic change due to phase transition in the frequency range of ∼1.3 kHz to 22 kHz. An additional process (Process II) was observed in the columnar phase with a broader relaxation in the frequency range of ∼10 Hz to 1 kHz. A bias field dependence study was performed in the columnar phase and we found that the relaxation strength rapidly decreased with increased applied dc bias field. This relaxation originates from a collective motion of polar groups within the columns. The results of dielectric spectroscopy were supported by a molecular dynamics simulation study to identify the origin of the relaxation processes, which could be related to the chirality and hydrogen bonds of the sugar lipid.
Filters
Contact Us

Please provide feedback to Administrator (afdal@afpm.org.my)

External Links