Displaying all 8 publications

Abstract:
Sort:
  1. Teo PT, Anasyida AS, Basu P, Nurulakmal MS
    Waste Manag, 2014 Dec;34(12):2697-708.
    PMID: 25242607 DOI: 10.1016/j.wasman.2014.08.015
    Recently, various solid wastes from industry such as glass waste, fly ash, sewage sludge and slag have been recycled into various value-added products such as ceramic tile. The conventional solutions of dumping the wastes in landfills or incineration, including in Malaysia are getting obsolete as the annual huge amount of the solid wastes would boost-up disposal cost and may cause permanent damage to the flora and fauna. This recent waste recycling approach is much better and greener as it can resolve problems associated with over-limit storage of industrial wastes and reduce exploration of natural resources for ceramic tile to continuously sustain the nature. Therefore, in this project, an attempt was made to recycle electric arc furnace (EAF) slag waste, obtained from Malaysia's steel making industry, into ceramic tile via conventional powder compaction method. The research work was divided into two stages. The first stage was to evaluate the suitability of EAF slag in ceramic tile by varying weight percentage of EAF slag (40 wt.%, 50 wt.% and 60 wt.%) and ball clay (40 wt.%, 50 wt.% and 60 wt.%), with no addition of silica and potash feldspar. In the second stage, the weight percentage of EAF slag was fixed at 40 wt.% and the percentage of ball clay (30 wt.% and 40 wt.%), feldspar (10 wt.% and 20 wt.%) and silica (10 wt.% and 20 wt.%) added was varied accordingly. Results obtained show that as weight percentage of EAF slag increased up to 60 wt.%, the percentage of apparent porosity and water absorption also rose, with a reduction in tile flexural strength and increased porosity. On the other hand, limiting the weight percentage of EAF slag to 40 wt.% while increasing the weight percentage of ball clay led to a higher total percentage of anorthite and wollastonite minerals, resulting in higher flexural strength. It was found that introduction of silica and feldspar further improved the flexural strength due to optimization of densification process. The highest flexural strength, lowest apparent porosity and water absorption of EAF slag based tile was attained at the composition of 40 wt.% EAF slag--30 wt.% ball clay--10 wt.% feldspar--20 wt.% silica. The properties of ceramic tile made with EAF slag waste (up to 40 wt.%), especially flexural strength are comparable to those of commercial ceramic tile and are, therefore, suitable as high flexural strength and heavy-duty green ceramic floor tile. Continuous development is currently underway to improve the properties of tile so that this recycling approach could be one of the potential effective, efficient and sustainable solutions in sustaining our nature.
    Matched MeSH terms: Ceramics/analysis*
  2. Rusnah M, Andanastuti M, Idris B
    Med J Malaysia, 2004 May;59 Suppl B:158-9.
    PMID: 15468866
    The present paper reports on the influence of sintering temperature on the porosity and strength of porous hydroxyapatite (HA). HA powder was first prepared by the sol-gel precipitation method using calcium hydroxide and ortho-phosporic acid. The fine HA powder, measuring <50 microm was then mixed into a slurry with the addition of binder agent, being a mixture of sago and PVA. A small amount of sodium dodecyl sulphate was also used as a foaming agent. Porous HA samples were then prepared via slip casting technique. The surface morphology of the sintered samples was observed under scanning electron microscopy at 20 kV and the compositions were determined via SEM-EDX. A universal testing machine was used to determine the compaction strength of the sintered samples.
    Matched MeSH terms: Ceramics/analysis*
  3. Jamaluddin O, Zainal AA
    Med J Malaysia, 2004 May;59 Suppl B:143-4.
    PMID: 15468859
    Raising the thermal expansion coefficient (CTE) of dental porcelains is important to match the CTE of the ceramic material with the higher CTE of the metal inlay in dental restorations. The higher thermal expansion of the leucite phase increases the overall thermal expansion coefficient of the dental porcelain. Potassium nitrate (KNO3) additions in controlled percentages to the base dental porcelain formulation help in the formation of a leucite phase. The percentage added was 5,10 and 20 weight percent of leucite, respectively, to the total base frit composition. The change in CTE values was then investigated using a Linseis Dilatometer. A 20wt% KNO3 addition resulted in a CTE of 9.0 microm/m-K compared to the 7.7 microm/m-K CTE of the base composition. The microstructures observed under the scanning electron microscope (SEM) show a multiphase material with the leucite phases dispersed within a glassy matrix. The results suggest that higher CTEs in the dental porcelain are possible by increasing the KNO3- additions within the limits tested.
    Matched MeSH terms: Ceramics/analysis*
  4. Choudhury D, Vrbka M, Mamat AB, Stavness I, Roy CK, Mootanah R, et al.
    J Mech Behav Biomed Mater, 2017 08;72:192-199.
    PMID: 28500998 DOI: 10.1016/j.jmbbm.2017.05.011
    Coefficient of friction (COF) tests were conducted on 28-mm and 36-mm-diameter hip joint prostheses for four different material combinations, with or without the presence of Ultra High Molecular Weight Polyethylene (UHMWPE) particles using a novel pendulum hip simulator. The effects of three micro dimpled arrays on femoral head against a polyethylene and a metallic cup were also investigated. Clearance played a vital role in the COF of ceramic on polyethylene and ceramic on ceramic artificial hip joints. Micro dimpled metallic femoral heads yielded higher COF against a polyethylene cup; however, with metal on metal prostheses the dimpled arrays significantly reduced the COF. In situ images revealed evidence that the dimple arrays enhanced film formation, which was the main mechanism that contributed to reduced friction.
    Matched MeSH terms: Ceramics/analysis*
  5. Pohchi A, Suzina AH, Samsudin AR, Al-Salihi KA
    Med J Malaysia, 2004 May;59 Suppl B:151-2.
    PMID: 15468863
    This in vivo study revealed that porous hydroxyapatite (PHA) and dense hydroxyapatite (DHA) are good implant materials that can accelerate bone healing and resorbed in acceptable time. But there were differences in the mechanism of the resorption of DHA and PHA due to variability in the physical properties and osteogenicity.
    Matched MeSH terms: Ceramics/analysis*
  6. Idris B, Rusnah M, Reusmaazran YM, Rohaida CH
    Med J Malaysia, 2004 May;59 Suppl B:67-8.
    PMID: 15468822
    Matched MeSH terms: Ceramics/analysis
  7. Rusnah M, Andanastuti M, Idris B
    Med J Malaysia, 2004 May;59 Suppl B:83-4.
    PMID: 15468830
    The paper discusses the influence of sintering temperature on the microstructure and strength of hydroxyapatite ceramics prepared using the extrusion process. The average pore diameters observed were in the range of approximately 150mm to 300mm whereas the compaction strength was found to be around 120-160 MPa.
    Matched MeSH terms: Ceramics/analysis*
  8. Cik Rohaida CH, Idris B, Mohd Reusmaazran Y, Rusnah M, Fadzley Izwan AM
    Med J Malaysia, 2004 May;59 Suppl B:156-7.
    PMID: 15468865
    A mixture with different compositions of HA and TCP were synthesize in this work by precipitation method using Ca(NO3)2 4H2 and (NH4)2HPO4 as the starting materials. A mixture with HA and TCP phases in different ratios were produced. The powders were sintered from 1000 degrees C to 1250 degrees C. The phase compositions of the mixtures were then studied via XRD. This work shows that the pH value determines the different phase compositions of the HA-TCP mixture. Chemical analyses were carried out by FTIR. The microstructure was observed under SEM.
    Matched MeSH terms: Ceramics/analysis