Affiliations 

  • 1 Department of Prosthetic Dentistry, Faculty of Dentistry, King Salman International University, South Sinai, Egypt
  • 2 Department of Restorative Dentistry, Faculty of Dentistry, Universiti Malaya, Kuala Lumpur, Malaysia
  • 3 Department of Conservative Dentistry, Faculty of Oral and Dental Medicine, Badr University in Cairo, Cairo, Egypt
  • 4 Department of Prosthodontics, Faculty of Oral and Dental Medicine, Badr University in Cairo, Cairo, Egypt
J Prosthodont, 2024 Sep 09.
PMID: 39248202 DOI: 10.1111/jopr.13937

Abstract

PURPOSE: To evaluate and compare internal fit and marginal adaptation of conventional lithium disilicate (LDS) glass ceramics and LDS containing virgilite computer-aided design and manufacturing (CAD-CAM) blocks before and after aging.

MATERIALS AND METHODS: Seventy-two epoxy replicated dies from two prepared maxillary right central incisors acrylic typodont were divided into two groups of different preparation designs (n = 36): Group I, incisal butt-joint, and Group P, incisal overlap. Each group was further subdivided into two equal groups according to ceramic material (n = 18): Group E, IPS e.max CAD, and Group T, Tessera advanced lithium disilicate (ALD) CAD-CAM blocks. The replica technique was used to assess the internal fit using a stereomicroscope at 45× magnification. Laminate veneers were cemented to their corresponding epoxy dies, then the vertical marginal gap was evaluated before and after thermal cycling. Repeated measures analysis of variance (ANOVA) were used for marginal fit data and 2-way ANOVA for internal fit measurements (α = 0.05).

RESULTS: For internal fit, there were no significant differences between tested groups. For vertical marginal gap results, two-way ANOVA showed that only aging had a significant effect on the vertical marginal gap (p 