Abstract

This study aimed to evaluate surface roughness (SR) changes with surface treatments and shear bond strength (SBS) of two prefabricated and one laboratory-made composite veneer systems. The prefabricated groups, Edelweiss (EDL) and Componeer (CMP) while, SR Nexco (NEX) was a laboratory-made group. A total of hundred twenty samples, comprising 40 samples for each group were divided into four subgroups of surface treatment (n=10): (a) no treatment (control), (b) 9% hydrofluoric acid (HF), (c) abrasion with a high-speed diamond bur and (d) sandblast with aluminum trioxide (Al2O3) particles. A profilometer was used to evaluate the SR before and after surface treatments applications. Stereo electron microscope was utilized to assess changes occurred on the surface texture of the veneers. For SBS test, the prepared veneer was uploaded over an epoxy resin mould. Two cylindrical adhesive resins were bonded binary and perpendicular over the inner surface of the veneer and tested using Universal Testing Machine (SHIMADZUTM, Japan). Data was analyzed using One-way ANOVA, post-hoc student’s t-test and Duncan test with p