Displaying publications 121 - 140 of 375 in total

Abstract:
Sort:
  1. Thomas B, Gupta K
    J Esthet Restor Dent, 2017 Nov 12;29(6):435-441.
    PMID: 28703476 DOI: 10.1111/jerd.12317
    OBJECTIVE: Nano-hydroxyapatite-added GIC has been developed to improve the physical properties of conventional GIC. However, biological response of periodontal cells to this potentially useful cervical restorative material has been unexplored. The aim of this study was to investigate the in vitro response of human periodontal ligament fibroblasts to hydroxyapatite-added GIC.

    MATERIALS AND METHODS: Three categories of materials, namely, test group 1 (cGIC or type IX GIC), test group 2 (HA-GIC or hydroxyapatite-added GIC), and positive control (glass cover slips) were incubated with human periodontal ligament fibroblasts. The samples were viewed under scanning electron microscope to study the morphological characteristics of fibroblasts. Additionally, elemental analysis was performed to differentiate between the two test groups based on surface chemical composition.

    RESULTS: Test group 1 (cGIC) exhibited cells with curled up morphology, indicative of poor attachment to the substrate. Test group 2 (Ha-GIC) exhibited cells with flattened morphology and numerous cellular extensions such as lamellipodia and blebs, indicative of good attachment to the substrate. The test group 2 (Ha-GIC) demonstrated higher surface elemental percentages of calcium and phosphorus.

    CONCLUSION: Within the limitations of this study, it may be concluded that hydroxyapatite-added GIC is more biocompatible than conventional GIC (type IX), probably attributed to high elemental percentages of calcium and phosphorus.

    CLINICAL SIGNIFICANCE: The search for an ideal cervical restorative dental material has been ever elusive. Hydroxyapatite-added GIC is a simple and economical dental material to fabricate from basic conventional GIC. The results from this study strengthen its candidature for cervical and root surface restorations which may later require soft tissue augmentation. The possibility of connective tissue adhesion to this material is an exciting prospect in the field of periorestorative dentistry.

    Matched MeSH terms: Materials Testing
  2. Mohamad N, Buang F, Mat Lazim A, Ahmad N, Martin C, Mohd Amin MCI
    J Biomed Mater Res B Appl Biomater, 2017 Nov;105(8):2553-2564.
    PMID: 27690276 DOI: 10.1002/jbm.b.33776
    The use of bacterial cellulose (BC)-based hydrogel has been gaining attention owing to its biocompatibility and biodegradability. This study was designed to investigate the effect of radiation doses and acrylic acid (AA) composition on in vitro and in vivo biocompatibility of BC/AA as wound dressing materials. Physical properties of the hydrogel, that is, thickness, adhesiveness, rate of water vapor transmission, and swelling were measured. Moreover, the effect of these parameters on skin irritation and sensitization, blood compatibility, and cytotoxicity was studied. Increased AA content and irradiation doses increased the thickness, crosslinking density, and improved the mechanical properties of the hydrogel, but reduced its adhesiveness. The swelling capacity of the hydrogel increased significantly with a decrease in the AA composition in simulated wound fluid. The water vapor permeability of polymeric hydrogels was in the range of 2035-2666 [g/(m-2  day-1 )]. Dermal irritation and sensitization test demonstrated that the hydrogel was nonirritant and nonallergic. The BC/AA hydrogel was found to be nontoxic to primary human dermal fibroblast skin cells with viability >88% and was found to be biocompatible with blood with a low hemolytic index (0.80-1.30%). Collectively, these results indicate that these hydrogels have the potential to be used as wound dressings. © 2016 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 105B: 2553-2564, 2017.
    Matched MeSH terms: Materials Testing*
  3. Rizwan M, Hamdi M, Basirun WJ
    J Biomed Mater Res A, 2017 Nov;105(11):3197-3223.
    PMID: 28686004 DOI: 10.1002/jbm.a.36156
    Bioglass® 45S5 (BG) has an outstanding ability to bond with bones and soft tissues, but its application as a load-bearing scaffold material is restricted due to its inherent brittleness. BG-based composites combine the amazing biological and bioactive characteristics of BG with structural and functional features of other materials. This article reviews the composites of Bioglass® in combination with metals, ceramics and polymers for a wide range of potential applications from bone scaffolds to nerve regeneration. Bioglass® also possesses angiogenic and antibacterial properties in addition to its very high bioactivity; hence, composite materials developed for these applications are also discussed. BG-based composites with polymer matrices have been developed for a wide variety of soft tissue engineering. This review focuses on the research that suggests the suitability of BG-based composites as a scaffold material for hard and soft tissues engineering. Composite production techniques have a direct influence on the bioactivity and mechanical behavior of scaffolds. A detailed discussion of the bioactivity, in vitro and in vivo biocompatibility and biodegradation is presented as a function of materials and its processing techniques. Finally, an outlook for future research is also proposed. © 2017 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 105A: 3197-3223, 2017.
    Matched MeSH terms: Materials Testing
  4. Matinmanesh A, Li Y, Clarkin O, Zalzal P, Schemitsch EH, Towler MR, et al.
    J Mech Behav Biomed Mater, 2017 11;75:212-221.
    PMID: 28756281 DOI: 10.1016/j.jmbbm.2017.07.030
    Bioactive glasses have been used as coatings for biomedical implants because they can be formulated to promote osseointegration, antibacterial behavior, bone formation, and tissue healing through the incorporation and subsequent release of certain ions. However, shear loading on coated implants has been reported to cause the delamination and loosening of such coatings. This work uses a recently developed fracture mechanics testing methodology to quantify the critical strain energy release rate under nearly pure mode II conditions, GIIC, of a series of borate-based glass coating/Ti6Al4V alloy substrate systems. Incorporating increasing amounts of SrCO3in the glass composition was found to increase the GIICalmost twofold, from 25.3 to 46.9J/m2. The magnitude and distribution of residual stresses in the coating were quantified, and it was found that the residual stresses in all cases distributed uniformly over the cross section of the coating. The crack was driven towards, but not into, the glass/Ti6Al4V substrate interface due to the shear loading. This implied that the interface had a higher fracture toughness than the coating itself.
    Matched MeSH terms: Materials Testing*
  5. Baba Ismail YM, Ferreira AM, Bretcanu O, Dalgarno K, El Haj AJ
    Colloids Surf B Biointerfaces, 2017 Nov 01;159:445-453.
    PMID: 28837894 DOI: 10.1016/j.colsurfb.2017.07.086
    This paper presents a new approach in assembling bone extracellular matrix components onto PLA films, and investigates the most favourable environment which can be created using the technique for cell-material interactions. Poly (lactic acid) (PLA) films were chemically modified by covalently binding the poly(ethylene imine) (PEI) as to prepare the substrate for immobilization of polyelectrolyte multilayers (PEMs) coating. Negatively charged polyelectrolyte consists of well-dispersed silicon-carbonated hydroxyapatite (SiCHA) nanopowders in hyaluronic acid (Hya) was deposited onto the modified PLA films followed by SiCHA in collagen type I as the positively charged polyelectrolyte. The outermost layer was finally cross-linked by 1-ethyl-3-(3-dimethylaminopropyl) carbodiimide hydrocholoride and N-hydroxysulfosuccinimide sodium salt (EDC/NHS) solutions. The physicochemical features of the coated PLA films were monitored via X-ray Photoelectron Spectroscopy (XPS) and Atomic Force Microscope (AFM). The amounts of calcium and collagen deposited on the surface were qualitatively and quantitatively determined. The surface characterizations suggested that 5-BL has the optimum surface roughness and highest amounts of calcium and collagen depositions among tested films. In vitro human mesenchymal stem cells (hMSCs) cultured on the coated PLA films confirmed that the coating materials greatly improved cell attachment and survival compared to unmodified PLA films. The cell viability, cell proliferation and Alkaline Phosphatase (ALP) expression on 5-BL were found to be the most favourable of the tested films. Hence, this newly developed coating materials assembly could contribute to the improvement of the bioactivity of polymeric materials and structures aimed to bone tissue engineering applications.
    Matched MeSH terms: Materials Testing/methods*
  6. Zeimaran E, Pourshahrestani S, Pingguan-Murphy B, Kong D, Naveen SV, Kamarul T, et al.
    Carbohydr Polym, 2017 Nov 01;175:618-627.
    PMID: 28917909 DOI: 10.1016/j.carbpol.2017.08.038
    Blends of poly (1, 8-octanediol citrate) (POC) and chitosan (CS) were prepared through solution casting technique. Films with different component fractions (POC/CS: 100/0, 90/10, 80/20, 70/30, 60/40, and 0/100) were successfully prepared and characterized for their mechanical, thermal, structural and morphological properties as well as biocompatibility. The incorporation of CS to POC significantly increased tensile strength and elastic modulus and presented limited influences on pH variation which is important to the biocompatibility of biomaterial implants. The assessment of surface topography indicated that blending could enhance and control the surface roughness of the pure films. POC/CS blends well-supported human dermal fibroblast cells attachment and proliferation, and thus can be used for a range of tissue engineering applications.
    Matched MeSH terms: Materials Testing
  7. Ullah S, Zainol I, Idrus RH
    Int J Biol Macromol, 2017 Nov;104(Pt A):1020-1029.
    PMID: 28668615 DOI: 10.1016/j.ijbiomac.2017.06.080
    The zinc oxide nanoparticles (particles size <50nm) incorporated into chitosan-collagen 3D porous scaffolds and investigated the effect of zinc oxide nanoparticles incorporation on microstructure, mechanical properties, biodegradation and cytocompatibility of 3D porous scaffolds. The 0.5%, 1.0%, 2.0% and 4.0% zinc oxide nanoparticles chitosan-collagen 3D porous scaffolds were fabricated via freeze-drying technique. The zinc oxide nanoparticles incorporation effects consisting in chitosan-collagen 3D porous scaffolds were investigated by mechanical and swelling tests, and effect on the morphology of scaffolds examined microscopically. The biodegradation and cytocompatibility tests were used to investigate the effects of zinc oxide nanoparticles incorporation on the ability of scaffolds to use for tissue engineering application. The mean pore size and swelling ratio of scaffolds were decreased upon incorporation of zinc oxide nanoparticles however, the porosity, tensile modulus and biodegradation rate were increased upon incorporation of zinc oxide nanoparticles. In vitro culture of human fibroblasts and keratinocytes showed that the zinc oxide nanoparticles facilitated cell adhesion, proliferation and infiltration of chitosan-collagen 3D porous scaffolds. It was found that the zinc oxide nanoparticles incorporation enhanced porosity, tensile modulus and cytocompatibility of chitosan-collagen 3D porous scaffolds.
    Matched MeSH terms: Materials Testing
  8. Revati R, Majid MSA, Ridzuan MJM, Basaruddin KS, Rahman Y MN, Cheng EM, et al.
    J Mech Behav Biomed Mater, 2017 10;74:383-391.
    PMID: 28688321 DOI: 10.1016/j.jmbbm.2017.06.035
    The in vitro degradation and mechanical properties of a 3D porous Pennisetum purpureum (PP)/polylactic acid (PLA)-based scaffold were investigated. In this study, composite scaffolds with PP to PLA ratios of 0%, 10%, 20%, and 30% were immersed in a PBS solution at 37°C for 40 days. Compression tests were conducted to evaluate the compressive strength and modulus of the scaffolds, according to ASTM F451-95. The compression strength of the scaffolds was found to increase from 1.94 to 9.32MPa, while the compressive modulus increased from 1.73 to 5.25MPa as the fillers' content increased from 0wt% to 30wt%. Moreover, field emission scanning electron microscopy (FESEM) and X-ray diffraction were employed to observe and analyse the microstructure and fibre-matrix interface. Interestingly, the degradation rate was reduced for the PLA/PP20scaffold, though insignificantly, this could be attributed to the improved mechanical properties and stronger fibre-matrix interface. Microstructure changes after degradation were observed using FESEM. The FESEM results indicated that a strong fibre-matrix interface was formed in the PLA/PP20scaffold, which reflected the addition of P. purpureum into PLA decreasing the degradation rate compared to in pure PLA scaffolds. The results suggest that the P. purpureum/PLA scaffold degradation rate can be altered and controlled to meet requirements imposed by a given tissue engineering application.
    Matched MeSH terms: Materials Testing
  9. Eweis AH, Yap AU, Yahya NA
    J Mech Behav Biomed Mater, 2017 10;74:183-188.
    PMID: 28605721 DOI: 10.1016/j.jmbbm.2017.06.004
    This study investigated the effect of food simulating liquids on visco-elastic properties of bulk-fill restoratives using dynamic mechanical analysis. One conventional composite (Filtek Z350 [FZ]), two bulk-fill composites (Filtek Bulk-fill [FB] and Tetric N Ceram [TN]) and a bulk-fill giomer (Beautifil-Bulk Restorative [BB]) were evaluated. Specimens (12 × 2 × 2mm) were fabricated using customized stainless steel molds. The specimens were light-cured, removed from their molds, finished, measured and randomly divided into six groups. The groups (n = 10) were conditioned in the following mediums for 7 days at 37°C: air (control), artificial saliva (SAGF), distilled water, 0.02N citric acid, heptane, 50% ethanol-water solution. Specimens were assessed using dynamic mechanical testing in flexural three-point bending mode and their respective mediums at 37°C and a frequency range of 0.1-10Hz. The distance between the supports were fixed at 10mm and an axial load of 5N was employed. Data for elastic modulus, viscous modulus and loss tangent were subjected to ANOVA/Tukey's tests at significance level p < 0.05. Significant differences in visco-elastic properties were observed between materials and mediums. Apart from bulk-fill giomer, elastic modulus was the highest after conditioning in heptane. No apparent trends were noted for viscous modulus. Generally, loss tangent was the highest after conditioning in ethanol. The effect of food-simulating liquids on the visco-elastic properties of bulk-fill composites was material and medium dependent.
    Matched MeSH terms: Materials Testing*
  10. Elshereksi NW, Ghazali M, Muchtar A, Azhari CH
    Dent Mater J, 2017 Sep 26;36(5):539-552.
    PMID: 28652551 DOI: 10.4012/dmj.2016-014
    Silane is a dominant coupler that is widely used in dentistry to promote adhesion among the components of dental composites. Silica-based fillers can be easily silanized because of their similarly ordered structure. However, silane is hydrolytically degraded in the aqueous oral environment and inefficiently bonds to non-silica fillers. Thus, the development of hydrolytically stable dental composites is an important objective in the research on dental materials. Titanate coupling agents (TCAs) exhibit satisfactory interfacial bonding, enhanced homogeneous filler dispersion, and improved mechanical properties of the composites. Titanates also provide superior hydrolytic stability in wet environments, which should be considered in fabricating dental composites. The addition of a small amount of titanates can improve the resistance of the composites to moisture. This paper reviews the effects of the instability of silanes in moisture on the performance of dental composites and presents TCAs as alternative couplers to silanes for fabricating dental composites.
    Matched MeSH terms: Materials Testing
  11. Sahapaibounkit P, Prasertsung I, Mongkolnavin R, Wong CS, Damrongsakkul S
    J Biomed Mater Res B Appl Biomater, 2017 08;105(6):1658-1666.
    PMID: 27177842 DOI: 10.1002/jbm.b.33708
    In this study, polycaprolactone (PCL) film, a high potential material used in biomedical applications, was treated by air plasma prior to a conjugation by carbodiimide cross-linking with various types of proteins, including type A gelatin, type B gelatin, and collagen hydrolysate. The properties of modified PCL films were characterized by X-ray photoelectron spectroscopy (XPS), contact angle measurement, and atomic force microscopy. The XPS results showed that oxygen and nitrogen atoms were successfully introduced on the air plasma-treated PCL surface. Primary amine was found on the air plasma-treated PCL films. All proteins were shown to be successfully cross-linked on air plasma-treated PCL films. The wettability and roughness of protein-conjugated PCL films were significantly increased compared to those of neat PCL film. In vitro biocompatibility test using L929 mouse fibroblast showed that the attachment percentage and spreading area of attached cells on all protein-conjugated PCL films were markedly increased. Comparing among modified PCL films, no significant difference on the attachment of L929 on modified PCL films was noticed. However, the spreading areas of cells after 24 hours of culture on type A gelatin- and type B gelatin-modified PCL surfaces were higher than that on collagen hydrolysate-modified surface, possibly related to the lower percentage of amide bond on collagen hydrolysate-conjugated surface compared to those on both gelatin-conjugated PCL ones. This indicated that the two-step modification of PCL film via air plasma and carbodiimide cross-linking with collagen-derived proteins could enhance the biocompatibility of PCL films. © 2016 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 105B: 1658-1666, 2017.
    Matched MeSH terms: Materials Testing*
  12. Choudhury D, Vrbka M, Mamat AB, Stavness I, Roy CK, Mootanah R, et al.
    J Mech Behav Biomed Mater, 2017 08;72:192-199.
    PMID: 28500998 DOI: 10.1016/j.jmbbm.2017.05.011
    Coefficient of friction (COF) tests were conducted on 28-mm and 36-mm-diameter hip joint prostheses for four different material combinations, with or without the presence of Ultra High Molecular Weight Polyethylene (UHMWPE) particles using a novel pendulum hip simulator. The effects of three micro dimpled arrays on femoral head against a polyethylene and a metallic cup were also investigated. Clearance played a vital role in the COF of ceramic on polyethylene and ceramic on ceramic artificial hip joints. Micro dimpled metallic femoral heads yielded higher COF against a polyethylene cup; however, with metal on metal prostheses the dimpled arrays significantly reduced the COF. In situ images revealed evidence that the dimple arrays enhanced film formation, which was the main mechanism that contributed to reduced friction.
    Matched MeSH terms: Materials Testing*
  13. Kakavand M, Yazdanpanah G, Ahmadiani A, Niknejad H
    J Tissue Eng Regen Med, 2017 06;11(6):1701-1709.
    PMID: 26190586 DOI: 10.1002/term.2064
    Amniotic membrane (AM), a placenta-derived natural biomaterial, has several characteristics which make it a potential substitute for blood vessels. However, there are no reports on the effects of the AM on blood components. The aim of this study was to evaluate the blood compatibility of the epithelial and mesenchymal surfaces of the amnion for potential use in vascular tissue engineering. The activation of intrinsic and extrinsic pathways of the clotting system, haemolysis and platelet adhesion were studied and the results were compared with heparin-coated expanded polytetrafluoroethylene (ePTFE) as a standard synthetic vascular graft. Prothrombin time (PT), activated partial thromboplastin time (aPTT), clotting time (CT) and haemolysis (%) tests showed that both the epithelial and mesenchymal sides of the AM are haemocompatible. Platelet aggregation and P-selectin production from the platelets showed that the epithelial surface of the AM has less induction of platelet activation than ePTFE. The results of scanning electron microscopy (SEM) demonstrated that platelets in contact with ePTFE had a higher rate of adhesion than with the epithelial and mesenchymal surfaces of the AM. Moreover, the morphological distribution of the platelets showed that the majority of platelets were round, while a large number of cells on ePTFE were dendritic. These results suggest that the AM which contains epithelial and mesenchymal stem cells has appropriate haemocompatibility to be employed in vascular tissue engineering, especially as a vein substitute. Copyright © 2015 John Wiley & Sons, Ltd.
    Matched MeSH terms: Materials Testing*
  14. Baba Ismail YM, Wimpenny I, Bretcanu O, Dalgarno K, El Haj AJ
    J Biomed Mater Res A, 2017 Jun;105(6):1775-1785.
    PMID: 28198131 DOI: 10.1002/jbm.a.36038
    Ionic substitutions have been proposed as a tool to control the functional behavior of synthetic hydroxyapatite (HA), particularly for Bone Tissue Engineering applications. The effect of simultaneous substitution of different levels of carbonate (CO3) and silicon (Si) ions in the HA lattice was investigated. Furthermore, human bone marrow-derived mesenchymal stem cells (hMSCs) were cultured on multi-substituted HA (SiCHA) to determine if biomimetic chemical compositions were osteoconductive. Of the four different compositions investigates, SiCHA-1 (0.58 wt % Si) and SiCHA-2 (0.45 wt % Si) showed missing bands for CO3and Si using FTIR analysis, indicating competition for occupation of the phosphate site in the HA lattice; 500°C was considered the most favorable calcination temperature as: (i) the powders produced possessed a similar amount of CO3(2-8 wt %) and Si (<1.0 wt %) as present in native bone; and (ii) there was a minimal loss of CO3and Si from the HA structure to the surroundings during calcination. Higher Si content in SiCHA-1 led to lower cell viability and at most hindered proliferation, but no toxicity effect occurred. While, lower Si content in SiCHA-2 showed the highest ALP/DNA ratio after 21 days culture with hMSCs, indicating that the powder may stimulate osteogenic behavior to a greater extent than other powders. © 2017 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 105A: 1775-1785, 2017.
    Matched MeSH terms: Materials Testing
  15. Revati R, Abdul Majid MS, Ridzuan MJM, Normahira M, Mohd Nasir NF, Rahman Y MN, et al.
    Mater Sci Eng C Mater Biol Appl, 2017 Jun 01;75:752-759.
    PMID: 28415525 DOI: 10.1016/j.msec.2017.02.127
    The mechanical, thermal, and morphological properties of a 3D porous Pennisetum purpureum (PP)/polylactic acid (PLA) based scaffold were investigated. In this study, a scaffold containing P. purpureum and PLA was produced using the solvent casting and particulate leaching method. P. purpureum fibre, also locally known as Napier grass, is composed of 46% cellulose, 34% hemicellulose, and 20% lignin. PLA composites with various P. purpureum contents (10%, 20%, and 30%) were prepared and subsequently characterised. The morphologies, structures and thermal behaviours of the prepared composite scaffolds were characterised using field-emission scanning electron microscopy (FESEM), Fourier transform infrared spectroscopy (FTIR), and thermogravimetric analysis (TGA). The morphology was studied using FESEM; the scaffold possessed 70-200μm-sized pores with a high level of interconnectivity. The moisture content and mechanical properties of the developed porous scaffolds were further characterised. The P. purpureum/PLA scaffold had a greater porosity factor (99%) and compression modulus (5.25MPa) than those of the pure PLA scaffold (1.73MPa). From the results, it can be concluded that the properties of the highly porous P. purpureum/PLA scaffold developed in this study can be controlled and optimised. This can be used to facilitate the construction of implantable tissue-engineered cartilage.
    Matched MeSH terms: Materials Testing
  16. Gaaz TS, Sulong AB, Kadhum AAH, Al-Amiery AA, Nassir MH, Jaaz AH
    Molecules, 2017 May 20;22(5).
    PMID: 28531126 DOI: 10.3390/molecules22050838
    Nanotubular clay minerals, composed of aluminosilicate naturally structured in layers known as halloysite nanotubes (HNTs), have a significant reinforcing impact on polymer matrixes. HNTs have broad applications in biomedical applications, the medicine sector, implant alloys with corrosion protection and manipulated transportation of medicines. In polymer engineering, different research studies utilize HNTs that exhibit a beneficial enhancement in the properties of polymer-based nanocomposites. The dispersion of HNTs is improved as a result of pre-treating HNTs with acids. The HNTs' percentage additive up to 7% shows the highest improvement of tensile strength. The degradation of the polymer can be also significantly improved by doping a low percentage of HNTs. Both the mechanical and thermal properties of polymers were remarkably improved when mixed with HNTs. The effects of HNTs on the mechanical and thermal properties of polymers, such as ultimate strength, elastic modulus, impact strength and thermal stability, are emphasized in this study.
    Matched MeSH terms: Materials Testing
  17. Zailani MZ, Ismail AF, Sheikh Abdul Kadir SH, Othman MH, Goh PS, Hasbullah H, et al.
    J Biomed Mater Res A, 2017 05;105(5):1510-1520.
    PMID: 28000366 DOI: 10.1002/jbm.a.35986
    In this study, poly (1,8-octanediol citrate) (POC) was used to modify polyethersulfone (PES)-based membrane to enhance its hemocompatibility. Different compositions of POC (0-3%) were added into the polyethersulfone (PES) dope solutions and polyvinylpyrrolidone (PVP) was used as pore forming agent. The hemocompatible POC modified PES membranes were fabricated through phase-inversion technique. The prepared membranes were characterized using attenuated total reflectance-Fourier transform infrared (ATR-FTIR), thermogravimetric analysis (TGA), scanning electron microscopy (SEM), Atomic-force microscopy (AFM), contact angle, Zeta-potential, membrane porosity and pore size and pure water flux (PWF) and BSA rejection. The hemocompatibility of the modified PES membranes was evaluated by human serum fibrinogen (FBG) protein adsorption, platelet adhesion, activated partial thromboplastin time (APTT) and prothrombin time (PT), and thrombin-antithrombin III (TAT), complement (C3a and C5a) activation and Ca2+ absorption on membrane. Results showed that by increasing POC concentration, FBG adsorption was reduced, less platelets adhesion, prolonged APTT and PT, lower TAT, C5a and C3a activation and absorb more Ca2+ ion. These results indicated that modification of PES with POC has rendered improved hemocompatibility properties for potential application in the field of blood purification, especially in hemodialysis. © 2017 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 105A: 1510-1520, 2017.
    Matched MeSH terms: Materials Testing*
  18. Butcher AL, Koh CT, Oyen ML
    J Mech Behav Biomed Mater, 2017 May;69:412-419.
    PMID: 28208112 DOI: 10.1016/j.jmbbm.2017.02.007
    Electrospinning is a simple and efficient process for producing sub-micron fibres. However, the process has many variables, and their effects on the non-woven mesh of fibres is complex. In particular, the effects on the mechanical properties of the fibre meshes are poorly understood. This paper conducts a parametric study, where the concentration and bloom strength of the gelatin solutions are varied, while all electrospinning process parameters are held constant. The effects on the fibrous meshes are monitored using scanning electron microscopy and mechanical testing under uniaxial tension. Mesh mechanical properties are relatively consistent, despite changes to the solutions, demonstrating the robustness of electrospinning. The gel strength of the solution is shown to have a statistically significant effect on the morphology, stiffness and strength of the meshes, while the fibre diameter has surprisingly little influence on the stiffness of the meshes. This experimental finding is supported by finite element analysis, demonstrating that the stiffness of the meshes is controlled by the volume fraction, rather than fibre diameter. Our results demonstrate the importance of understanding how electrospinning parameters influence the pore size of the meshes, as controlling fibre diameter alone is insufficient for consistent mechanical properties.
    Matched MeSH terms: Materials Testing*
  19. Bakhsheshi-Rad HR, Hamzah E, Low HT, Kasiri-Asgarani M, Farahany S, Akbari E, et al.
    Mater Sci Eng C Mater Biol Appl, 2017 Apr 01;73:215-219.
    PMID: 28183601 DOI: 10.1016/j.msec.2016.11.138
    In this work, binary Zn-0.5Al and ternary Zn-0.5Al-xMg alloys with various Mg contents were investigated as biodegradable materials for implant applications. Compared with Zn-0.5Al (single phase), Zn-0.5Al-xMg alloys consisted of the α-Zn and Mg2(Zn, Al)11 with a fine lamellar structure. The results also revealed that ternary Zn-Al-Mg alloys presented higher micro-hardness value, tensile strength and corrosion resistance compared to the binary Zn-Al alloy. In addition, the tensile strength and corrosion resistance increased with increasing the Mg content in ternary alloys. The immersion tests also indicated that the corrosion rates in the following order Zn-0.5Al-0.5Mg
    Matched MeSH terms: Materials Testing*
  20. Rezvanian M, Ahmad N, Mohd Amin MC, Ng SF
    Int J Biol Macromol, 2017 Apr;97:131-140.
    PMID: 28064048 DOI: 10.1016/j.ijbiomac.2016.12.079
    Natural polymer-based hydrogel films have great potential for biomedical applications and are good candidates for wound dressings. In this study, we aimed to develop simvastatin-loaded crosslinked alginate-pectin hydrogel films by ionic crosslinking to improve the mechanical characteristics, wound fluid uptake and drug release behavior. Alginate-pectin hydrocolloid films were chemically crosslinked by immersing in different concentrations of CaCl2 (0.5-3% w/v) for 2-20min. The degree of crosslinking was influenced by both contact time and CaCl2 concentration. The optimized conditions for crosslinking were 0.5% and 1% (CaCl2) for 2min. The optimized hydrogel films were then characterized for their physical, mechanical, morphological, thermal, in vitro drug release, and cytocompatibility profiles. Crosslinking improved the mechanical profile and wound fluid uptake capacity of dressings. The hydrogel films were able to maintain their physical integrity during use, and the best results were obtained with the film in which the extent of crosslinking was low (0.5%). Thermal analysis confirmed that the crosslinking process enhanced the thermal stability of hydrogel films. Sustained, slow release of simvastatin was obtained from the crosslinked films and in vitro cytotoxicity assay demonstrated that the hydrogel films were non-toxic.
    Matched MeSH terms: Materials Testing
Filters
Contact Us

Please provide feedback to Administrator (afdal@afpm.org.my)

External Links