MATERIAL AND METHOD: Forty sound permanent mandibular premolars were collected from a dental clinical setting and disinfected. All forty samples were mounted vertically in a rubber mold exposing only the clinical crown. All samples were bleached using Opalescence Boost Professional Teeth Whitening. After the bleaching procedure, each sample was randomly allocated into four groups according to surface treatment. Samples in group 1 were treated with methylene blue photosensitizer (MBP). Samples in group 2 were exposed to 10% sodium ascorbate. Samples in group 3 were treated with Er, Cr: YSGG laser (ECL). Samples in group 4 were not treated (control). All Samples were treated with 37% phosphoric acid and a bonding agent was applied. A bulk-fill composite was cured to all specimens and all samples were treated in a thermocycler. Specimens were placed in a universal testing machine for shear bond strength (SBS) testing. Descriptive statistics were associated by analysis of variance (ANOVA) and Tukey's post hoc test maintaining level of significance (p<0.05) RESULTS: The lowest SBS scores were achieved in the bleached enamel (BE) group (15.25±1.745 MPa). Whereas, the highest bond integrity was attained by AA group (32.23±1.854 MPa). Samples treated with ECL (31.87±1.659 MPa) and AA (32.23±1.854) were comparable (p>0.05). Samples treated with PDT exhibited significantly different SBS (22.41±1.258) compared to other experimental groups CONCLUSION: ECL showed a reversal effect of BE compared to AA and has the potential to be used in clinical settings. BE reversal using MBP needs further investigation.
Materials and Methods: Ninety aluminum oxide ceramic (Turkom-Ceramic Sdn. Bhd., Kuala Lumpur, Malaysia) specimens were produced and divided into nine groups to receive the following surface treatments: control group, no treatment (Group C), sandblasting (Group B), silica coating (Group S), erbium: yttrium-aluminum-garnet (Er:YAG) laser irradiation at 150 mJ 10 Hz (Group L1), Er:YAG laser irradiation at 300 mJ 10 Hz (Group L2), sandblasting + L1 (Group BL1), sandblasting + L2 (Group BL2), silica coating + L1 (Group SL1), and silica coating + L2 (Group SL2). After surface treatments, surface roughness (SR) values were measured and surface topography was evaluated. Resin cement was applied on the specimen surface, and shear bond strength (SBS) tests were performed. Data were statistically analyzed using one-way ANOVA and Tukey's multiple comparisons at a significance level of P < 0.05.
Results: Group S, SL1, and SL2 showed significantly increased SR values compared to the control group (P < 0.05); therefore, no significant differences were found among the SR values of Groups B, BL1, BL2, L1, and L2 and the control group (P > 0.05). Group S showed the highest SBS values, whereas the control group showed the lowest SBS values.
Conclusion: Silica coating is the most effective method for resin bonding of high strength ceramic, but Er:YAG laser application decreased the effectiveness.
BACKGROUND DATA: The response of human blood to LLL irradiation gives important information about the mechanism of interaction of laser light with living organisms. Materials and methods Blood samples were collected into ethylenediaminetetraacetic acid (EDTA)-containing tubes, and each sample was divided into two equal aliquots, one to serve as control and the other for irradiation. The aliquot was subjected to laser irradiation for 20, 30, 40, or 50 min at a fixed power density of 0.03 W/cm(2). Mean cell volume (MCV) and red blood cell (RBC) counts were measured immediately after irradiation using a computerized hemtoanalyzer.
RESULTS: Significant decrease in RBC volume (p