Affiliations 

  • 1 Faculty of Chemical and Energy Engineering, Universiti Teknologi Malaysia, 81310 Skudai, Johor, Malaysia
  • 2 Department of Biological Sciences and Biotechnology, Faculty of Science and Technology, Universiti Kebangsaan Malaysia, 43600 Bangi, Selangor Darul Ehsan, Malaysia
  • 3 Department of Biosciences, Faculty of Science, Universiti Teknologi Malaysia, Johor Bahru 81310, Malaysia
  • 4 Faculty of Chemical and Energy Engineering, Universiti Teknologi Malaysia, 81310 Skudai, Johor, Malaysia; Institute of Bioproduct Development, Universiti Teknologi Malaysia, 81310 Skudai, Johor, Malaysia
  • 5 Faculty of Chemical and Energy Engineering, Universiti Teknologi Malaysia, 81310 Skudai, Johor, Malaysia; Institute of Bioproduct Development, Universiti Teknologi Malaysia, 81310 Skudai, Johor, Malaysia. Electronic address: r-rosli@utm.my
Int J Biol Macromol, 2024 Apr;263(Pt 1):130284.
PMID: 38382786 DOI: 10.1016/j.ijbiomac.2024.130284

Abstract

Polyethylene terephthalate (PET) is one of the most produced plastics globally and its accumulation in the environment causes harm to the ecosystem. Polyethylene terephthalate hydrolyse (PETase) is an enzyme that can degrade PET into its monomers. However, free PETase lacks operational stabilities and is not reusable. In this study, development of cross-linked enzyme aggregate (CLEA) of PETase using amylopectin (Amy) as cross-linker was introduced to solve the limitations of free PETase. PETase-Amy-CLEA exhibited activity recovery of 81.9 % at its best immobilization condition. Furthermore, PETase-Amy-CLEA exhibited 1.37-, 2.75-, 2.28- and 1.36-fold higher half-lives than free PETase at 50 °C, 45 °C, 40 °C and 35 °C respectively. Moreover, PETase-Amy-CLEA showed broader pH stability from pH 5 to 10 and could be reused up to 5 cycles. PETase-Amy-CLEA retained >70 % of initial activity after 40 days of storage at 4 °C. In addition, lower Km of PETase-Amy-CLEA indicated better substrate affinity than free enzyme. PETase-Amy-CLEA corroded PET better and products yielded was 66.7 % higher than free PETase after 32 h of treatment. Hence, the enhanced operational stabilities, storage stability, reusability and plastic degradation ability are believed to make PETase-Amy-CLEA a promising biocatalyst in plastic degradation.