Abstract

Three types of binder PVA, PVC and PVA/PVC mixtures have been evaluated for PANi-TiO2 immobilized system. These binders have been varied to several weights of loading for optimization purposes. As a result, it shows that higher loading of binders improved the photodegradation of RR4 dye but the mechanical properties of each immobilized system started to decreases. This behavior occurs due to the immobilized particles coated on the plate easy to peel off despite weak attachment toward to the continuous photodegradation operation system. Therefore 4 times of dipping PVA and PVC layers was selected as the optimum loading of binders to the PANi/TiO2 system during photocatalytic degradation of Reactive Red 4 with the rate constant of 0.5568 K/min for PVA and 0.5742 K/min for PVC. Meanwhile for PVA/PVC mixture binder system at 4 times dipping showed the highest rate constant of photodegradation of RR4 dye with 0.6026 K/min. In addition, SEM analysis has also been carried out for further investigation.