METHODS: Sixty-six (66) patients with unilateral uncomplicated inguinal hernia were randomized into 34 patients in the tacker and 32 patients in cyanoacrylate glue mesh fixation in TEP repair. The extent of surgical trauma was evaluated by measuring inflammatory markers of C-reactive protein, white blood cell count at 48 h, and ESR at 3 months postoperatively. Postoperative acute and chronic pain was assessed by recording the visual analogue scale scores and surgical complications were recorded over 3 months of the study period.
RESULTS: The median CRP and WBC levels at postoperative 48 h in both groups raised significantly from the baseline values (p 0.05). The median ESR level increased significantly at 3 months postoperatively from baseline in the glue mesh fixation group only (p 0.05). There was no significant difference for VAS scores at all timelines between the tacker and glue mesh fixation group (p > 0.05).
CONCLUSION: Cyanoacrylate glue mesh fixation technique as an alternative method to mechanical fixation in TEP repair is comparable to tacker and can be considered to be safe and feasible.
METHODS: A prospective, randomized, single-blinded clinical trial to assess the efficacy of autologous blood in place of fibrin glue in pterygium surgery. A total of 120 eyes of 111 patients were randomized according to pterygium morphology, to undergo pterygium surgery with autografting using either autologous blood or fibrin glue. All patients were operated by a single surgeon; 58 eyes were operated using fibrin glue and 62 eyes had a conjunctival autograft with autologous blood. Patients were seen on postoperative day 1, 1 week, 1 month, 6 months, and 1 year after surgery. Graft stability and pterygium recurrence were graded by an independent observer who was masked to the method of treatment.
RESULTS: All 120 eyes completed the 1-year follow-up. Graft loss was seen only in the autologous blood group. Of the 62 eyes in this group, a total of 15 (24.2%) grafts dislodged. Recurrence was calculated after excluding grafts that were dislodged. Of the 105 patients, there were a total of 7 recurrences, 2 (3.4%) from the fibrin adhesive method and 5 (10.6%) from the autologous blood method. This was not statistically significant (P = 0.238).
CONCLUSIONS: Autologous blood does not exhibit similar graft stability seen with fibrin glue. Although the recurrence rate may not be significant, careful patient selection and a standard method needs to be laid out before the use of this method is widely accepted.
MATERIALS AND METHODS: Sound extracted human molars were randomly divided into: manufacturer's instructions (MI), manual blend 2 mm (MB2), and manual blend 4 mm (MB4). Occlusal enamel was removed and flattened, dentin surfaces were bonded by Prime & Bond universal (Dentsply and Optibond FL, Kerr). For the MI group, adhesives were applied following the manufacturer's instructions then light-cured. For MB groups, SDR flow+ bulk-fill flowable composite resin was applied in 2- or 4-mm increment then manually rubbed by a micro brush for 15 s with uncured dentine bonding agents and the mixture was light-cured. Composite buildup was fabricated incrementally using Ceram.X One, Dentsply nanohybrid composite resin restorative material. After 24-h water storage, the teeth were sectioned to obtain beams of about 0.8 mm2 for 24-h and thermocycled micro-tensile bond strength at 0.5 mm/min crosshead speed. Degree of conversion was evaluated with micro-Raman spectroscopy. Contraction gaps at 24 h after polymerization were evaluated and atomic force microscopy (AFM) nano-indentation processes were undertaken for measuring the hardness across the interface. Depth of resin penetration was studied using a scanning electron microscope (SEM). Bond strength data was expressed using two-way ANOVA followed by Tukey's test. Nanoindentation hardness was separately analyzed using one-way ANOVA.
RESULTS: Factors "storage F = 6.3" and "application F = 30.11" significantly affected the bond strength to dentine. For Optibond FL, no significant difference in nanoleakage was found in MI/MB4 groups between baseline and aged specimens; significant difference in nanoleakage score was observed in MB2 groups. Confocal microscopy analysis showed MB2 Optibond FL and Prime & Bond universal specimens diffusing within the dentine. Contraction gap was significantly reduced in MB2 specimens in both adhesive systems. Degree of conversion (DC) of the MB2 specimens were numerically more compared to MS1 in both adhesive systems.
CONCLUSION: Present study suggests that the new co-blend technique might have a positive effect on bond strengths of etch-and-rinse adhesives to dentine.
METHODS: Six makes, three each monocrystalline (M) and polycrystalline (P) were used; PureSapphire (M), SPA Aesthetic (M), Ghost (M), Mist (P), Reflections (P), and Dual Ceramic (P). The Ortholux™ Light Curing Unit (LCU) was used to cure the orthodontic adhesive Transbond™XT. The LCU's tip irradiance was measured and TLE transmitted through the ceramic bracket was obtained, then adhesive added to the bracket, and transmitted TLE measured through bracket-plus-adhesive samples. The LCU was set at five seconds as recommended for curing adhesive through ceramic brackets.
RESULTS: Mean tip irradiance was 1859.2±16.2mW/cm2. The TLE transmitted through brackets alone ranged 1.7 to 3.9J/cm2, in the descending order: Ghost>Pure Sapphire>Reflections>Mist>SPA Aesthetics>Dual Ceramic. The TLE transmitted through bracket-plus-adhesive samples ranged 1.6 to 3.7J/cm2, in the descending order: Ghost>Mist>Reflections>Pure Sapphire>SPA Aesthetics>Dual Ceramic. TLE was reduced with the addition of adhesive (range -0.1 to -0.7J/cm2). There was a significant difference for Pure Sapphire, Reflections, and Mist (P<0.05), but not for SPA Aesthetics, Ghost, and Dual Ceramic. There was no overall significant difference between the monocrystalline and polycrystalline makes. The two best makes were of the monocrystalline type, concerning TLE transmission, but with the exception of polycrystalline Dual Ceramic; the next worst make was a monocrystalline bracket, SPA Aesthetics.
CONCLUSION: Light energy attenuation through ceramic orthodontic brackets is make-dependent, with no overall difference between monocrystalline and polycrystalline brackets. Light energy is further attenuated with the addition of resin-based orthodontic adhesive.