  1. Mat Yazik MH, Sultan MTH, Jawaid M, Abu Talib AR, Mazlan N, Md Shah AU, et al.
    Polymers (Basel), 2021 Feb 25;13(5).
    PMID: 33669149 DOI: 10.3390/polym13050700
    The aim of the present study has been to evaluate the effect of hybridization of montmorillonite (MMT) and multi-walled carbon nanotubes (MWCNT) on the thermal and viscoelastic properties of shape memory epoxy polymer (SMEP) nanocomposites. In this study, ultra-sonication was utilized to disperse 1%, 3%, and 5% MMT in combination with 0.5%, 1%, and 1.5% MWCNT into the epoxy system. The fabricated SMEP hybrid nanocomposites were characterized via differential scanning calorimetry, dynamic mechanical analysis, and thermogravimetric analysis. The storage modulus (E'), loss modulus (E"), tan δ, decomposition temperature, and decomposition rate, varied upon the addition of the fillers. Tan δ indicated a reduction of glass transition temperature (Tg) for all the hybrid SMEP nanocomposites. 3% MMT/1% MWCNT displayed best overall performance compared to other hybrid filler concentrations and indicated a better mechanical property compared to neat SMEP. These findings open a way to develop novel high-performance composites for various potential applications, such as morphing structures and actuators, as well as biomedical devices.
  2. Meraj A, Jawaid M, Singh SP, Nasef MM, Ariffin H, Fouad H, et al.
    Sci Rep, 2024 Apr 15;14(1):8672.
    PMID: 38622317 DOI: 10.1038/s41598-024-59200-6
    Extraction of lignin via green methods is a crucial step in promoting the bioconversion of lignocellulosic biomasses. In the present study, utilisation of natural deep eutectic solvent for the pretreatment of kenaf fibres biomass is performed. Furthermore, extracted lignin from natural deep eutectic solvent pretreated kenaf biomass was carried out and its comparative study with commercial lignin was studied. The extracted lignin was characterized and investigated through Infrared Fourier transform spectroscopy, X-ray Diffraction, thermogravimetric analysis, UV-Vis spectroscopy, and scanning electron microscopy. FTIR Spectra shows that all samples have almost same set of absorption bands with slight difference in frequencies. CHNS analysis of natural deep eutectic solvent pretreated kenaf fibre showed a slight increase in carbon % from 42.36 to 43.17% and an increase in nitrogen % from - 0.0939 to - 0.1377%. Morphological analysis of commercial lignin shows irregular/uneven surfaces whereas natural deep eutectic solvent extracted lignin shows smooth and wavy surface. EDX analysis indicated noticeable peaks for oxygen and carbon elements which are present in lignocellulosic biomass. Thermal properties showed that lignin is constant at higher temperatures due to more branching and production of extremely condensed aromatic structures. In UV-VIS spectroscopy, commercial lignin shows slightly broad peak between 300 and 400 nm due to presence of carbonyl bond whereas, natural deep eutectic solvent extracted lignin does not show up any peak in this range. XRD results showed that the crystallinity index percentage for kenaf and natural deep eutectic solvent treated kenaf was 70.33 and 69.5% respectively. Therefore, these innovative solvents will undoubtedly have significant impact on the development of clean, green, and sustainable products for biocatalysts, extraction, electrochemistry, adsorption applications.
  3. Mohamad Haafiz MK, Eichhorn SJ, Hassan A, Jawaid M
    Carbohydr Polym, 2013 Apr 2;93(2):628-34.
    PMID: 23499105 DOI: 10.1016/j.carbpol.2013.01.035
    In this work, we successfully isolated microcrystalline cellulose (MCC) from oil palm empty fruit bunch (OPEFB) fiber-total chlorine free (TCF) pulp using acid hydrolysis method. TCF pulp bleaching carried out using an oxygen-ozone-hydrogen peroxide bleaching sequence. Fourier transform infrared (FT-IR) spectroscopy indicates that acid hydrolysis does not affect the chemical structure of the cellulosic fragments. The morphology of the hydrolyzed MCC was investigated using scanning electron microscopy (SEM), showing a compact structure and a rough surface. Furthermore, atomic force microscopy (AFM) image of the surface indicates the presence of spherical features. X-ray diffraction (XRD) shows that the MCC produced is a cellulose-I polymorph, with 87% crystallinity. The MCC obtained from OPEFB-pulp is shown to have a good thermal stability. The potential for a range of applications such as green nano biocomposites reinforced with this form of MCC and pharmaceutical tableting material is discussed.
  4. Mohamad N, Mazlan MM, Tawakkal ISMA, Talib RA, Kian LK, Fouad H, et al.
    Int J Biol Macromol, 2020 Nov 15;163:1451-1457.
    PMID: 32738328 DOI: 10.1016/j.ijbiomac.2020.07.209
    The growing global awareness for environmental protection has inspired the exploration on producing active packaging films from bio-based materials. In present work, three types of active agents were studied by incorporating thymol(T), kesum(K), and curry(C) (10% wt.) into polylactic acid (PLA) to produce PLA-10T, PLA-10K, and PLA10-C packaging films via solvent casting method. The morphology, functional chemistry, thermal stability, permeability, and antimicrobial properties were evaluated for PLA films. Functional chemical analysis confirmed the presence of interfacial bonding between aromatic groups of active agents and PLA carbonyl group. PLA-10K exhibited the highest thermal resistance comparing to PLA-10T and PLA-10C while water vapor barrier was enhanced after incorporation of active agents. Qualitative observation had indicated that chicken meat could be preserved in the active films until 15 days, while odourless and firm texture properties retained in food sample. For disc diffusion assay (in vitro), it showed positive results against Gram-positive bacteria (Staphylococcus aureus) whereas with negative results against Gram-negative bacteria (Escherichia coli) and Aspergillus Brasiliensis due to embedded active agents within PLA matrix. We concluded that produced active agents filled PLA films potential to use in food packaging application to enhance the shelf life of meats, fruits and vegetables product.
  5. Mohd Hawari N, Jawaid M, Md Tahir P, Azmeer RA
    Disabil Rehabil Assist Technol, 2017 Nov;12(8):868-874.
    PMID: 28068847 DOI: 10.1080/17483107.2016.1269209
    The aim of this case study was to explore patient satisfaction with the quality of prosthetic leg sockets intended for persons with lower limb amputations. A qualitative study based on in-depth interviews, preceded by a questionnaire session, was carried out with patients from the Rehabilitation Center and Hospital in Malaysia. Twelve out-patient and in-patient amputees with lower limb amputations, specifically below-knee amputations, were chosen randomly. The analysis of patients' narratives aimed to identify the functional and esthetic characteristics of currently used prosthetic leg sockets and any problems related to them. The obtained results indicated that out of the 12 participants, 41.7% and 25% were satisfied and somewhat satisfied with their current prosthetic sockets. Durability and comfort were rated by the participants as the most important characteristics of prosthetic sockets, with 83.3%. As regards the esthetic appearance of the socket, 66.7% of the respondents considered that the most important feature was the material from which the socket was fabricated. Thus, we conclude that current satisfaction levels with the quality of prosthetic sockets among amputees in Malaysia are suitable, prosthesis being preferred by many amputees. The results can be used to direct future research on cosmesis and functionality of prosthetic socket design. Implications for Rehabilitation Case study will help participants to get cost effective prosthetic leg socket. Develop prosthetic leg socket comfortable as comparative to existing one. Help Malaysian government to make policy to develop local prosthetic leg socket at affordable price.
    Study site: Cheras Rehabilitation Hospital in Kuala Lumpur, Perkeso Rehab Center in Melaka, Pusat Latihan dan Perindustrian Bangi and Rumah Insaniah Tun Dr Siti Hasmah Ptaling Jaya in Selangor, Malaysia
  6. Muthulakshmi L, Rajini N, Nellaiah H, Kathiresan T, Jawaid M, Rajulu AV
    Int J Biol Macromol, 2017 Feb;95:1064-1071.
    PMID: 27984140 DOI: 10.1016/j.ijbiomac.2016.09.114
    In the present work, copper nanoparticles (CuNPs) were in situ generated inside cellulose matrix using Terminalia catappa leaf extract as a reducing agent. During this process, some CuNPs were also formed outside the matrix. The CuNPs formed outside the matrix were observed with transmission electron microscope (TEM) and scanning electron microscope (SEM). Majority of the CuNPs formed outside the matrix were in the size range of 21-30nm. The cellulose/CuNP composite films were characterized by Fourier transform infrared spectroscopic, X-Ray diffraction and thermogravimetric techniques. The crystallinity of the cellulose/CuNP composite films was found to be lower than that of the matrix indicating rearrangement of cellulose molecules by in situ generated CuNPs. Further, the expanded diffractogram of the composite films indicated the presence of a mixture of Cu, CuO and Cu2O nanoparticles. The thermal stability of the composites was found to be lower than that of the composites upto 350°C beyond which a reverse trend was observed. This was attributed to the catalytic behaviour of CuNPs for early degradation of the composites. The composite films possessed sufficient tensile strength which can replace polymer packaging films like polyethylene. Further, the cellulose/CuNP composite films exhibited good antibacterial activity against E.coli bacteria.
  7. Najeeb MI, Hameed Sultan MT, Md Shah AU, Muhammad Amir SM, Safri SNA, Jawaid M, et al.
    Polymers (Basel), 2021 Sep 21;13(18).
    PMID: 34578095 DOI: 10.3390/polym13183194
    The low-velocity impact behaviour of pineapple leaf fiber, PALF reinforce epoxy composite (P), PALF hybrid (GPG), and four-layer woven glass fiber (GGGG) composite was investigated. As for post-impact analysis, the damage evaluation was assessed through photographic images and X-ray computed tomography, using CT scan techniques. The key findings from this study are that a positive hybrid effect of PALF as a reinforcement was seen where the GPG shows the delayed time taken for damage initiation and propagation through the whole sample compared to GGGG. This clearly shows that the addition of fibers does have comparable composite properties with a fully synthetic composite. Through the visual inspection captured by photographic image, the presence of woven fiber glass mat in GPG presents a different damage mode compared to P. Moreover, CT scan results show extended internal damage at the cross-section of all impacted composite.
  8. Namvar F, Tahir PM, Mohamad R, Mahdavi M, Abedi P, Najafi TF, et al.
    Nat Prod Commun, 2013 Dec;8(12):1811-20.
    PMID: 24555303
    This review article summarizes in vitro and in vivo experiments on seaweed anticancer activity and seaweed chemical components. Seaweed use in cancer therapy, chemopreventive randomized control trials (RCTs) and quasi-experiments are discussed. The literature reviewed in this article was obtained from various scientific sources and encompasses publications from 2000-2012. Seaweed therapeutic effects were deemed scientifically plausible and may be partially explained by the in vivo and in vitro pharmacological studies described. Although the mechanisms of action remain unclear, seaweed's anticancer properties may be attributable to its major biologically active metabolites. Much of the seaweed research outlined in this paper can serve as a foundation for explaining seaweed anticancer bioactivity. This review will open doors for developing strategies to treat malignancies using seaweed natural products.
  9. Naveen J, Jawaid M, Goh KL, Reddy DM, Muthukumar C, Loganathan TM, et al.
    Nanomaterials (Basel), 2021 May 08;11(5).
    PMID: 34066661 DOI: 10.3390/nano11051239
    The development of armour systems with higher ballistic resistance and light weight has gained considerable attention as an increasing number of countries are recognising the need to build up advanced self-defence system to deter potential military conflicts and threats. Graphene is a two dimensional one-atom thick nanomaterial which possesses excellent tensile strength (130 GPa) and specific penetration energy (10 times higher than steel). It is also lightweight, tough and stiff and is expected to replace the current aramid fibre-based polymer composites. Currently, insights derived from the study of the nacre (natural armour system) are finding applications on the development of artificial nacre structures using graphene-based materials that can achieve high toughness and energy dissipation. The aim of this review is to discuss the potential of graphene-based nanomaterials with regard to the penetration energy, toughness and ballistic limit for personal body armour applications. This review addresses the cutting-edge research in the ballistic performance of graphene-based materials through theoretical, experimentation as well as simulations. The influence of fabrication techniques and interfacial interactions of graphene-based bioinspired polymer composites for ballistic application are also discussed. This review also covers the artificial nacre which is shown to exhibit superior mechanical and toughness behaviours.
  10. Naveen J, Jawaid M, Zainudin ES, Thariq Hameed Sultan M, Yahaya R
    Materials (Basel), 2019 Apr 16;12(8).
    PMID: 30988270 DOI: 10.3390/ma12081249
    This research investigated the effect of adding different wt.% (0, 0.25, 0.50, and 0.75) of GNP (graphene nanoplatelets) to improve the mechanical and moisture resistant properties of Kevlar (K)/cocos nucifera sheath (CS)/epoxy hybrid composites. The laminates were fabricated with different K/CS weight ratios such as 100/0 (S1), 75/25 (S2), 50/50 (S3), 25/75 (S4), and 0/100 (S5). The results revealed that the addition of GNP improved the tensile, flexural, and impact properties of laminated composites. However, the optimal wt.% of GNP varies with different laminates. A moisture diffusion analysis showed that the laminates with a 0.25 wt.% of GNP content efficiently hindered water uptake by closing all the unoccupied pores inside the laminate. Morphological investigations (SEM and FE-SEM (Field Emission Scanning Electron Microscope)) proved that the addition of GNP improved the interfacial adhesion and dispersion. Structural (XRD and FTIR) analyses reveals that at 0.25 wt.% of GNP, all the hybrid composites showed a better crystallinity index and the functional groups presents in the GNP can form strong interactions with the fibers and matrix. A statistical analysis was performed using One-way ANOVA, and it corroborates that the mechanical properties of different laminates showed a statistically significant difference. Hence, these GNP-modified epoxy hybrid composites can be efficiently utilized in load-bearing structures.
  11. Nurhanisah MH, Jawaid M, Ahmad Azmeer R, Paridah MT
    Disabil Rehabil Assist Technol, 2019 07;14(5):513-520.
    PMID: 29933703 DOI: 10.1080/17483107.2018.1479782
    This study describes a newly developed prosthetic leg socket design for a below-knee amputation. Excessive heat and the resulted perspiration within a prosthetic socket were the most common causes for reporting a reduced quality of life for prosthetic users. The product namely AirCirc means air circulation and it has been designed by approach of medical device design process in providing the amputees to maintain the skin temperature inside the socket. This device has been designed to provide the amputees with comfort and ultimate breathable. In order to design the device, the small hole was made in prosthetic socket surface since it has a function as air circulation. Four types of proposed sockets namely P1, P2, P3 and P4 and one control socket were compared on a single patient to determine the best design of prosthetic socket. The result successfully reveals that by using holes can be maintain the temperature inside prosthetic socket. In addition to the eco-friendly material, the woven kenaf was used as material that provides good strength as compared to glass fibre and offer sustainable and biodegradable product yet provides unique and aesthetic surface as came from woven kenaf itself. The objective of this paper is to provide the airflow prosthetic socket design and optimize the use of natural fibre in prostheses field. Thus, with the use of the environmental friendly material, functionality device and heat removal capability make the device suitable for maintaining a comfortable and healthy environment for prosthesis. Implications of Rehabilitation Newly developed prosthetic leg socket design for a below-knee amputation Device has been designed to provide the amputees with comfort and ultimate breathable Woven kenaf was used as material that provides good strength as compared to glass fibre for sustainable and biodegradable product Results show that by using holes can be maintain the temperature inside prosthetic socket.
  12. Radakisnin R, Abdul Majid MS, Jamir MRM, Jawaid M, Sultan MTH, Mat Tahir MF
    Materials (Basel), 2020 Sep 17;13(18).
    PMID: 32957438 DOI: 10.3390/ma13184125
    The purpose of the study is to investigate the utilisation of Napier fiber (Pennisetum purpureum) as a source for the fabrication of cellulose nanofibers (CNF). In this study, cellulose nanofibers (CNF) from Napier fiber were isolated via ball-milling assisted by acid hydrolysis. Acid hydrolysis with different molarities (1.0, 3.8 and 5.6 M) was performed efficiently facilitate cellulose fiber size reduction. The resulting CNFs were characterised through Fourier-transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), thermogravimetric analysis (TGA), particle size analyser (PSA), field-emission scanning electron microscopy (FESEM), atomic force microscopy (AFM), and transmission electron microscopy (TEM). The FTIR results demonstrated that there were no obvious changes observed between the spectra of the CNFs with different molarities of acid hydrolysis. With 5.6 M acid hydrolysis, the XRD analysis displayed the highest degree of CNF crystallinity at 70.67%. In a thermal analysis by TGA and DTG, cellulose nanofiber with 5.6 M acid hydrolysis tended to produce cellulose nanofibers with higher thermal stability. As evidenced by the structural morphologies, a fibrous network nanostructure was obtained under TEM and AFM analysis, while a compact structure was observed under FESEM analysis. In conclusion, the isolated CNFs from Napier-derived cellulose are expected to yield potential to be used as a suitable source for nanocomposite production in various applications, including pharmaceutical, food packaging and biomedical fields.
  13. Rahman MR, Hamdan S, Lai JCH, Jawaid M, Yusof FABM
    Heliyon, 2017 Jul;3(7):e00342.
    PMID: 28725868 DOI: 10.1016/j.heliyon.2017.e00342
    In this study, the physical, morphological, mechanical and thermal properties of furfuryl alcohol/2-ethylhexyl methacrylate/halloysite nanoclay wood polymer nanocomposites (FA-co-EHMA-HNC WPNCs) were investigated. FA-co-EHMA-HNC WPNCs were prepared via an impregnation method and the properties of the nanocomposites were characterized through the weight percent gain, Fourier transform infrared (FT-IR) spectroscopy, scanning electron microscopy (SEM), three-point flexural test, dynamic mechanical thermal analysis (DMTA), thermogravimetric analysis (TGA), differential scanning calorimetry (DSC) analysis and moisture absorption test. The weight percent gain in the 50:50 FA-co-EHMA-HNC WPNC was the highest compared with the raw wood (RW) and other WPNCs. The FT-IR results confirmed that polymerization took place in the nanocomposites, especially 50:50 FA-co-EHMA-HNC WPNC, which had a reduced amount of hydroxyl groups. The SEM results revealed that the 50:50 FA-co-EHMA-HNC WPNC had the smoothest and most uniform surface among all of the nanocomposites. The 50:50 FA-co-EHMA-HNC WPNC showed the highest flexural strength and modulus of elasticity. The results revealed that the storage modulus and loss modulus of the FA-co-EHMA-HNC WPNCs were higher and the tan δ of FA-co-EHMA-HNC WNPCs was lower compared with the RW. The FA-co-EHMA-HNC WPNCs exhibited the higher thermal stability in the TGA and DSC analysis. The 50:50 FA-co-EHMA-HNC WPNC exhibited remarkably lower moisture absorption compared with the RW. Overall, this study proved that the ratio 50:50 FA-co-EHMA ratio was the most suitable for introduction in the in the RW.
  14. Rangappa SM, Parameswaranpillai J, Siengchin S, Jawaid M, Ozbakkaloglu T
    Sci Rep, 2022 01 10;12(1):397.
    PMID: 35013525 DOI: 10.1038/s41598-021-04386-2
    In this work, fillers of waste chicken feather and abundantly available lignocellulose Ceiba Pentandra bark fibers were used as reinforcement with Biopoxy matrix to produce the sustainable composites. The aim of this work was to evaluate the mechanical, thermal, dimensional stability, and morphological performance of waste chicken feather fiber/Ceiba Pentandra bark fiber filler as potential reinforcement in carbon fabric-layered bioepoxy hybrid composites intended for engineering applications. These composites were prepared by a simple, low cost and user-friendly fabrication methods. The mechanical (tensile, flexural, impact, hardness), dimensional stability, thermal stability, and morphological properties of composites were characterized. The Ceiba Pentandra bark fiber filler-reinforced carbon fabric-layered bioepoxy hybrid composites display better mechanical performance compared to chicken feather fiber/Ceiba Pentandra bark fiber reinforced carbon fabrics layered bioepoxy hybrid composites. The Scanning electron micrographs indicated that the composites exhibited good adhesion at the interface of the reinforcement material and matrix system. The thermogravimetric studies revealed that the composites possess multiple degradation steps, however, they are stable up to 300 °C. The thermos-mechanical studies showed good dimensional stability of the composites. Both studied composites display better thermal and mechanical performance compared to neat bioepoxy or non-bioepoxy thermosets and are suitable for semi-structural applications.
  15. Rasheed M, Jawaid M, Parveez B, Zuriyati A, Khan A
    Int J Biol Macromol, 2020 Oct 01;160:183-191.
    PMID: 32454108 DOI: 10.1016/j.ijbiomac.2020.05.170
    This work investigates the extraction of cellulose nanocrystals (CNC) from bamboo fibre as an alternative approach to utilize the waste bamboo fibre. In this study, bamboo fibre was subjected to acid hydrolysis for efficient isolation of CNC from bamboo fibre. The extracted CNC's were morphologically, characterized via Scanning Electron Microscopy (SEM), Transmission Electron Microscopy (TEM) and Atomic Force Microscopy (AFM). The energy Dispersive X-rays (EDX) provided the elemental composition of the prepared CNC's and X-ray diffractometer (XRD) exhibited their crystallinity. The physiochemical analysis was done via Fourier Transform Infrared (FTIR); and their thermal analysis was revealed by Thermogravimetric Analysis (TGA) and Differential scanning calorimetry (DSC). As from their morphological investigations, rod like structures of CNC's were observed under SEM analysis with higher carbon content as demonstrated by EDX, while needle shaped CNC's were observed from TEM and AFM studies. Acid hydrolysis for 45 min resulted into higher degree of crystallinity and higher yield of CNC's about 86.96% and 22% respectively. Owing to higher quality of CNC's obtained as a result of efficient and modified techniques, these can find potential usage in nanocomposites for biomedical and food packaging application.
  16. Rasheed M, Jawaid M, Parveez B, Hussain Bhat A, Alamery S
    Polymers (Basel), 2021 Feb 01;13(3).
    PMID: 33535490 DOI: 10.3390/polym13030465
    The present study aims to develop a biodegradable polymer blend that is environmentally friendly and has comparable tensile and thermal properties with synthetic plastics. In this work, microcrystalline cellulose (MCC) extracted from bamboo-chips-reinforced poly (lactic acid) (PLA) and poly (butylene succinate) (PBS) blend composites were fabricated by melt-mixing at 180 °C and then hot pressing at 180 °C. PBS and MCC (0.5, 1, 1.5 wt%) were added to improve the brittle nature of PLA. Field emission scanning electron microscopy (FESEM), scanning electron microscopy (SEM), X-ray diffraction (XRD), Fourier transform infrared spectroscope (FTIR), thermogravimetric analysis (TGA), differential thermogravimetry (DTG), differential scanning calorimetry (DSC)), and universal testing machine were used to analyze morphology, crystallinity, physiochemical, thermal, and tensile properties, respectively. The thermal stability of the PLA-PBS blends enhanced on addition of MCC up to 1wt % due to their uniform dispersion in the polymer matrix. Tensile properties declined on addition of PBS and increased with MCC above (0.5 wt%) however except elongation at break increased on addition of PBS then decreased insignificantly on addition of MCC. Thus, PBS and MCC addition in PLA matrix decreases the brittleness, making it a potential contender that could be considered to replace plastics that are used for food packaging.
  17. Rasheed M, Jawaid M, Karim Z, Abdullah LC
    Molecules, 2020 Jun 18;25(12).
    PMID: 32570929 DOI: 10.3390/molecules25122824
    Bamboo fibers are utilized for the production of various structures, building materials, etc. and is of great significance all over the world especially in southeast Asia. In this study, the extraction of microcrystalline cellulose (MCC) was performed using bamboo fibers through acid hydrolysis and subsequently different characterizations were carried out using various advanced techniques. Fourier transform infrared (FTIR) spectroscopy analysis has indicated the removal of lignin from MCC extracted from bamboo pulp. Scanning Electron Microscopy (SEM) revealed rough surface and minor agglomeration of the MCC. Pure MCC, albeit with small quantities of impurities and residues, was obtained, as revealed by Energy Dispersive X-ray (EDX) analysis. X-ray diffraction (XRD) indicates the increase in crystallinity from 62.5% to 82.6%. Furthermore, the isolated MCC has slightly higher crystallinity compared to commercial available MCC (74%). The results of thermal gravimetric analysis (TGA) demonstrate better thermal stability of isolated MCC compared to its starting material (Bamboo fibers). Thus, the isolated MCC might be used as a reinforcing element for the production of green composites and it can also be utilized as a starting material for the production of crystalline nanocellulose in future.
  18. Rasheed M, Jawaid M, Parveez B
    Polymers (Basel), 2021 Mar 29;13(7).
    PMID: 33805433 DOI: 10.3390/polym13071076
    The purpose of this work was to investigate the effect of cellulose nanocrystals (CNC) from bamboo fiber on the properties of poly (lactic acid) (PLA)/poly (butylene succinate) (PBS) composites fabricated by melt mixing at 175 °C and then hot pressing at 180 °C. PBS and CNC (0.5, 0.75, 1, 1.5 wt.%) were added to improvise the properties of PLA. The morphological, physiochemical and crystallinity properties of nanocomposites were analysed by field emission scanning electron microscope (FESEM), Fourier-transform infrared spectroscopy (FTIR) and X-ray diffractometry (XRD), respectively. The thermal and tensile properties were analysed by thermogravimetic analysis (TGA), Differential scanning calorimetry (DSC) and Universal testing machine (UTM). PLA-PBS blend shows homogeneous morphology while the composite shows rod-like CNC particles, which are embedded in the polymer matrix. The uniform distribution of CNC particles in the nanocomposites improves their thermal stability, tensile strength and tensile modulus up to 1 wt.%; however, their elongation at break decreases. Thus, CNC addition in PLA-PBS matrix improves structural and thermal properties of the composite. The composite, thus developed, using CNC (a natural fiber) and PLA-PBS (biodegradable polymers) could be of immense importance as they could allow complete degradation in soil, making it a potential alternative material to existing packaging materials in the market that could be environment friendly.
  19. Saba N, Safwan A, Sanyang ML, Mohammad F, Pervaiz M, Jawaid M, et al.
    Int J Biol Macromol, 2017 Sep;102:822-828.
    PMID: 28455253 DOI: 10.1016/j.ijbiomac.2017.04.074
    The current study presents about the effect of cellulose nanofibers (CNFs) filler on the thermal and dynamic mechanical analysis (DMA) of epoxy composites as a function of temperature. In this study hand lay-up method was used to fabricate CNF reinforced Epoxy nanocomposites with CNF loading of 0.5%, 0.75%, and 1% into epoxy resin. The obtained thermal and DMA results illustrates that thermal stability, char content, storage modulus (E'), loss modulus (E") and glass transition temperature (Tg) increases for all CNF/epoxy nanocomposites compared to the pure epoxy. Thermal results revealed that 0.75% offers superior resistance or stability towards heat compared to its counterparts. In addition, 0.75% CNF/epoxy nanocomposites confers highest value of storage modulus as compared to 0.5% and 1% filler loading. Hence, it is concluded that 0.75% CNFs loading is the minimal to enhance both thermal and dynamic mechanical properties of the epoxy composites and can be utilized for advance material applications where thermal stability along with renewability are prime requirements.
  20. Saba N, Mohammad F, Pervaiz M, Jawaid M, Alothman OY, Sain M
    Int J Biol Macromol, 2017 Apr;97:190-200.
    PMID: 28082223 DOI: 10.1016/j.ijbiomac.2017.01.029
    Present study, deals about isolation and characterization of cellulose nanofibers (CNFs) from the Northern Bleached Softwood Kraft (NBSK) pulp, fabrication by hand lay-up technique and characterization of fabricated epoxy nanocomposites at different filler loadings (0.5%, 0.75%, 1% by wt.). The effect of CNFs loading on mechanical (tensile, impact and flexural), morphological (scanning electron microscope and transmission electron microscope) and structural (XRD and FTIR) properties of epoxy composites were investigated. FTIR analysis confirms the introduction of CNFs into the epoxy matrix while no considerable change in the crystallinity and diffraction peaks of epoxy composites were observed by the XRD patterns. Additions of CNFs considerably enhance the mechanical properties of epoxy composites but a remarkable improvement is observed for 0.75% CNFs as compared to the rest epoxy nanocomposites. In addition, the electron micrographs revealed the perfect distribution and dispersion of CNFs in the epoxy matrix for the 0.75% CNFs/epoxy nanocomposites, while the existence of voids and agglomerations were observed beyond 0.75% CNFs filler loadings. Overall results analysis clearly revealed that the 0.75% CNFs filler loading is best and effective with respect to rest to enhance the mechanical and structural properties of the epoxy composites.
Filters
Contact Us

Please provide feedback to Administrator (afdal@afpm.org.my)

External Links