MATERIAL AND METHOD: Two hundred discs of PEEK were prepared of 6 mm × 2 mm × 10 mm dimension. The discs were randomly divided into five groups (n = 40) for treatment, Group I: treatment with deionized distilled water (control group); Group II: PD therapy using curcumin PS; Group III: discs treated and abraded with air-borne particles (ABP) silica (30 μm particle size) modified alumina (Al); Group IV: ABP of alumina (110 μm particle size); and Group V: The PEEK were finished with 600-μm grit size straight diamond cutting bur installed in high speed hand-piece. The surface profilometer was used to evaluate the values of surface roughness (SRa) of pretreated PEEK discs. The discs were luted and bonded to discs of composite resin. The bonded PEEK samples were placed in Universal testing machine to evaluate shear BS. The type of BS failure for PEEK discs pre-treated with five regimes respectively was evaluated under stereo-microscope. The data was statistically analyzed using one-way ANOVA and the comparisons between mean values of shear BS were evaluated by Tukey's test (ρ≤0.05).
RESULTS: The PEEK samples pre-treated with diamond cutting straight fissure burs displayed statistically significant highest value of SRa values (3.258± 0.785 µm). Similarly, the shear BS was observed to be higher for the PEEK discs pre-treated with straight fissure bur (22.37±0.78 MPa). A comparable difference but not statistically significant difference was observed between PEEK discs pre-treated by curcumin PS and ABP-silica modified alumina (ρ ≥ 0.05).
CONCLUSION: PEEK discs pre-treated with diamond grit straight fissure bur displayed highest values of SRa and shear BS. It was trailed by ABP-Al pre-treated discs; whereas the SRa and shear BS values for the discs pre-treated with ABP-silica modified Al and curcumin PS did not show competitive difference.
Materials and Methods: Ninety aluminum oxide ceramic (Turkom-Ceramic Sdn. Bhd., Kuala Lumpur, Malaysia) specimens were produced and divided into nine groups to receive the following surface treatments: control group, no treatment (Group C), sandblasting (Group B), silica coating (Group S), erbium: yttrium-aluminum-garnet (Er:YAG) laser irradiation at 150 mJ 10 Hz (Group L1), Er:YAG laser irradiation at 300 mJ 10 Hz (Group L2), sandblasting + L1 (Group BL1), sandblasting + L2 (Group BL2), silica coating + L1 (Group SL1), and silica coating + L2 (Group SL2). After surface treatments, surface roughness (SR) values were measured and surface topography was evaluated. Resin cement was applied on the specimen surface, and shear bond strength (SBS) tests were performed. Data were statistically analyzed using one-way ANOVA and Tukey's multiple comparisons at a significance level of P < 0.05.
Results: Group S, SL1, and SL2 showed significantly increased SR values compared to the control group (P < 0.05); therefore, no significant differences were found among the SR values of Groups B, BL1, BL2, L1, and L2 and the control group (P > 0.05). Group S showed the highest SBS values, whereas the control group showed the lowest SBS values.
Conclusion: Silica coating is the most effective method for resin bonding of high strength ceramic, but Er:YAG laser application decreased the effectiveness.