In this work, nanocomposite ultrafiltration (UF) membranes were synthesized through addition of different quantities of amino-functionalized nanocrystalline cellulose (NCs) in order to improve membrane anti-fouling resistance against oil depositions. The characterization results demonstrated that the overall porosity and hydrophilicity of the membranes were improved significantly upon addition of NCs despite a decrease in the pore size of nanocomposite membranes. The UF performance results showed that the nanocomposite membrane incorporated with 1 wt% NCs achieved an optimal water flux improvement, i.e., approximately 43% higher than the pristine membrane. Such nanocomposite membrane also exhibited promising oil rejection (>98.2%) and excellent water flux recovery rate of ˜98% and ˜85% after one and four cycles of treating 250-ppm oil-in-water emulsion solution, respectively. The desirable anti-fouling properties of nanocomposite membrane can be attributed to the existence of hydrophilic functional groups (-OH) on the surface of membrane stemming from addition of NCs that renders the membrane less vulnerable to fouling during oil-in-water emulsion treatment.
This article demonstrates a novel nanoscale surface modification method to enhance the selectivity of porous poly(dimethylsiloxane) (PDMS) in removing oil from water. The surface modification method is simple and low cost by using sugar as a sacrificial template for temporal adhering of carbon nanotubes (CNT) before addition of PDMS prepolymer to encapsulate the CNT on its surface once polymerized. The PDMS-CNT demonstrated a tremendous increase in absorption capacity up to 3-fold compared to previously reported absorbents composed solely of PDMS. Besides showcasing excellent absorption capacity, the PDMS-CNT also shows a faster absorption rate (25 s) as compared to that of pure PDMS (40 s). The enhanced absorption rate is due to the incorporation of CNT, which roughens the surface of the polymer at the nanoscale and lowers the surface energy of porous PDMS while at the same time increasing the absorbent hydrophobicity and oleophilicity. This property makes the absorbent unique in absorbing only oil but repelling water at the same time. The PDMS-CNT is an excellent absorbent material with outstanding recyclability and selectivity for removing oil from water.
The environment sustenance and preservation of global climate are known as the crucial issues of the world today. Currently, the crisis of global warming due to CO2 emission has turned into a paramount concern. To address such a concern, diverse CO2 capture and sequestration techniques (CCS) have been introduced so far. In line with this, Metal Organic Frameworks (MOFs) have been considered as the newest and most promising material for CO2 adsorption and separation. Due to their outstanding properties, this new class of porous materials a have exhibited a conspicuous potential for gas separation technologies especially for CO2 storage and separation. Thus, the present review paper is aimed to discuss the adsorption properties of CO2 on the MOFs based on the adsorption mechanisms and the design of the MOF structures. In addition, the main challenge associated with using this prominent porous material has been mentioned.
Asymmetric supercapacitors (ASC) have shown a great potential candidate for high-performance supercapacitor due to their wide operating potential which can remarkably enhance the capacitive behaviour. In present work, a novel positive electrode derived from functionalised carbon nanofibers/poly(3,4-ethylenedioxythiophene)/manganese oxide (f-CNFs/PEDOT/MnO2) was prepared using a multi-step route and activated carbon (AC) was fabricated as a negative electrode for ASC. A uniform distribution of PEDOT and MnO2 on f-CNFs as well as porous granular of AC are well-observed in FESEM. The assembled f-CNFs/PEDOT/MnO2//AC with an operating potential of 1.6 V can achieve a maximum specific capacitance of 537 F/g at a scan rate of 5 mV/s and good cycling stability (81.06% after cycling 8000 times). Furthermore, the as-prepared ASC exhibited reasonably high specific energy of 49.4 Wh/kg and low charge transfer resistance (Rct) of 2.27 Ω, thus, confirming f-CNFs/PEDOT/MnO2//AC as a promising electrode material for the future energy storage system.
This study was conducted to determine the influence of the oil palm boiler ash (OPBA) reinforcement on the microstructural, physical, mechanical and thermal properties of epoxy polymer composites. The chemical composition analysis of OPBA revealed that it contains about 55 wt.% of SiO2 along with other metallic oxides and elements. The surface morphology of OPBA showed angular and irregular shapes with porous structures. The influence of OPBA as a reinforcement in epoxy composite was studied with varying filler loadings (10-50 wt.%) and different particle sizes (50-150 μm). The result showed that the incorporation of OPBA in composites has improved the physical, mechanical and thermal properties of the epoxy matrix. The highest physical and mechanical properties of fabricated composites were attained with 30 wt.% loading and size of 50 μm. Also, thermal stability and the percentage of char residue of the composite increased with increasing filler loading. Furthermore, the contact angle of OPBA reinforced epoxy composites increased with the increase of filler loading. The lowest value of the contact angle was obtained at 30 wt.% of filler loading with the OPBA particle size of 50 μm. The finding of this study reveals that the OPBA has the potential to be used as reinforcement or filler as well as an alternative of silica-based inorganic fillers used in the enhancement of mechanical, physical and thermal properties of the epoxy polymer composite.
The combination of exceptional functionalities offered by 3D graphene-based macrostructures (GBMs) has attracted tremendous interest. 2D graphene nanosheets have a high chemical stability, high surface area and customizable porosity, which was extensively researched for a variety of applications including CO2 adsorption, water treatment, batteries, sensors, catalysis, etc. Recently, 3D GBMs have been successfully achieved through few approaches, including direct and non-direct self-assembly methods. In this review, the possible routes used to prepare both 2D graphene and interconnected 3D GBMs are described and analyzed regarding the involved chemistry of each 2D/3D graphene system. Improvement of the accessible surface of 3D GBMs where the interface exchanges are occurring is of great importance. A better control of the chemical mechanisms involved in the self-assembly mechanism itself at the nanometer scale is certainly the key for a future research breakthrough regarding 3D GBMs.
Infusion of saline prior to radiofrequency ablation (RFA) is known to enlarge the thermal coagulation zone. The abundance of ions in saline elevate the electrical conductivity of the saline-saturated region. This promotes greater electric current flow inside the tissue, which increases the amount of RF energy deposition and subsequently enlarges the coagulation zone. In theory, infusion of higher concentration of saline should lead to larger coagulation zone due to the greater number of ions. Nevertheless, existing studies on the effects of concentration on saline-infused RFA have been conflicting, with the exact role of saline concentration yet to be fully elucidated. In this paper, computational models of saline-infused RFA were developed to investigate the role of saline concentration on the outcome of saline-infused RFA. The elevation in tissue electrical conductivity was modelled using the microscopic mixture model, while RFA was modelled using the coupled dual porosity-Joule heating model. Results obtained indicated that the presence of a concentration threshold to which no further elevation in tissue electrical conductivity and enlargement in thermal coagulation can occur. This threshold was determined to be at 15% NaCl. Analysis of the Joule heating distribution revealed the presence of a secondary Joule heating site located along the interface between wet and dry tissue. This secondary Joule heating was responsible for the enlargement in coagulation volume and its rapid growth phase during ablation.
The present work deals with the production of paper materials from onion peels (Allium Cepa) fibers
as an alternative potential non-wood fiber. The onion peels were obtained from a local small and
medium food industry. The onion peels were cooked at 120, 150 and 180 minutes. The peels were
grinded and poured in a set of mould and deckle for the formation of a thin sheet of paper. The
physical, mechanical, morphological characteristics and water rise capillary values (KLEMM
Method) were evaluated to determine its suitability for a paper material. The results show that the
increase in cooking time from 120 to 180 minutes resulted in an increase in the tensile index from
32.28N*m/g to 42.13N*m/g and tear index from 9.80mN*m2
/g to 15.62mN*m2
/g. The bonding
strength increased due to higher number of fibers, finer fiber size, and increase in the fiber contact
area and fiber distribution. The high porosity area affects the performance of water rise capillary
values of the paper sheets. The onion peels fiber gave impressive handsheets characteristics when
compared with other sources of non-wood fibers.
This paper presents a comparative study of the characteristic of unfoamed and foamed geopolymers after exposure to elevated temperatures (200-800 °C). Unfoamed geopolymers were produced with Class F fly ash and sodium hydroxide and liquid sodium silicate. Porous geopolymers were prepared by foaming with hydrogen peroxide. Unfoamed geopolymers possessed excellent strength of 44.2 MPa and degraded 34% to 15 MPa in foamed geopolymers. The strength of unfoamed geopolymers decreased to 5 MPa with increasing temperature up to 800 °C. Foamed geopolymers behaved differently whereby they deteriorated to 3 MPa at 400 °C and increased up to 11 MPa at 800 °C. Even so, the geopolymers could withstand high temperature without any disintegration and spalling up to 800 °C. The formation of crystalline phases at higher temperature was observed deteriorating the strength of unfoamed geopolymers but enhance the strength of foamed geopolymers. In comparison, foamed geopolymer had better thermal resistance than unfoamed geopolymers as pores provide rooms to counteract the internal damage.
Ceramic foams are a class of high porosity materials that are used or being considered for a wide range of technological applications. Ceramic foam was produce by polymer replication method. In this process, commercial polymeric sponge was use as template, dipping with ceramic particles slurry, drying and then sintered to yield a replica of the original foams. The study was focus on the fabrication of different density of ceramic foams by varying the density of ceramic slurries (1.1876, 1.2687, 1.3653 and 1.5295 g/cm3). Properties of ceramic foam produced such as density was characterized accordingly to ASTM C 271-94 and porosity were characterized using Archimedes methods. Compressive and bending strength was performed accordingly to ASTM C1161-94 and C773-88 (1999), respectively. The morphological study was performed using Scanning Electron Microscopy (SEM) and EDX. Density of ceramic foams produced was about 0.5588 and 1.1852 g/cm3, where as porosity was around 26.28 and 70.59 %. Compressive and bending strength was increase from strength also increases from 2.60 to 23.07 MPa and 1.20 to 11.10 MPa, respectively, with increasing of slurries density from 1.1876 to 1.3653 g/cm3. The SEM micrographs show that the cells structure become denser as the slurries density increased. EDX proved that the ceramic used is porcelain. As a conclusion, increasing in slurries density produced ceramic foams with good mechanical properties such as compressive and bending strength and denser body.
Biocompatible metals have been revolutionizing the biomedical field, predominantly in human implant applications, where these metals widely used as a substitute to or as function restoration of degenerated tissues or organs. Powder metallurgy techniques, in specific the metal injection moulding (MIM) process, have been employed for the fabrication of controlled porous structures used for dental and orthopaedic surgical implants. The porous metal implant allows bony tissue ingrowth on the implant surface, thereby enhancing fixation and recovery. This paper elaborates a systematic classification of various biocompatible metals from the aspect of MIM process as used in medical industries. In this study, three biocompatible metals are reviewed-stainless steels, cobalt alloys, and titanium alloys. The applications of MIM technology in biomedicine focusing primarily on the MIM process setting parameters discussed thoroughly. This paper should be of value to investigators who are interested in state of the art of metal powder metallurgy, particularly the MIM technology for biocompatible metal implant design and development.
This work analyses free convection flow of a nanofluid in an inclined square enclosure consisting of a porous layer and a nanofluid layer using the finite difference methodology. Sinusoidal temperature boundary conditions are imposed on the two opposing vertical walls. Nanofluids with water as base and Ag or Cu or Al2O3 or TiO2 nanoparticles are considered for the problem. The related parameters of this study are the Darcy number, nanoparticle volume fraction, phase deviation, amplitude ratio, porous layer thickness and the inclination angle of the cavity. A comparison with previously published work is performed and the results are in good agreement. Detailed numerical data for the fluid flow and thermal distributions inside the square enclosure, and the Nusselt numbers are presented. The obtained results show that the heat transfer is considerably affected by the porous layer increment. Several nanoparticles depicted a diversity improvement on the convection heat transfer.
In-depth analyses of post-corrosion mechanical properties and architecture of open cell iron foams with hollow struts as absorbable bone scaffolds were carried out. Variations in the architectural features of the foams after 14 days of immersion in a Hanks' solution were investigated using micro-computed tomography and scanning electron microscope images. Finite element Kelvin foam model was developed, and the numerical modeling and experimental results were compared against each other. It was observed that the iron foam samples were mostly corroded in the periphery regions. Except for quasi-elastic gradient, other mechanical properties (i.e. compressive strength, yield strength and energy absorbability) decreased monotonically with immersion time. Presence of adherent corrosion products enhanced the load-bearing capacity of the open cell iron foams at small strains. The finite element prediction for the quasi-elastic response of the 14-day corroded foam was in an agreement with the experimental results. This study highlights the importance of considering corrosion mechanism when designing absorbable scaffolds; this is indispensable to offer desirable mechanical properties in porous materials during degradation in a biological environment.
Electrospinning is a promising technique for the fabrication of bioscaffolds in tissue engineering applications. Pertaining issues of multiple polymer jets and bending instabilities result in random paths which lend poor controllability over scaffolds morphology for affecting the porosity and mechanical stability. The present study alleviates these challenges by demonstrating a novel self-directing single jet taking a specifically patterned path to deposit fibers into circular and uniform scaffolds without tuning any externally controlled parameters. High-speed camera observation revealed that the charge retention and dissipation on the collected fibers caused rapid autojet switching between the two jetting modes, namely, a microcantilever-like armed jet motion and a whipping motion, which sequentially expand the area and thickness of the scaffolds, respectively, in a layered-like fashion. The physical properties showed that the self-switching dual-jet modes generated multilayered microfibrous scaffolds (MFSs) with dual morphologies and varied fiber packing density, thereby establishing the gradient porosity and mechanical strength (through buckled fibers) in the scaffolds. In vitro studies showed that as-spun scaffolds are cell-permeable hierarchical 3D microporous structures enabling lateral cell seeding into multiple layers. The cell proliferation on days 6 and 9 increased 21% and 38% correspondingly on MFSs than on nanofibrous scaffolds (NFSs) done by conventional multijets electrospinning. Remarkably, this novel and single-step process is highly reproducible and tunable for developing fibrous scaffolds for tissue engineering applications.
In the development of artificial cancellous bones, two major factors need to be considered: the integrity of the overall structure and its permeability. Whilst there have been many studies analysing the mechanical properties of artificial and natural cancellous bones, permeability studies, especially those using numerical simulation, are scarce. In this study, idealised cancellous bones were simulated from the morphological indices of natural cancellous bone. Three different orientations were also simulated to compare the anisotropic nature of the structure. Computational fluid dynamics methods were used to analyse fluid flow through the cancellous structures. A constant mass flow rate was used to determine the intrinsic permeability of the virtual specimens. The results showed similar permeability of the prismatic plate-and-rod model to the natural cancellous bone. The tetrakaidecahedral rod model had the highest permeability under simulated blood flow conditions, but the plate counterpart had the lowest. Analyses on the anisotropy of the virtual specimens showed the highest permeability for the horizontal orientation. Linear relationships were found between permeability and the two physical properties, porosity and bone surface area.
This study investigates the effects of an arbitrary wall shear stress on unsteady magnetohydrodynamic (MHD) flow of a Newtonian fluid with conjugate effects of heat and mass transfer. The fluid is considered in a porous medium over a vertical plate with ramped temperature. The influence of thermal radiation in the energy equations is also considered. The coupled partial differential equations governing the flow are solved by using the Laplace transform technique. Exact solutions for velocity and temperature in case of both ramped and constant wall temperature as well as for concentration are obtained. It is found that velocity solutions are more general and can produce a huge number of exact solutions correlative to various fluid motions. Graphical results are provided for various embedded flow parameters and discussed in details.
This study assessed the corrosion resistance, intracutaneous reactivity, acute systemic toxicity, and in situ tissue effect of the implantation of porous NiTi fabricated by metal injection molding in animal models. For the intracutaneous reactivity study, five intracutaneous injections were administered per site with and without the tested extract in polar and nonpolar solutions. The extract was also delivered via intravenous and intraperitoneal routes for acute systemic toxicity. TiAl6 V4 (control) and porous NiTi were implanted in rabbit femora for a period of 13 weeks to evaluate the in situ tissue response. Corrosion was evaluated through open and cyclic polarization in PBS, while biocompatibility was investigated by assessing the general conditions, skin irritation score (edema and erythema), and histopathology. No active dissolution or hysteresis loop was observed in the corrosion study. None of the animals exhibited death, moribundity, impending death, severe pain, self-mutilation, or overgrooming. No edema was observed at injection sites. Only the positive control showed an erythematous reaction at 24, 48, and 72 h observations (p < 0.001). Porous NiTi showed a low in situ biological response for inflammation, neovascularization, and fibrosis in comparison to the control implant (p = 0.247, 0.005, and 0.011, respectively). Porous NiTi also demonstrated high pitting corrosion resistance while causing no acute hypersensitivity or acute systemic toxicity. The study concludes that porous NiTi implants were unlikely to cause local sensitization, acute systemic toxicity, or chronic inflammatory reactions in an animal model. Porous NiTi also exhibited osseointegration equivalent to Ti6AI4 V of known biocompatibility.
To develop a green and facile adsorbent for removing indoor polluted formaldehyde (HCHO) gas, the biomass porous nanofibrous membranes (BPNMs) derived from microcrystalline cellulose/chitosan were fabricated by electrospinning. The enhanced chemical adsorption sites with diverse oxygen (O) and nitrogen (N)-containing functional groups were introduced on the surface of BPNMs by non-thermal plasma modification under carbon dioxide (CO2) and nitrogen (N2) atmospheres. The average nanofiber diameters of nanofibrous membranes and their nanomechanical elastic modulus and hardness values decreased from 341 nm to 175-317 nm and from 2.00 GPa and 0.25 GPa to 1.70 GPa and 0.21 GPa, respectively, after plasma activation. The plasma-activated nanofibers showed superior hydrophilicity (WCA = 0°) and higher crystallinity than that of the control. The optimal HCHO adsorption capacity (134.16 mg g-1) of BPNMs was achieved under a N2 atmosphere at a plasma power of 30 W and for 3 min, which was 62.42 % higher compared with the control. Pyrrolic N, pyridinic N, CO and O-C=O were the most significant O and N-containing functional groups for the improved chemical adsorption of the BPNMs. The adsorption mechanism involved a synergistic combination of physical and chemical adsorption. This study provides a novel strategy that combines clean plasma activation with electrospinning to efficiently remove gaseous HCHO.
We have successfully used continuous microwave flow synthesis (CMFS) technique for the template free synthesis of mesoporous hydroxyapatite. The continuous microwave flow reactor consisted of a modified 2.45GHz household microwave, peristaltic pumps and a Teflon coil. This cost effective and efficient system was exploited to produce semi-crystalline phase pure nano-sized hydroxyapatite. Effect of microwave power, retention time and the concentration of reactants on the phase purity, degree of crystallinity and surface area of the final product was studied in detail. X-ray diffraction (XRD) and Fourier transform infrared spectroscopy (FTIR) were used to study the phase purity and composition of the product, while transmission electron microscopy (TEM) was used to study the effect of process parameters on the morphology of hydroxyapatite. The TEM analysis confirmed the formation of spherical particles at low microwave power; however the morphology of the particles changed to mesoporous needle and rod-like structure upon exposing the reaction mixture to higher microwave power and longer retention time inside the microwave. The in-vitro ion dissolution behavior of the as synthesized hydroxyapatite was studied by determining the amount of Ca(2+) ion released in SBF solution.
The present study evaluates the corrosion behavior of poly[xylitol-(1,12-dodecanedioate)](PXDD)-HA coated porous iron (PXDD140/HA-Fe) and its cell-material interaction aimed for temporary bone scaffold applications. The physicochemical analyses show that the addition of 20 wt.% HA into the PXDD polymers leads to a higher crystallinity and lower surface roughness. The corrosion assessments of the PXDD140/HA-Fe evaluated by electrochemical methods and surface chemistry analysis indicate that HA decelerates Fe corrosion due to a lower hydrolysis rate following lower PXDD content and being more crystalline. The cell viability and cell death mode evaluations of the PXDD140/HA-Fe exhibit favorable biocompatibility as compared to bare Fe and PXDD-Fe scaffolds owing to HA's bioactive properties. Thus, the PXDD140/HA-Fe scaffolds possess the potential to be used as a biodegradable bone implant.