RESULTS: The adsorption of bovine serum albumin (BSA) onto anion-exchange Q-sepharose solid particulate support was investigated in batch adsorption experiments. Adsorption kinetics and isotherms were developed as a function of key industrially relevant parameters such as polymer loading, stirring speed, buffer pH, protein concentration and the state of protein dispersion (solid/aqueous) in order to optimize binding performance and adsorption capacity. Experimental results showed that the first order rate constant is higher at higher stirring speed, higher polymer loading, and under alkaline conditions, with a corresponding increase in equilibrium adsorption capacity. Increasing the stirring speed and using aqueous dispersion protein system increased the adsorption rate, but the maximum protein adsorption was unaffected. Regardless of the stirring speed, the adsorption capacity of the polymer was 2.8 mg/ml. However, doubling the polymer loading increased the adsorption capacity to 9.4 mg/ml.
CONCLUSIONS: The result demonstrates that there exists a minimum amount of polymer loading required to achieve maximum protein adsorption capacity under specific process conditions.
PURPOSE: The purpose of this in vitro study was to incorporate microparticles into a commercially available 3D printed denture base resin and compare its mechanical and biological properties with the conventional polymethyl methacrylate (PMMA) denture base material.
MATERIAL AND METHODS: Microparticles were collected from milled zirconia blanks and were blended with a 3D printing denture base resin (NextDent Denture 3D+). The optimal zirconia microparticle content (2%) for blending and printed was determined by using a liquid-crystal display (LCD) 3D printer. The printed specimens were then postrinsed and postpolymerized based on the manufacturer's instructions. Mechanical and biological characterization were carried out in terms of flexural strength, fracture toughness, and fungal adhesion. One-way ANOVA was carried out to analyze the results statistically.
RESULTS: The incorporation of microparticles in the 3D printed denture demonstrated higher mechanical strength (104.77 ±7.60 MPa) compared with conventional heat-polymerized denture base resin (75.15 ±24.41 MPa) (P