Displaying publications 81 - 100 of 136 in total

Abstract:
Sort:
  1. Solhan Yahya, Afidah Abdul Rahim, Affaizza Mohd Shah, Rohana Adnan
    Anticorrosion potential of mangrove tannins on aluminium alloys AA6061 in NaCl solution has been studied using potentiodynamic polarisation method and scanning electron microscopy (SEM). The study was carried out in different pH of corrosive medium in the absence and presence of various concentrations of tannin. The corrosion inhibition behaviour of the mangrove tannin on AA6061 aluminium alloy corrosion was found to be dependant on the pH of NaCl solution. Our results showed that the inhibition efficiency increased with increasing tannins concentration in chloride solution at pH 6. Treatment of aluminium alloy 6061 with all concentrations of mangrove tannins reduced the current density, thus decreased the corrosion rate. Tannins behaved as mixed inhibitors at pH 6 and reduction in current density predominantly affected in cathodic reaction. Meanwhile, at pH 12, addition of tannins shifted the corrosion potential to more cathodic potentials and a passivating effect was observed in anodic potentials. SEM studies have shown that the addition of tannins in chloride solution at pH 12 reduced the surface degradation and the formation of pits.
    Matched MeSH terms: Alloys
  2. Rosnita M, Yussof W, Zuhairi I, Zulkafli O, Samsudi S
    Sains Malaysiana, 2012;41:1133-1138.
    Annealing temperature plays an important role in the formation of an Au-Ga eutectic alloy. The effects of the annealing temperature on gold nanoparticles colloid and substrate surface were studied using AFM, FE-SEM and TEM. At 600oC, the layer of gold colloids particle formed an island in the state of molten eutectic alloy and absorbed evaporated metalorganics to formed nanowire (NW) underneath the alloy. Pit formed on the substrate surface due to the chemical reactions during the annealing process have an impact on the direction of growth of the NW. Without annealing, the NW formed vertically on the GaAs (100) surface. The growth direction depends on the original nucleation facets and surface energy when annealed. When annealed, the wire base is large and curved due to the migration of Ga atoms on the substrate surface towards the tip of the wire and the line tension between the substrate surface and gold particle.
    Matched MeSH terms: Alloys
  3. Muhamad Daud, Sarimah Mahat, Mohd Sharif Sattar
    MyJurnal
    Surface free energies have been evaluated from Young’s moduli and lattice parameter data of five aluminium alloys with varying amounts of stanum to determine the inter-correlation with anode capacity of the alloys. The composition containing ~1.47%Sn exhibits a minimum in the surface free energy which accounts for the decrease in the tendency of the alloy to undergo passivation thus resulting in a higher anode capacity of 2478Ah/kg at ≈ 0.08mA/cm 2 , current density. The results showed that aluminium alloy containing certain amount of stanum has lowered surface free energy, leading to reduction in passive film thickness and reduces metal/oxide bond strength. These factors in turn result in a better cathodic protection property of aluminium alloy containing stanum.
    Matched MeSH terms: Alloys
  4. Jiang H, Peng H, Guo H, Zeng Y, Li L, Zhang Y, et al.
    ACS Appl Mater Interfaces, 2020 Nov 18;12(46):51344-51356.
    PMID: 33146507 DOI: 10.1021/acsami.0c13139
    Thin-film lithium-ion microbatteries with a high energy density and long lifespan are exceedingly desired for developing self-powered integrated micro-nano devices and systems. However, exploring high-performance thin-film anodes still remains a challenge. Herein, a double-layer-structure diamond-like carbon-ZnS (DLC-ZnS) thin-film anode fabricated by radio frequency magnetron sputtering exhibits high specific capacity and good cycling stability up to 1000 cycles, superior to the pure ZnS thin-film anode. To understand the mechanism, the bimodal amplitude modulated-frequency modulated atomic force microscopy was used to explore the mechanical properties of the thin films, and the DLC layer shows significantly higher Young's modulus than the ZnS thin film. The DLC interface with a high Young's modulus can effectively buffer the mechanical stress originating from the huge volume changes of the ZnS layer during lithiation/delithiation processes; therefore, the DLC interface maintains the higher mechanical integrity of the DLC-ZnS thin film and improves the utilization of ZnS. In addition, the electrochemical kinetics of the DLC-ZnS and ZnS thin films were also investigated by electrochemical methods. Electrochemical impedance spectroscopy tests indicate the obstacle of the DLC interface to Li+ ion diffusion in the initial charge/discharge processes; however, the DLC-ZnS thin film exhibits lower total resistance than the ZnS thin film afterward. In particular, galvanostatic intermittent titration technique tests were performed to find out the differences between the two thin films during the galvanostatical charge/discharge processes. The results demonstrate the obviously enhanced conversion reaction reversibility and decreased alloy reaction polarization of the DLC-ZnS thin film; therefore, it delivers higher reversible capacity.
    Matched MeSH terms: Alloys
  5. Mayappan, Ramani, Ahmad Badri Ismail, Zainal Arifin Ahmad, Hussain, Luay Bakir, Ariga, Tadashi
    MyJurnal
    In this study the intermetallic (IMC) thickness of Sn-Pb, Sn-Zn and Sn-Zn-Bi solders on copper (Cu) substrate were measured at different temperatures using reflow methods. Cu6Sn5 intermetallic phase was detected between Sn-Pb solder and Cu substrate. The J-Cu5Zn8 phase was detected between Sn-Zn and Sn-Zn-Bi lead-free solders with Cu substrate. The thickness of the intermetallics increases with temperature. The IMC thickness for Sn-8Zn-3Bi solder is lower than Sn-9Zn solder for all the soldering temperatures, indicating that Bi has suppressed the initial IMC formation.
    Matched MeSH terms: Alloys
  6. Aslantas K, Danish M, Hasçelik A, Mia M, Gupta M, Ginta T, et al.
    Materials (Basel), 2020 Jul 06;13(13).
    PMID: 32640567 DOI: 10.3390/ma13132998
    Micro-turning is a micro-mechanical cutting method used to produce small diameter cylindrical parts. Since the diameter of the part is usually small, it may be a little difficult to improve the surface quality by a second operation, such as grinding. Therefore, it is important to obtain the good surface finish in micro turning process using the ideal cutting parameters. Here, the multi-objective optimization of micro-turning process parameters such as cutting speed, feed rate and depth of cut were performed by response surface method (RSM). Two important machining indices, such as surface roughness and material removal rate, were simultaneously optimized in the micro-turning of a Ti6Al4V alloy. Further, the scanning electron microscope (SEM) analysis was done on the cutting tools. The overall results depict that the feed rate is the prominent factor that significantly affects the responses in micro-turning operation. Moreover, the SEM results confirmed that abrasion and crater wear mechanism were observed during the micro-turning of a Ti6Al4V alloy.
    Matched MeSH terms: Alloys
  7. Padmakumar V, Premkala Raveendran K, Abdulla AM, Ganapathy S, Sainudeen S, Nasim VS, et al.
    J Pharm Bioallied Sci, 2019 May;11(Suppl 2):S397-S401.
    PMID: 31198376 DOI: 10.4103/JPBS.JPBS_44_19
    Background: Mercury is a naturally occurring metal that exists in three forms: elemental (metallic), inorganic, and organic mercury. Amalgam, which is an alloy of inorganic mercury, is used as a restorative material in dentistry. Organic mercury gets ingested in the body mainly by the consumption of seafood. Mercury is also stated to cause various adverse health effects such as gastrointestinal disturbances, dermatitis, muscle weakness, and neurological disorders. In recent years, the use of amalgam has become a controversy stating the various adverse effects of mercury. Hence, the study was conducted to determine and compare the variation in levels of organic and inorganic mercury in fish-eating children before and after placement of amalgam restoration.

    Materials and Methods: Seventy-five subjects, 42 males (56%) and 35 females (44%) of age group ranging 7-13 years, living in South Canara district of Karnataka, India, were selected as a part of the study. Hair and urine samples were collected for estimation of organic and inorganic levels of mercury, respectively. Informed consent was collected from all the participating subjects.

    Results: On comparison between organic and inorganic mercury levels during the study period, the concentration of organic mercury in hair samples was greater irrespective of amalgam restorations present (1.172 and 0.085, respectively; P < 0.001).

    Conclusion: Thus inorganic levels of mercury do not seem to pose a threat as much as the organic levels observed in hair, which remain fairly constant for a longer period of time. Hence in a coastal region where this study was undertaken and fish being a staple food, the risk could probably be attributed to more of an organic toxicity than an inorganic one. Thus amalgam is relatively safe to be practiced and the controversy against it should be reevaluated.

    Matched MeSH terms: Alloys
  8. Soo SY, Silikas N, Satterthwaite J
    Materials (Basel), 2019 Jun 23;12(12).
    PMID: 31234580 DOI: 10.3390/ma12122009
    A single paragraph of about 200 words maximum. For research articles, abstracts should give a pertinent overview of the work. We strongly encourage authors to use the following style of structured abstracts, but without headings: (1) Background: Place the question addressed in a broad context and highlight the purpose of the study; (2) Methods: Describe briefly the main methods or treatments applied; (3) Results: Summarize the article's main findings; and (4) Conclusions: Indicate the main conclusions or interpretations. The abstract should be an objective representation of the article, it must not contain results which are not presented and substantiated in the main text and should not exaggerate the main conclusions. Please add in this section. The aim of the study was to investigate the fracture behaviour of four different groups of zirconia abutments with internal and external connections: (A) Astra Tech ZirDesign™ abutment on Astra Tech Implants, (B) Procera® Esthetic abutment on Nobel Biocare MK III Groovy Implants, (C) IPS e.max® on Straumann Implants, and (D) ZiReal® Posts on Biomet 3I implants. The load was applied on the assemblies using a Zwick universal testing machine: the initial and final failure loads and amplitude were recorded using acoustic emission technique. Mean initial and final failure force was found to be significantly different in each group (P < 0.001). IPS e.max® Straumann abutments exhibited the highest resistance to final fracture force compared to other abutment types. Acoustic emission can be used as one of the methods to detect fracture behaviour of implant abutments. There were no significant differences in fracture loads between the internal and externally connected zirconia abutments studied. However, externally connected abutments demonstrated screw loosening and some deformations.
    Matched MeSH terms: Metal Ceramic Alloys
  9. Mahmoodian R, Hamdi M, Hassan MA, Akbari A
    PLoS One, 2015;10(6):e0130836.
    PMID: 26111217 DOI: 10.1371/journal.pone.0130836
    Titanium carbide-graphite (TiC/C) composite was successfully synthesized from Ti and C starting elemental powders using self-propagating high-temperature synthesis technique in an ultra-high plasma inert medium in a single stage. The TiC was exposed to a high-temperature inert medium to allow recrystallization. The product was then characterized using field emission scanning electron microscopy (FESEM) coupled with energy dispersive X-ray analysis (EDX), X-ray diffraction (XRD), Rietveld refinement, nanoindentation, and micro-hardness to determine the product's properties. The recorded micro-hardness of the product was 3660 HV, which is a 14% enhancement and makes is comparable to TiC materials.
    Matched MeSH terms: Alloys/chemistry*
  10. Muhammad Fauzinizam Razali, Abdus Samad Mahmud
    MyJurnal
    Introduction: Most patients with malocclusion are given orthodontic leveling therapy with the aim of reducing the vertical discrepancy between teeth. This computational study aims to evaluate the degree of deformation of su- perelastic NiTi arch wire upon bending at different deflections in a bracket system. Methods: A three-dimensional finite-element model of a wire-bracket system was developed to simulate the bending behavior of superelastic NiTi arch wire in three-brackets configuration. A superelastic subroutine was integrated in the model to anticipate the superelastic behavior of the arch wire. The mid span of the arch wire was loaded to different extent of deflections, ranging from 1.0 to 4.0 mm. The mechanical deformation of the arch wires was accessed from three parameters, in specific the unloading force, the bending stress and the martensite fraction. Results: The superelastic wire deflected at 4.0 mm yielded smaller unloading force than the wire bent at 1.0 mm. The bending stress was highly localized at the wire curvature, with the stress magnitude increased from 465 MPa at 1.0 mm to 951 MPa at 4.0 mm deflection. The martensite volume consistently increased throughout the bending, with a fully transformed martensite was ob- served as early as 2.0 mm of deflection. The magnitude of bending stress and the volume of fully transformed mar- tensite increased gradually in relation to the wire deflection. Conclusion: The wire-bracket system induced localize wire deformation, hindering complete utilization of superelasticity during orthodontic treatment.
    Matched MeSH terms: Dental Alloys
  11. M.O.H. Amuda, T.A. Olaniyan, L.O. Osoba, E.T. Akinlabi
    Sains Malaysiana, 2017;46:743-753.
    The mechanical properties of Dual Phase Steel (DPS)-duplex structure-produced by quenching in pre-heated bitumen have been investigated. Medium carbon steels intercritically heated at different temperatures and holding times were quenched in hot bitumen. Optical and scanning electron microscopy characterisation of the duplex structure showed extensive network of fibrous martensite in a ferritic matrix with occasional presence of polygonal martensite. The duplex phase structure exhibited continuous yielding dynamics, improving the tensile and hardness values by about 42 and 35%, respectively, relative to the normalised structure. But, the elongation and impact values decreased by about 42 and 50%, respectively, when compared to the normalised structure. These values are similar to those obtained in duplex structure produced using conventional oil quenching. The tensile fractured surface showed transition between a predominantly cleavage mode in the lower annealing temperature to a mixed mode in the upper bound of the annealing temperature. These findings suggest that pre-heated bitumen can be exploited for the production of DPSs.
    Matched MeSH terms: Dental Alloys
  12. Amjad M, Badshah S, Rafique AF, Adil Khattak M, Khan RU, Abdullah Harasani WI
    Materials (Basel), 2020 May 16;13(10).
    PMID: 32429420 DOI: 10.3390/ma13102299
    Implants are widely used in the human body for the replacement of affected bones. Fatigue failure is one of the serious concerns for implants. Therefore, understanding of the underlying mechanism leading to fatigue failure is important for the longevity of biomaterial implants. In this paper, the fracture toughness and fatigue crack growth of titanium alloy biomaterial Ti-27Nb has been experimentally investigated. The Ti-27Nb material is tested for fatigue crack growth in different environmental conditions representing the ambient and in vitro environments for 504 hours and 816 hours, respectively. Fractography of the tested specimen is conducted using Scanning Electron Microscope (SEM). The results of the fatigue crack growth propagation of the ambient and in vitro samples are similar in the Paris crack growth region. However, in the threshold region, the crack growth rate is higher for the Simulated Body Fluid (SBF) treated specimen. The fracture surface morphology of in vitro samples shows brittle fracture as compared to ambient specimens with significant plasticity and striations marks. It is proposed that a similar investigation may be conducted with specimens treated in SBF for prolonged periods to further ascertain the findings of this study.
    Matched MeSH terms: Alloys
  13. Baig MR, Gunaseelan R
    J Oral Implantol, 2012 Apr;38(2):149-53.
    PMID: 20932151 DOI: 10.1563/AAID-JOI-D-09-00089
    Passive fit of a long-span screw-retained implant prosthesis is an important criteria for the success of the restoration. This article describes a technique for fabricating a ceramometal implant fixed dental prosthesis (FDP) for a long-span partially edentulous situation by altering the conventional screw-retained design. The possibility of a passive fit is maximized by intraoral luting of the cast frame to milled abutments, and the potential framework distortion during fabrication is compensated to a major extent. Retrievability is ensured by screw retention of the prosthesis to the implants. Compared with conventional porcelain fused to metal screw-retained FDP, this prosthesis is relatively inexpensive to fabricate.
    Matched MeSH terms: Metal Ceramic Alloys/chemistry*
  14. Kokubo T
    Med J Malaysia, 2004 May;59 Suppl B:91-2.
    PMID: 15468833
    Metallic materials implanted into bone defects are generally encapsulated by a fibrous tissue. Some metallic materials such as titanium and tantalum, however, have been revealed to bond to the living bone without forming the fibrous tissue, when they were subjected to NaOH solution and heat treatments. Thus treated metals form bone tissue around them even in muscle, when they take a porous form. This kind of osteoconductive and osteoinductive properties are attributed to sodium titanate or tantalate layer on their surfaces formed by the NaOH and heat treatments. These layers induce the deposition of bonelike apatite on the surface of the metals in the living body. This kind of bioactive metals are useful as bone substitutes even highly loaded portions, such as hip joint, spine and tooth root.
    Matched MeSH terms: Alloys
  15. Pramanik A, Basak AK, Littlefair G, Debnath S, Prakash C, Singh MA, et al.
    Heliyon, 2020 Dec;6(12):e05554.
    PMID: 33344787 DOI: 10.1016/j.heliyon.2020.e05554
    Titanium alloys are difficult to machine using conventional methods, therefore, nonconventional processes are often chosen in many applications. Electrical discharge machining (EDM) is one of those nonconventional processes that is used frequently for shaping titanium alloys with their respective pros and cons. However, a good understanding of this process is very difficult to achieve as research results are not properly connected and presented. Therefore, this study investigates different types of EDM processes such as, wire EDM, die-sink EDM, EDM drill and hybrid EDM used to machine titanium alloys. Machining mechanism, tool electrode, dielectric, materials removal rate (MRR), and surface integrity of all these processes are critically analysed and correlated based on the evidence accessible in literature. Machining process suffer from lower material removal rate and high tool wear while applied on titanium alloys. Formation of recast layer, heat affected zone and tool wear is common in all types of EDM processes. Additional challenge in wire EDM of titanium alloys is wire breakage under severe machining conditions. The formation of TiC and TiO2 are noticed in recast layer depending on the type of dielectrics. Removal of debris from small holes during EDM drilling is a challenge. All these restricts the applications EDMed titanium alloys in high-tech applications such as, aerospace and biomedical areas. Most of these challenges come up due to extraordinary properties such as, low thermal conductivity, high melting point and high hardness, of titanium alloys. Though hybrid EDM has been introduced and there is some work on simulation of EDM process, further developments in EDM of this alloy is required for widening the application of this methods.
    Matched MeSH terms: Alloys
  16. Tamjidy M, Baharudin BTHT, Paslar S, Matori KA, Sulaiman S, Fadaeifard F
    Materials (Basel), 2017 May 15;10(5).
    PMID: 28772893 DOI: 10.3390/ma10050533
    The development of Friction Stir Welding (FSW) has provided an alternative approach for producing high-quality welds, in a fast and reliable manner. This study focuses on the mechanical properties of the dissimilar friction stir welding of AA6061-T6 and AA7075-T6 aluminum alloys. The FSW process parameters such as tool rotational speed, tool traverse speed, tilt angle, and tool offset influence the mechanical properties of the friction stir welded joints significantly. A mathematical regression model is developed to determine the empirical relationship between the FSW process parameters and mechanical properties, and the results are validated. In order to obtain the optimal values of process parameters that simultaneously optimize the ultimate tensile strength, elongation, and minimum hardness in the heat affected zone (HAZ), a metaheuristic, multi objective algorithm based on biogeography based optimization is proposed. The Pareto optimal frontiers for triple and dual objective functions are obtained and the best optimal solution is selected through using two different decision making techniques, technique for order of preference by similarity to ideal solution (TOPSIS) and Shannon's entropy.
    Matched MeSH terms: Alloys
  17. Patil PG, Nimbalkar-Patil SP, Karandikar AB
    J Contemp Dent Pract, 2014 Jan 1;15(1):112-5.
    PMID: 24939276
    This case report demonstrates sequential periodontic, orthodontic and prosthodontic treatment modalities to save and restore deep horizontally fractured maxillary central incisor. The location of fracture was deep in the mucosa which reveals less than 2 mm of tooth structure to receive the crown. The procedures like surgical crown lengthening, endodontic post placement, orthodontic forced eruption, core build-up and metal-ceramic crown restoration were sequentially performed to conserve the fractured tooth. Forced eruption is preferred to surgical removal of supporting alveolar bone, since forced eruption preserves the biologic width, maintains esthetics, and at the same time exposes sound tooth structure for the placement of restorative margins.
    Matched MeSH terms: Metal Ceramic Alloys/chemistry
  18. Norman NH, Worthington H, Chadwick SM
    J Orthod, 2016 Sep;43(3):176-85.
    PMID: 26836747 DOI: 10.1080/14653125.2015.1122260
    OBJECTIVE: To compare the clinical performance of nickel titanium (NiTi) versus stainless steel (SS) springs during orthodontic space closure.
    DESIGN: Two-centre parallel group randomized clinical trial.
    SETTING: Orthodontic Department University of Manchester Dental Hospital and Orthodontic Department Countess of Chester Hospital, United Kingdom.
    SUBJECTS AND METHODS: Forty orthodontic patients requiring fixed appliance treatment were enrolled, each being randomly allocated into either NiTi (n = 19) or SS groups (n = 21). Study models were constructed at the start of the space closure phase (T0) and following the completion of space closure (T1). The rate of space closure achieved for each patient was calculated by taking an average measurement from the tip of the canine to the mesiobuccal groove on the first permanent molar of each quadrant.
    RESULTS: The study was terminated early due to time constraints. Only 30 patients completed, 15 in each study group. There was no statistically significant difference between the amounts of space closed (mean difference 0.17 mm (95%CI -0.99 to 1.34; P = 0.76)). The mean rate of space closure for NiTi coil springs was 0.58 mm/4 weeks (SD 0.24) and 0.85 mm/4 weeks (SD 0.36) for the stainless steel springs. There was a statistically significant difference between the two groups (P = 0.024), in favour of the stainless steel springs, when the mean values per patient were compared.
    CONCLUSIONS: Our study shows that stainless steel springs are clinically effective; these springs produce as much space closure as their more expensive rivals, the NiTi springs.
    Matched MeSH terms: Alloys; Dental Alloys
  19. Roslinda Shamsudin, Abdul Razak Daud, Muhammad Azmi Abdul Hamid, Saiful Rizam Shamsudin
    Sains Malaysiana, 2007;36:195-200.
    Nitridation behaviour of Al-Mg-Si alloys was studied as a function of temperature by means of thermogravimetry method. A reactive gas, N2-4%H2 at a rate of 10 ml/min was purged into the thermogravimetry analyser chamber. The Al alloys were heated from 25oC to 625oC at the heating rate of 15oC/min and then reduced to 3oC/min until it reached 1500oC. It was found that by varying the amount of Mg and Si in Al-Mg-Si alloys significantly influenced the growth of the composites. A differential thermogravimetric curve shows the Mg containing alloys experienced many steps of chemical reactions. This indicates that besides AlN presence as a major phase, other compounds also exist in the final product. The X-ray diffraction results confirmed the existence of oxide phases such as a-Al2O3, MgAl2O4 and MgO in addition to residual Si and Al metal. The presence of oxide compounds is believed to be due to the reaction between the alloying elements and residual oxygen gas left in the reaction atmosphere. It was also found that Si could play a role in promoting the weight gain of the composite produced. The heating rate has also a profound effect on the weight gain, whereby higher heating rate resulted in low yielded of AlN during the nitridation reaction of the Al-Mg-Si alloys.
    Matched MeSH terms: Alloys
  20. Ali B, Tasirin SM, Aminayi P, Yaakob Z, Ali NT, Noori W
    Nanomaterials (Basel), 2018 Dec 14;8(12).
    PMID: 30558256 DOI: 10.3390/nano8121053
    Porous Ni, Ni-Co, Ni-Fe, and Ni-Cu magnetic alloys with a morphology similar to a giant barrel sponge were synthesized via a facile co-precipitation procedure and then by hydrogen reduction treatment. For the first time, the non-supported alloys with their unique morphology were employed in catalytic biogas decomposition (CBD) at a reaction temperature of 700 °C and 100 mL min-1 to produce syngas and carbon bio-nanofilaments, and the catalysts' behavior, CH₄ and CO₂ conversion, and the carbon produced during the reaction were investigated. All of the equimolar alloy catalysts showed good activity and stability for the catalytic biogas decomposition. The highest sustainability factor (0.66) and carbon yield (424%) were accomplished with the Ni-Co alloy without any significant inactivation for six hours, while the highest carbon efficiency of 36.43 was obtained with the Ni-Co catalyst, which is considered relatively low in comparison with industry standards, indicating a low carbon production process efficiency, possibly due to the relatively high biogas flow rate. The higher activity of the Ni-Co alloy catalyst was associated with the synergistic impact between nickel and cobalt, allowing the catalyst to maintain a high stability throughout the reaction period. Moreover, highly uniform, interwoven carbon bio-nanofilaments with a parallel and fishbone structure were achieved.
    Matched MeSH terms: Alloys
Filters
Contact Us

Please provide feedback to Administrator (afdal@afpm.org.my)

External Links