Displaying publications 81 - 100 of 135 in total

Abstract:
Sort:
  1. Ullah F, Othman MB, Javed F, Ahmad Z, Md Akil H
    Mater Sci Eng C Mater Biol Appl, 2015 Dec 1;57:414-33.
    PMID: 26354282 DOI: 10.1016/j.msec.2015.07.053
    This article aims to review the literature concerning the choice of selectivity for hydrogels based on classification, application and processing. Super porous hydrogels (SPHs) and superabsorbent polymers (SAPs) represent an innovative category of recent generation highlighted as an ideal mould system for the study of solution-dependent phenomena. Hydrogels, also termed as smart and/or hungry networks, are currently subject of considerable scientific research due to their potential in hi-tech applications in the biomedical, pharmaceutical, biotechnology, bioseparation, biosensor, agriculture, oil recovery and cosmetics fields. Smart hydrogels display a significant physiochemical change in response to small changes in the surroundings. However, such changes are reversible; therefore, the hydrogels are capable of returning to its initial state after a reaction as soon as the trigger is removed.
    Matched MeSH terms: Elastic Modulus
  2. Huong KH, Kannusamy S, Lim SY, Amirul AA
    J Ind Microbiol Biotechnol, 2015 Sep;42(9):1291-7.
    PMID: 26233315 DOI: 10.1007/s10295-015-1657-y
    Two-stage fermentation was normally employed to achieve a high poly(3-hydroxybutyrate-co-4-hydroxybutyrate) [P(3HB-co-4HB)] productivity with higher 4HB molar fraction. Here, we demonstrated single-stage fermentation method which is more industrial feasible by implementing mixed-substrate cultivation strategy. Studies on bioreactor scale show a remarkably high PHA accumulation of 73 wt%, contributing to a high PHA concentration and product yield of 8.6 g/L and 2.7 g/g, respectively. This fermentation strategy has resulted in copolymers with wider range of 4HB monomer composition, which ranges from 12 to 55 mol%. These copolymers show a broad range of weight average molecular weight (M w ) from 119.5 to 407.0 kDa. The copolymer characteristics were found to be predominantly affected by the nature of the substrates and the mixture strategies, regardless of the 4HB monomer compositions. This was supported by the determination of copolymer randomness using (13)C-NMR analysis. The study warrants significantly in the copolymer scale-up and modeling at industrial level.
    Matched MeSH terms: Elastic Modulus
  3. Zakaria NM, Yusoff NI, Hardwiyono S, Nayan KA, El-Shafie A
    ScientificWorldJournal, 2014;2014:594797.
    PMID: 25276854 DOI: 10.1155/2014/594797
    Enhanced resonance search (ERS) is a nondestructive testing method that has been created to evaluate the quality of a pavement by means of a special instrument called the pavement integrity scanner (PiScanner). This technique can be used to assess the thickness of the road pavement structure and the profile of shear wave velocity by using the principle of surface wave and body wave propagation. In this study, the ERS technique was used to determine the actual thickness of the asphaltic pavement surface layer, while the shear wave velocities obtained were used to determine its dynamic elastic modulus. A total of fifteen locations were identified and the results were then compared with the specifications of the Malaysian PWD, MDD UKM, and IKRAM. It was found that the value of the elastic modulus of materials is between 3929 MPa and 17726 MPa. A comparison of the average thickness of the samples with the design thickness of MDD UKM showed a difference of 20 to 60%. Thickness of the asphalt surface layer followed the specifications of Malaysian PWD and MDD UKM, while some of the values of stiffness obtained are higher than the standard.
    Matched MeSH terms: Elastic Modulus*
  4. Baradaran S, Moghaddam E, Nasiri-Tabrizi B, Basirun WJ, Mehrali M, Sookhakian M, et al.
    Mater Sci Eng C Mater Biol Appl, 2015 Apr;49:656-668.
    PMID: 25686995 DOI: 10.1016/j.msec.2015.01.050
    The effect of the addition of an ionic dopant to calcium phosphates for biomedical applications requires specific research due to the essential roles played in such processes. In the present study, the mechanical and biological properties of Ni-doped hydroxyapatite (HA) and Ni-doped HA mixed with graphene nanoplatelets (GNPs) were evaluated. Ni (3wt.% and 6wt.%)-doped HA was synthesized using a continuous precipitation method and calcined at 900°C for 1h. The GNP (0.5-2wt.%)-reinforced 6% Ni-doped HA (Ni6) composite was prepared using rotary ball milling for 15h. The sintering process was performed using hot isostatic pressing at processing conditions of 1150°C and 160MPa with a 1-h holding time. The results indicated that the phase compositions and structural features of the products were noticeably affected by the Ni and GNPs. The mechanical properties of Ni6 and 1.5Ni6 were increased by 55% and 75% in hardness, 59% and 163% in fracture toughness and 120% and 85% in elastic modulus compared with monolithic HA, respectively. The in-vitro biological behavior was investigated using h-FOB osteoblast cells in 1, 3 and 5days of culture. Based on the osteoblast results, the cytotoxicity of the products was indeed affected by the Ni doping. In addition, the effect of GNPs on the growth and proliferation of osteoblast cells was investigated in Ni6 composites containing different ratios of GNPs, where 1.5wt.% was the optimum value.
    Matched MeSH terms: Elastic Modulus/drug effects
  5. Feng Z, Ishiguro Y, Fujita K, Kosawada T, Nakamura T, Sato D, et al.
    Biomaterials, 2015 Oct;67:365-81.
    PMID: 26247391 DOI: 10.1016/j.biomaterials.2015.07.038
    In this paper, we present a general, fibril-based structural constitutive theory which accounts for three material aspects of crosslinked filamentous materials: the single fibrillar force response, the fibrillar network model, and the effects of alterations to the fibrillar network. In the case of the single fibrillar response, we develop a formula that covers the entropic and enthalpic deformation regions, and introduce the relaxation phase to explain the observed force decay after crosslink breakage. For the filamentous network model, we characterize the constituent element of the fibrillar network in terms its end-to-end distance vector and its contour length, then decompose the vector orientation into an isotropic random term and a specific alignment, paving the way for an expanded formalism from principal deformation to general 3D deformation; and, more important, we define a critical core quantity over which macroscale mechanical characteristics can be integrated: the ratio of the initial end-to-end distance to the contour length (and its probability function). For network alterations, we quantitatively treat changes in constituent elements and relate these changes to the alteration of network characteristics. Singular in its physical rigor and clarity, this constitutive theory can reproduce and predict a wide range of nonlinear mechanical behavior in materials composed of a crosslinked filamentous network, including: stress relaxation (with dual relaxation coefficients as typically observed in soft tissues); hysteresis with decreasing maximum stress under serial cyclic loading; strain-stiffening under uniaxial tension; the rupture point of the structure as a whole; various effects of biaxial tensile loading; strain-stiffening under simple shearing; the so-called "negative normal stress" phenomenon; and enthalpic elastic behaviors of the constituent element. Applied to compacted collagen gels, the theory demonstrates that collagen fibrils behave as enthalpic elasticas with linear elasticity within the gels, and that the macroscale nonlinearity of the gels originates from the curved fibrillar network. Meanwhile, the underlying factors that determine the mechanical properties of the gels are clarified. Finally, the implications of this study on the enhancement of the mechanical properties of compacted collagen gels and on the cellular mechanics with this model tissue are discussed.
    Matched MeSH terms: Elastic Modulus/drug effects
  6. Ahmad S, Singh VA, Hussein SI
    J Orthop Surg (Hong Kong), 2017 8 29;25(3):2309499017727946.
    PMID: 28844199 DOI: 10.1177/2309499017727946
    Meniscal allograft transplantation may be a better alternative for the treatment of irreparable meniscal injury compared to other forms of treatment. However, it remains to be seen whether the use fresh frozen allograft is better than cryopreserved allograft in treating this type of injury. We hypothesized that cryopreserved meniscal allograft would work better in maintaining the original biomechanical properties compared to fresh frozen ones, due to the lower amount of damage it incurs during the storage process. We examined young and healthy human menisci obtained from orthopedic oncology patients who underwent resection surgeries around the knee. The menisci obtained were preserved via cryopreservation and deep-freezing process. Traction tests were carried out on the menisci after 6 weeks of preservation. Twelve pairs ( N = 24) of menisci were divided equally into two groups, cryopreservation and deep frozen. There were six males and six female menisci donors for this study. The age range was between 15 and 35 years old (24.9 ± 8.6 years). Cryopreserved specimens had a higher ultimate tensile strength (UTS; 8.2 ± 1.3 Mpa vs. 13.3 ± 1.7 Mpa: p < 0.05) and elastic modulus (61.7 ± 27.6 Mpa vs. 87.0 ± 44.10 Mpa: p < 0.05) compared to the fresh frozen specimens. There was a significant difference in UTS ( p < 0.05) between the two groups but no significant difference in their elastic modulus ( p > 0.05). The elastic modulus of the preserved meniscus was similar to fresh normal menisci taken from other studies (60-120 Mpa; cryopreserved (87.0 ± 44.1) and fresh frozen (61.7 ± 27.5)). Cryopreserved menisci had a higher elastic modulus and point of rupture (UTS) compared to fresh frozen menisci. Cryopreservation proved to be a significantly better method of preservation, among the two methods of preservation in this study.
    Matched MeSH terms: Elastic Modulus
  7. Mahmood SK, Zakaria MZAB, Razak ISBA, Yusof LM, Jaji AZ, Tijani I, et al.
    Biochem Biophys Rep, 2017 Jul;10:237-251.
    PMID: 28955752 DOI: 10.1016/j.bbrep.2017.04.008
    The demands for applicable tissue-engineered scaffolds that can be used to repair load-bearing segmental bone defects (SBDs) is vital and in increasing demand. In this study, seven different combinations of 3 dimensional (3D) novel nanocomposite porous structured scaffolds were fabricated to rebuild SBDs using an extraordinary blend of cockle shells (CaCo3) nanoparticles (CCN), gelatin, dextran and dextrin to structure an ideal bone scaffold with adequate degradation rate using the Freeze Drying Method (FDM) and labeled as 5211, 5400, 6211, 6300, 7101, 7200 and 8100. The micron sized cockle shells powder obtained (75 µm) was made into nanoparticles using mechano-chemical, top-down method of nanoparticles synthesis with the presence of the surfactant BS-12 (dodecyl dimethyl bataine). The phase purity and crystallographic structures, the chemical functionality and the thermal characterization of the scaffolds' powder were recognized using X-Ray Diffractometer (XRD), Fourier transform infrared (FTIR) spectrophotometer and Differential Scanning Calorimetry (DSC) respectively. Characterizations of the scaffolds were assessed by Scanning Electron Microscopy (SEM), Degradation Manner, Water Absorption Test, Swelling Test, Mechanical Test and Porosity Test. Top-down method produced cockle shell nanoparticles having averagely range 37.8±3-55.2±9 nm in size, which were determined using Transmission Electron Microscope (TEM). A mainly aragonite form of calcium carbonate was identified in both XRD and FTIR for all scaffolds, while the melting (Tm) and transition (Tg) temperatures were identified using DSC with the range of Tm 62.4-75.5 °C and of Tg 230.6-232.5 °C. The newly prepared scaffolds were with the following characteristics: (i) good biocompatibility and biodegradability, (ii) appropriate surface chemistry and (iii) highly porous, with interconnected pore network. Engineering analyses showed that scaffold 5211 possessed 3D interconnected homogenous porous structure with a porosity of about 49%, pore sizes ranging from 8.97 to 337 µm, mechanical strength 20.3 MPa, Young's Modulus 271±63 MPa and enzymatic degradation rate 22.7 within 14 days.
    Matched MeSH terms: Elastic Modulus
  8. Aziz J, Ahmad MF, Rahman MT, Yahya NA, Czernuszka J, Radzi Z
    Int J Biol Macromol, 2018 Feb;107(Pt A):1030-1038.
    PMID: 28939521 DOI: 10.1016/j.ijbiomac.2017.09.066
    Successful use of tissue expanders depends on the quality of expanded tissue. This study evaluates the impact of anisotropic self-inflating tissue expander (SITE) on the biomechanics of skin. Two different SITE were implanted subcutaneously on sheep scalps; SITE that requires 30days for maximum expansion (Group A; n=5), and SITE that requires 21days for maximum expansion (Group B; n=5). Control animals (n=5) were maintained without SITE implantation. Young's Modulus, D-periodicity, overlap and gap region length, diameter, and height difference between overlap and gap regions on collagen fibrils were analyzed using atomic force microscopy. Histology showed no significant differences in dermal thickness between control and expanded skin of groups A and B. Furthermore, most parameters of expanded skin were similar to controls (p>0.05). However, the height difference between overlap and gap regions was significantly smaller in group B compared to both control and group A (p<0.01). Strong correlation was observed between Young's Modulus of overlap and gap regions of the control and group A, but not group B. Results suggest that a relatively slower SITE can be useful in reconstructive surgery to maintain the biomechanical properties of expanded skin.
    Matched MeSH terms: Elastic Modulus
  9. Zakaria S, Mat-Husain SZ, Ying-Hwey K, Xin-Kai K, Mohd-Badawi A, Abd-Ghani NA, et al.
    Iran J Basic Med Sci, 2017 Dec;20(12):1360-1367.
    PMID: 29238472 DOI: 10.22038/IJBMS.2017.9610
    Objectives: Alcohol consumption induces oxidative stress on bone, which in turn increases the risk of osteoporosis. This study determined the effects of vitamin E on bone strength and bone mineral content in alcohol-induced osteoporotic rats.

    Materials and Methods: Three months old Sprague Dawley male rats were randomly divided into 5 groups: (I) control group; (II) alcohol (3g/kg) + normal saline; (III) alcohol (3g/kg) + olive oil; (IV) alcohol (3g/kg) + alpha-tocopherol (60mg/kg) and (V) alcohol (3g/kg) + palm vitamin E (60mg/kg). The treatment lasted for three months. Following sacrifice, the right tibia was subjected to bone biomechanical test while the lumbar (fourth and fifth lumbar) and left tibia bones were harvested for bone mineral measurement.

    Results: Alcohol caused reduction in bone biomechanical parameters (maximum force, ultimate stress, yield stress and Young's modulus) and bone minerals (bone calcium and magnesium) compared to control group (P<0.05). Palm vitamin E was able to improve bone biomechanical parameters by increasing the maximum force, ultimate stress and Young's modulus (P<0.05) while alpha-tocopherol was not able to. Both alpha-tocopherol and palm vitamin E were able to significantly increase tibia calcium and magnesium content while only alpha-tocopherol caused significant increase in lumbar calcium content (P<0.05).

    Conclusion: Both palm vitamin E and alpha-tocopherol improved bone mineral content which was reduced by alcohol. However, only palm vitamin E was able to improve bone strength in alcohol treated rats.

    Matched MeSH terms: Elastic Modulus
  10. Razali MH, Ismail NA, Mat Amin KA
    Int J Biol Macromol, 2020 Jun 15;153:1117-1135.
    PMID: 31751725 DOI: 10.1016/j.ijbiomac.2019.10.242
    The synthesized titanium dioxide nanotubes (TiO2-NTs) were emerged as wound healing enhancer as well as exhibited significant wound healing activity on Sprague Dawley rats. In our present study, the blends of GG and TiO2-NTs bio-nanocomposite film was characterised by fourier transform infrared (FTIR), x-ray diffraction (XRD), scanning electron microscopy (SEM), thermogravimetric analysis, atomic force microscopy (AFM). The morphology of TiO2-NTs was investigated using transmission electron microscopy (TEM). The mechanical properties study shows that the GG + TiO2-NTs (20 w/w %) bio-nanocomposite film possessed the highest tensile strength and young modulus which are (4.56 ± 0.15) MPa and (68 ± 1.63) MPa, respectively. GG + TiO2-NTs (20 w/w %) also displays the highest antibacterial activity with (16 ± 0.06) mm, (16 ± 0.06) mm, (14 ± 0.06) mm, and (12 ± 0.25) mm inhibition zone were recorded against Staphylococcus aureus, Streptococcus, Escherichia coli, and Pseudomonas aeruginosa. The prepared bio-nanocomposite films have good biocompatibility against 3T3 mouse fibroblast cells and caused accelerated healing of open excision type wounds on Sprague Dawley rat model. The synergistic effects of bio-nanocomposite film like good swelling and WVTR properties, excellent hydrophilic nature, biocompatibility, wound appearance and wound closure rate through in vivo test makes it a suitable candidate for wound healing applications.
    Matched MeSH terms: Elastic Modulus
  11. Leong SS, Wong JHD, Md Shah MN, Vijayananthan A, Jalalonmuhali M, Chow TK, et al.
    Nephrology (Carlton), 2021 Jan;26(1):38-45.
    PMID: 33058334 DOI: 10.1111/nep.13805
    AIM: Renal biopsy is the gold standard for the histological characterization of chronic kidney disease (CKD), of which renal fibrosis is a dominant component, affecting its stiffness. The aim of this study was to investigate the correlation between kidney stiffness obtained by shear wave elastography (SWE) and renal histological fibrosis.

    METHODS: Shear wave elastography assessments were performed in 75 CKD patients who underwent renal biopsy. The SWE-derived estimates of the tissue Young's modulus (YM), given as kilopascals (kPa), were measured. YM was correlated to patients' renal histological scores, broadly categorized into glomerular, tubulointerstitial and vascular scores.

    RESULTS: Young's modulus correlates significantly with tubulointerstitial score (ρ = 0.442, P 

    Matched MeSH terms: Elastic Modulus
  12. Sharip NS, Ariffin H, Andou Y, Shirosaki Y, Bahrin EK, Jawaid M, et al.
    Molecules, 2020 Sep 30;25(19).
    PMID: 33008017 DOI: 10.3390/molecules25194498
    Incorporation of nanocellulose could improve wear resistance of ultra-high molecular weight polyethylene (UHMWPE) for an artificial joint application. Yet, the extremely high melt viscosity of the polymer may constrict the mixing, leading to fillers agglomeration and poor mechanical properties. This study optimized the processing condition of UHMWPE/cellulose nanofiber (CNF) bionanocomposite fabrication in triple screw kneading extruder by using response surface methodology (RSM). The effect of the process parameters-temperature (150-190 °C), rotational speed (30-60 rpm), and mixing time (30-45 min)-on mechanical properties of the bionanocomposites was investigated. Homogenous filler distribution, as confirmed by scanning electron microscopy-energy dispersive spectroscopy (SEM-EDS) analysis, was obtained through the optimal processing condition of 150 °C, 60 rpm, and 45 min. The UHMWPE/CNF bionanocomposites exhibited improved mechanical properties in terms of Young's and flexural modulus by 11% and 19%, respectively, as compared to neat UHMWPE. An insignificant effect was observed when maleic anhydride-grafted-polyethylene (MAPE) was added as compatibilizer. The obtained results proved that homogenous compounding of high melt viscosity UHMWPE with CNF was feasible by optimizing the melt blending processing condition in triple screw kneading extruder, which resulted in improved stiffness, a contributing factor for wear resistance.
    Matched MeSH terms: Elastic Modulus
  13. Ooi KS, Haszman S, Wong YN, Soidin E, Hesham N, Mior MAA, et al.
    Materials (Basel), 2020 Sep 30;13(19).
    PMID: 33007893 DOI: 10.3390/ma13194352
    The eminent aim for advance wound management is to provide a great impact on the quality of life. Therefore, an excellent strategy for an ideal wound dressing is being developed that eliminates certain drawbacks while promoting tissue regeneration for the prevention of bacterial invasion. The aim of this study is to develop a bilayer hybrid biomatrix of natural origin for wound dressing. The bilayer hybrid bioscaffold was fabricated by the combination of ovine tendon collagen type I and palm tree-based nanocellulose. The fabricated biomatrix was then post-cross-linked with 0.1% (w/v) genipin (GNP). The physical characteristics were evaluated based on the microstructure, pore size, porosity, and water uptake capacity followed by degradation behaviour and mechanical strength. Chemical analysis was performed using energy-dispersive X-ray spectroscopy (EDX), Fourier transform infrared spectrophotometry (FTIR), and X-ray diffraction (XRD). The results demonstrated a uniform interconnected porous structure with optimal pore size ranging between 90 and 140 μm, acceptable porosity (>70%), and highwater uptake capacity (>1500%). The biodegradation rate of the fabricated biomatrix was extended to 22 days. Further analysis with EDX identified the main elements of the bioscaffold, which contains carbon (C) 50.28%, nitrogen (N) 18.78%, and oxygen (O) 30.94% based on the atomic percentage. FTIR reported the functional groups of collagen type I (amide A: 3302 cm-1, amide B: 2926 cm-1, amide I: 1631 cm-1, amide II: 1547 cm-1, and amide III: 1237 cm-1) and nanocellulose (pyranose ring), thus confirming the presence of collagen and nanocellulose in the bilayer hybrid scaffold. The XRD demonstrated a smooth wavy wavelength that is consistent with the amorphous material and less crystallinity. The combination of nanocellulose with collagen demonstrated a positive effect with an increase of Young's modulus. In conclusion, the fabricated bilayer hybrid bioscaffold demonstrated optimum physicochemical and mechanical properties that are suitable for skin wound dressing.
    Matched MeSH terms: Elastic Modulus
  14. Olaiya NG, Nuryawan A, Oke PK, Khalil HPSA, Rizal S, Mogaji PB, et al.
    Polymers (Basel), 2020 Mar 05;12(3).
    PMID: 32151004 DOI: 10.3390/polym12030592
    The current research trend for excellent miscibility in polymer mixing is the use of plasticizers. The use of most plasticizers usually has some negative effects on the mechanical properties of the resulting composite and can sometimes make it toxic, which makes such polymers unsuitable for biomedical applications. This research focuses on the improvement of the miscibility of polymer composites using two-step mixing with a rheomixer and a mix extruder. Polylactic acid (PLA), chitin, and starch were produced after two-step mixing, using a compression molding method with decreasing composition variation (between 8% to 2%) of chitin and increasing starch content. A dynamic mechanical analysis (DMA) was used to study the mechanical behavior of the composite at various temperatures. The tensile strength, yield, elastic modulus, impact, morphology, and compatibility properties were also studied. The DMA results showed a glass transition temperature range of 50 °C to 100 °C for all samples, with a distinct peak value for the loss modulus and factor. The single distinct peak value meant the polymer blend was compatible. The storage and loss modulus increased with an increase in blending, while the loss factor decreased, indicating excellent compatibility and miscibility of the composite components. The mechanical properties of the samples improved compared to neat PLA. Small voids and immiscibility were noticed in the scanning electron microscopy images, and this was corroborated by X-ray diffraction graphs that showed an improvement in the crystalline nature of PLA with starch. Bioabsorption and toxicity tests showed compatibility with the rat system, which is similar to the human system.
    Matched MeSH terms: Elastic Modulus
  15. Shahril Anuar Bahari, Kamrie Kamlon, Masitah Abu Kassim
    MyJurnal
    In this study, the rice husk flour-plastic waste composites (RPC) was produced from polypropylene (PP) and high density polyethylene (HDPE) wastes with 30 and 50% rice husk flour (RHF) contents. RPC was made by melt compounding and compression moulding processes. The electrical resistivity, thermal stability and tensile strength of RPC were determined. The RPC was tested in electrical resistivity and tensile strength according to the ASTM D-257 and ASTM D-638 respectively, while thermal stability was tested using thermogravimetric analysis (TGA) method. From the results, high content of RHF reduces all properties, except for tensile modulus of elasticity (TMOE) in tensile strength test. The ability of moisture absorption and the presence of hemicelluloses, cellulose and silica in RHF reduce the electrical resistivity and thermal stability behaviour of RPC from 50% RHF. The good binding elements and filler agglomeration in RPC from 50% RHF improve only TMOE. Insufficient stress transfer and rigid interphase occurred between RHF and plastics during tensile maximum load and elongation at break (Eb) in tensile strength test. In general, RPC from HDPE indicates better thermal stability, tensile modulus of rupture and Eb (in tensile strength test) compared to PP, based on the good behaviour of thermal conductivity, low water absorption, high molecular weight and good elongation properties of HDPE. However, RPC from PP shows good electrical resistance due to the low thermal expansion coefficient of PP.
    Matched MeSH terms: Elastic Modulus
  16. Nor Faadila, M.I., Harivaindaran, K.V., Tajul, A. Yang
    MyJurnal
    Texture and biochemical changes, specifically in moisture, protein content and amino acid profile were studied throughout the molt cycle of Panaeus monodon. This study was initiated to investigate changes that may occur in mass and tissue composition during different molting stages. Molting of Penaeus monodon are classified into 3 main stages; postmolt, intermolt and premolt. Result of biochemical analysis, shows that moisture varies from 78.02-80.88%, indicating a maximum value during postmolt and minimum value during premolt. Total protein content was found to be higher during intermolt (23.48%) and postmolt (22.27%) compared to premolt (23.10%). The result of SDS-PAGE electrophoresis shows a higher intensity of protein band during intermolt which corresponds to higher protein content. Thus, this electrophoresis method is useful as an alternative to determine different stages of shrimp molting. This is based on intensity of the protein band which is referring to protein content of the shrimp at its different stages. The amino acid profile showed that arginine, alanine, glutamic acid, glycine, lycine, and thronine increased during premolt whilst isoleucine and phenylalanine higher during postmolt. Aspartic acid and histidine was higher in intermolt than in premolt and postmolt. Texture analysis carried out give an elastic modulus value that is high during premolt compared to postmolt and intermolt. There are significant changes in texture and biochemical composition through elastic modules value and protein composition of Penaeus monodon during each stages of moltcycle.
    Matched MeSH terms: Elastic Modulus
  17. Al-Mansob RA, Ismail A, Yusoff NI, Rahmat RA, Borhan MN, Albrka SI, et al.
    PLoS One, 2017;12(2):e0171648.
    PMID: 28182724 DOI: 10.1371/journal.pone.0171648
    Road distress results in high maintenance costs. However, increased understandings of asphalt behaviour and properties coupled with technological developments have allowed paving technologists to examine the benefits of introducing additives and modifiers. As a result, polymers have become extremely popular as modifiers to improve the performance of the asphalt mix. This study investigates the performance characteristics of epoxidized natural rubber (ENR)-modified hot-mix asphalt. Tests were conducted using ENR-asphalt mixes prepared using the wet process. Mechanical testing on the ENR-asphalt mixes showed that the resilient modulus of the mixes was greatly affected by testing temperature and frequency. On the other hand, although rutting performance decreased at high temperatures because of the increased elasticity of the ENR-asphalt mixes, fatigue performance improved at intermediate temperatures as compared to the base mix. However, durability tests indicated that the ENR-asphalt mixes were slightly susceptible to the presence of moisture. In conclusion, the performance of asphalt pavement can be enhanced by incorporating ENR as a modifier to counter major road distress.
    Matched MeSH terms: Elastic Modulus
  18. Abedinia A, Ariffin F, Huda N, Nafchi AM
    Int J Biol Macromol, 2017 May;98:586-594.
    PMID: 28174080 DOI: 10.1016/j.ijbiomac.2017.01.139
    The effects of different pretreatments on yield and composition of extraction, physicochemical, and rheological properties of duck feet gelatin (DFG) were investigated. Gelatins were extracted from the whole feet of Pekin duck with an average yield of 4.09%, 3.65%, and 5.75% for acidic (Ac-DFG), alkaline (Al-DFG), and enzymatic (En-DFG) pretreatment on a wet weight basis, respectively. Proteins at 81.38%, 79.41%, 82.55%, and 87.38% were the major composition for Ac-DFG, Al-DFG, En-DFG, and bovine, respectively. Amino acid analysis showed glycine as the predominant amino acid in Ac-DFG, followed by hydroxyproline, proline, and alanine for Ac-DFG, Al-DFG, and En-DFG, respectively. Rheological analysis indicated that the maximum elastic modulus (9972.25Pa) and loss modulus (4956.28Pa) for Ac-DFG gelatin were significantly higher than those of other gelatins. Extracted gelatins contained α1 and α2 chains as the predominant components, and enzymatic gelatin had low molecular weight peptides. Fourier transform infrared spectroscopy showed that the peak of the gelatins was mainly positioned in the amide band region (amides I, II, and III). A considerable loss of molecular-order triple helical structure was also observed after pepsin treatment. In summary, duck feet gelatin has potential to replace as mammalian gelatin in food and pharmaceutical industry.
    Matched MeSH terms: Elastic Modulus
  19. Gaaz TS, Sulong AB, Kadhum AAH, Al-Amiery AA, Nassir MH, Jaaz AH
    Molecules, 2017 May 20;22(5).
    PMID: 28531126 DOI: 10.3390/molecules22050838
    Nanotubular clay minerals, composed of aluminosilicate naturally structured in layers known as halloysite nanotubes (HNTs), have a significant reinforcing impact on polymer matrixes. HNTs have broad applications in biomedical applications, the medicine sector, implant alloys with corrosion protection and manipulated transportation of medicines. In polymer engineering, different research studies utilize HNTs that exhibit a beneficial enhancement in the properties of polymer-based nanocomposites. The dispersion of HNTs is improved as a result of pre-treating HNTs with acids. The HNTs' percentage additive up to 7% shows the highest improvement of tensile strength. The degradation of the polymer can be also significantly improved by doping a low percentage of HNTs. Both the mechanical and thermal properties of polymers were remarkably improved when mixed with HNTs. The effects of HNTs on the mechanical and thermal properties of polymers, such as ultimate strength, elastic modulus, impact strength and thermal stability, are emphasized in this study.
    Matched MeSH terms: Elastic Modulus
  20. Matsumura Y, Kamimura Y, Lee CY, Gorb SN, Rajabi H
    Sci Rep, 2021 04 12;11(1):7920.
    PMID: 33846369 DOI: 10.1038/s41598-021-86864-1
    We unveiled the penile penetration mechanics of two earwig species, Echinosoma horridum, whose intromittent organ, termed virga, is extraordinarily long, and E. denticulatum, whose virga is conversely short. We characterised configuration, geometry, material and bending stiffness for both virga and spermatheca. The short virga of E. denticulatum has a material gradient with the stiffer base, whereas the long virga of E. horridum and the spermathecae of both species are homogeneously sclerotised. The long virga of E. horridum has a lower bending stiffness than the spermatheca. The virga of E. denticulatum is overall less flexible than the spermatheca. We compared our results to a previous study on the penetration mechanics of elongated beetle genitalia. Based on the comparison, we hypothesised that the lower stiffness of the male intromittent organ comparing to the corresponding female structure is a universal prerequisite for the penetration mechanics of the elongated intromittent organ in insects.
    Matched MeSH terms: Elastic Modulus
Filters
Contact Us

Please provide feedback to Administrator (afdal@afpm.org.my)

External Links